# US 2021/0083057 A1 · Semiconductor device, manufacturing method thereof, and semiconductor storage device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0083057 A1
- Document ID: US20210083057A1
- Status: Published application
- Kind: A1
- Application number: 16/817,814
- Filed: 2020-03-13
- Published: 2021-03-18
- Earliest claimed: 2019-09-18
- Assignees: Kioxia Corporation
- Applicants: Kioxia Corporation
- Inventors: Masayuki KITAMURA
- Web page: https://patentgrep.com/patent/US20210083057A1

## CPC

- H10P 14/3434: {being oxide semiconductor materials (Group IIB-VIA semiconductor materials H10P14/3424)}
- H10D 64/01316: {the conductor comprising a layer of elemental metal contacting the insulator, e.g. Ta, W, Mo or Al}
- H10D 64/667: {the conductor comprising a layer of alloy material, compound material or organic material contacting the insulator, e.g. TiN workfunction layers (having lateral variation H10D64/671)}
- H10P 14/412: {Deposition of metallic or metal-silicide materials}
- H10D 62/80: characterised by the materials
- H10D 64/037: {comprising charge-trapping insulators}
- H10P 14/24: using chemical vapour deposition [CVD]
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A semiconductor device according to an embodiment includes an oxide film containing first element and a conductive film provided to be in contact with the oxide film, containing metal element and oxygen element, and having conductivity. A range of a volume density of the oxygen element in the conductive film is different between cases where the metal element are tungsten (W), molybdenum (Mo), titanium (Ti), chromium (Cr), vanadium (V), iron (Fe), copper (Cu), tantalum (Ta), or niobium (Nb).

## Claims

### Claim 1

A semiconductor device comprising:
an oxide film containing first element; and
a conductive film provided to be in contact with the oxide film, containing metal element and oxygen element, wherein
a volume density of the oxygen element in the conductive film is
less than 2.38×1022 atoms/cm3 when the metal element is tungsten (W),
less than 4.27×1022 atoms/cm3 when the metal element is molybdenum (Mo),
less than 2.28×1022 atoms/cm3 when the metal element is titanium (Ti),
less than 5.00×1022 atoms/cm3 when the metal element is chromium (Cr),
less than 4.23×1022 atoms/cm3 when the metal element is vanadium (V),
less than 4.84×1022 atoms/cm3 when the metal element is iron (Fe),
less than 2.82×1022 atoms/cm3 when the metal element is copper (Cu),
less than 3.32×1022 atoms/cm3 when the metal element is tantalum (Ta), and
less than 2.78×1022 atoms/cm3 when the metal element niobium (Nb).

### Claim 2 (depends on 1)

The device of claim 1, wherein the volume density of the oxygen element in the conductive film is 1.0×1016 atoms/cm3 or more.

### Claim 3 (depends on 1)

The device of claim 1, wherein an atom of the metal element is bounded with an atom of the oxygen element in the conductive film, and said atom of the oxygen element is bounded with an atom of the first element.

### Claim 4 (depends on 1)

The device of claim 1, wherein a binding energy between the metal element and an oxygen element is smaller than a binding energy between an oxygen element and the first element.

### Claim 5 (depends on 1)

The device of claim 1, further comprising a film on the conductive film, which contains metal element of a same type as or a different type from the metal element and has a lower oxygen concentration than the conductive film.

### Claim 6

A manufacturing method of a semiconductor device, comprising:
forming an oxide film containing first element on a semiconductor substrate; and
forming a conductive film on the oxide film by using a material gas that contains metal element, a reducing gas that reduces the metal element, and a carrier gas that introduces the material gas into the substrate, wherein
at least one of the material gas, the reducing gas, and the carrier gas contains oxygen element, and
a temperature of the substrate in formation of the conductive film is higher than a sublimation temperature of metal oxide of the metal element.

### Claim 7 (depends on 6)

The method of claim 6, wherein forming the conductive film comprising:
forming a first layer that is in contact with the oxide film and contains the metal element and the oxygen element; and
forming a second layer after forming the first layer, the second layer contains a metal element of a same type as or a different type from the metal element, and has a lower oxygen concentration than the first layer.

### Claim 8 (depends on 6)

The method of claim 6, wherein the metal element is tungsten (W), titanium (Ti), molybdenum (Mo), chromium (Cr), vanadium (V), iron (Fe), copper (Cu), tantalum (Ta), or niobium (Nb).

### Claim 9 (depends on 6)

The method of claim 6, wherein
the material gas contains a tungsten compound,
the reducing gas contains hydrogen gas (H2), nitrogen dioxide gas (NO2), nitrous oxide gas (N2O), carbon monoxide gas (CO), oxygen gas (O2), or ozone gas (O3), and
the carrier gas contains argon gas (Ar), nitrogen gas (N2), or carbon dioxide gas (CO2).

### Claim 10

A semiconductor storage device comprising:
a plurality of conductive films stacked apart from each other in a first direction;
a plurality of oxide films that are in contact with the conductive films in the first direction and are stacked via the conductive films;
a semiconductor layer penetrating through the conductive films and the oxide films in the first direction; and
a charge storage layer arranged between the semiconductor layer and the conductive films in a second direction crossing the first direction, wherein
the oxide films contain first element,
the conductive films contain metal element and oxygen element, and
a volume density of the oxygen element in the conductive film is
less than 2.38×1022 atoms/cm3 when the metal element is tungsten,
less than 4.27×1022 atoms/cm3 when the metal element is molybdenum,
less than 2.28×1022 atoms/cm3 when the metal element is titanium,
less than 5.00×1022 atoms/cm3 when the metal element is chromium,
less than 4.23×1022 atoms/cm3 when the metal element is vanadium,
less than 4.84×1022 atoms/cm3 when the metal element is iron,
less than 2.82×1022 atoms/cm3 when the metal element is copper,
less than 3.32×1022 atoms/cm3 when the metal element is tantalum, and
less than 2.78×1022 atoms/cm3 when the metal element is niobium.