# US 2021/0082774 A1 · Evaluation method of metal contamination

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0082774 A1
- Document ID: US20210082774A1
- Status: Published application
- Kind: A1
- Application number: 16/956,282
- Filed: 2018-08-02
- Published: 2021-03-18
- Earliest claimed: 2017-12-22
- Assignees: Globalwafers Japan Co., Ltd.
- Applicants: Globalwafers Japan Co., Ltd.
- Inventors: Nobue ARAKI; Takeshi ONOZUKA; Tomoyuki ISHIHARA
- Web page: https://patentgrep.com/patent/US20210082774A1

## CPC

- H10P 74/203: {Structural properties, e.g. testing or measuring thicknesses, line widths, warpage, bond strengths or physical defects}
- C30B 15/00: Single-crystal growth by pulling from a melt, e.g. Czochralski method (under a protective fluid C30B27/00)
- C30B 15/14: Heating of the melt or the crystallised materials
- C30B 15/203: {the relationship of pull rate (v) to axial thermal gradient (G)}
- C30B 29/06: Silicon
- G01N 21/6408: {with measurement of decay time, time resolved fluorescence}
- G01N 21/6489: {Photoluminescence of semiconductors}
- H01J 37/32073: {Corona discharge}
- H10P 14/00: Formation of materials, e.g. in the shape of layers or pillars
- H10P 74/232: {comprising connection or disconnection of parts of a device in response to a measurement}
- H01J 2237/24592: Inspection and quality control of devices
- H10P 74/23: {characterised by multiple measurements, corrections, marking or sorting processes}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR
- G01N: INVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIR CHEMICAL OR PHYSICAL PROPERTIES (measuring or testing apparatus or processes other than immunoassay, involving enzymes or microorganisms C12M, C12Q)
- H01J: ELECTRIC DISCHARGE TUBES OR DISCHARGE LAMPS (spark-gaps H01T; electric arc lamps H05B31/00; particle accelerators H05H)

## Abstract

A method of evaluating metal contamination by measuring the amount of metal contaminants to a silicon wafer in a rapid thermal processing apparatus includes steps of obtaining a Si single crystal grown by the Czochralski method at a pulling rate of 1.0 mm/min or lower, the crystal having oxygen concentration of 1.3×1018 atoms/cm3 or less, slicing silicon wafers from the Si single crystal except regions of 40 mm toward the central portion from the head of the single crystal and 40 mm toward the central portion from the tail, heat-treating the silicon wafer with a rapid thermal processing apparatus and transferring contaminants from members in a furnace of the rapid thermal processing apparatus to the silicon wafer, and measuring a lifetime of the silicon wafer to which contaminants are transferred.

## Claims

### Claim 1

A method of evaluating metal contamination by measuring an amount of metal contaminants transferred to a silicon wafer in a rapid thermal processing apparatus, comprising steps of:
obtaining a silicon single crystal grown by the Czochralski method at a pulling rate of 1.0 mm/min or lower, the crystal having an oxygen concentration of 1.3×1018 atoms/cm3 or less;
slicing silicon wafers from the silicon single crystal except a region of 40 mm toward a central portion from a head of the single crystal and a region of 40 mm toward the central portion from a tail;
heat-treating the silicon wafer in a rapid thermal processing apparatus to transfer contaminants from members in a furnace of the rapid thermal processing apparatus to the silicon wafer; and
measuring a lifetime of the silicon wafer to which contaminants are transferred.

### Claim 2 (depends on 1)

The method of evaluating metal contamination according to claim 1, wherein in the step of heat-treating a silicon wafer in a rapid thermal processing apparatus to transfer contaminants from members in a furnace of the rapid thermal processing apparatus to the silicon wafer, an oxide film having a thickness of 2 nm or more is formed on the silicon wafer by holding the silicon wafer at a temperature of not less than 1100° C. and not more than the melting point of silicon for 1 to 60 s in an oxidizing gas atmosphere and then cooling down at a rate of 5 to 150° C./s.

### Claim 3 (depends on 1)

The method of evaluating metal contamination according to claim 1, wherein in the step of measuring a lifetime of the wafer to which contaminants are transferred, lifetime measurement of the wafer is performed after using corona charging as passivation to the silicon wafer.

### Claim 4 (depends on 1)

The method of evaluating metal contamination according to claim 1, wherein lifetime measurement is performed using a μ-PCD apparatus in the step of measuring a lifetime of the silicon wafer to which contaminants are transferred.

### Claim 5 (depends on 1)

The method of evaluating metal contamination according to claim 1, wherein dopant concentration is set to 5×1014 atoms/cm3 or less, in the step of obtaining a silicon single crystal grown by the Czochralski method at a pulling rate of 1.0 mm/min or lower, the crystal having an oxygen concentration of 1.3×1018 atoms/cm3 or less.

### Claim 6 (depends on 1)

The method of evaluating metal contamination according to claim 1, further comprising a step of obtaining concentration y of a metal impurity that is given by substituting measured lifetime values for x of the following expression,
y=(−3.74E07)·x+(2.42E11), Expression 2: