# US 2021/0082771 A1 · Method for forming isolation structure having improved gap-fill capability

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0082771 A1
- Document ID: US20210082771A1
- Status: Published application
- Kind: A1
- Application number: 16/572,109
- Filed: 2019-09-16
- Published: 2021-03-18
- Earliest claimed: 2019-09-16
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Applicants: Taiwan Semiconductor Manufacturing Co., Ltd.
- Inventors: Wan-Yi KAO; Chung-Chi KO; Wei-Jin LI
- Web page: https://patentgrep.com/patent/US20210082771A1

## CPC

- H10D 30/795: {being in lateral device isolation regions, e.g. STI}
- H10D 84/038: {using silicon technology, e.g. SiGe}
- H10D 84/0151: {Manufacturing their isolation regions}
- H10D 84/0158: {the components including FinFETs}
- H10D 84/834: {comprising FinFETs}
- H10P 14/6309: {of silicon in uncombined form, i.e. pure silicon}
- H10P 14/6339: {deposition by cyclic CVD, e.g. ALD, ALE or pulsed CVD}
- H10P 14/6522: {introduced into a nitride material, e.g. changing SiN to SiON}
- H10P 14/6529: {by exposure to a gas or vapour}
- H10P 14/6682: {the compound being a silane, e.g. disilane, methylsilane or chlorosilane}
- H10P 14/69215: {the material being a silicon oxide, e.g. SiO2}
- H10P 14/6922: {the material containing Si, O and at least one of H, N, C, F or other non-metal elements, e.g. SiOC, SiOC:H or SiONC}
- H10P 95/062: {involving a dielectric removal step}
- H10W 10/014: {using trench refilling with dielectric materials, e.g. shallow trench isolations}
- H10W 10/0142: {the dielectric materials being chemical transformed from non-dielectric materials}
- H10W 10/0143: {comprising concurrently refilling multiple trenches having different shapes or dimensions}
- H10W 10/17: formed using trench refilling with dielectric materials, e.g. shallow trench isolations
- H10D 30/797: {being in source or drain regions, e.g. SiGe source or drain}
- H10D 62/822: comprising only Group IV materials heterojunctions, e.g. Si/Ge heterojunctions
- H10D 64/017: {using dummy gates in processes wherein at least parts of the final gates are self-aligned to the dummy gates, i.e. replacement gate processes}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A method for forming a semiconductor structure is provided. The method includes patterning a semiconductor substrate to form a first semiconductor fin and a second semiconductor fin, and depositing a first dielectric material on the first and second semiconductor fins. There is a trench between the first and second semiconductor fins. The method also includes depositing a semiconductor material on the first dielectric material, heating the semiconductor material to cause the semiconductor material to flow to a bottom region of the trench, filling a top region of the trench with a second dielectric material, and heating the first dielectric material, the second dielectric material, and the semiconductor material to form an isolation structure between the first and second semiconductor fins.

## Claims

### Claim 1

A method for forming a semiconductor structure, comprising:
patterning a semiconductor substrate to form a first semiconductor fin and a second semiconductor fin adjacent to the first semiconductor fin;
depositing a first dielectric material on the first semiconductor fin and the second semiconductor fin on the semiconductor substrate, wherein there is a first trench between the first semiconductor fin and the second semiconductor fin;
depositing a semiconductor material on the first dielectric material;
heating the semiconductor material to cause the semiconductor material to flow to a bottom region of the first trench;
filling a top region of the first trench with a second dielectric material; and
heating the first dielectric material, the second dielectric material, and the semiconductor material to form an isolation structure between the first semiconductor fin and the second semiconductor fin.

### Claim 2 (depends on 1)

The method for forming a semiconductor structure as claimed in claim 1, wherein the heating of the semiconductor material to cause the semiconductor material to flow to the bottom region of the first trench comprises:
heating the semiconductor material to a temperature in a range from about 500° C. to about 700° C.

### Claim 3 (depends on 1)

The method for forming a semiconductor structure as claimed in claim 1, wherein the semiconductor material is silicon.

### Claim 4 (depends on 1)

The method for forming a semiconductor structure as claimed in claim 1, wherein the deposition of the semiconductor material and the heating of the semiconductor material to cause the semiconductor material to flow to the bottom region of the first trench are performed in a same chamber.

### Claim 5 (depends on 1)

The method for forming a semiconductor structure as claimed in claim 1, further comprising:
patterning the semiconductor substrate to form a third semiconductor fin, wherein the second semiconductor fin is between the first semiconductor fin and the third semiconductor fin, the first dielectric material is also deposited on the third semiconductor fin on the semiconductor substrate, there is a second trench between the second semiconductor fin and the third semiconductor fin, and a first width of the first trench is smaller than a second width of the second trench.

### Claim 6 (depends on 5)

The method for forming a semiconductor structure as claimed in claim 5, further comprising:
depositing a third dielectric material on the semiconductor substrate after the formation of the isolation structure;
performing a planarization process to remove an upper portion of the third dielectric material to form a dielectric fin between the second semiconductor fin and the third semiconductor fin;
etching back the isolation structure;
forming a gate stack on the isolation structure and across the first semiconductor fin, the second semiconductor fin, the third semiconductor fin and the dielectric fin; and
forming source/drain structures on the first semiconductor fin, the second semiconductor fin and the third semiconductor fin on opposite sides of the gate stack.

### Claim 7 (depends on 6)

The method for forming a semiconductor structure as claimed in claim 6 wherein after the planarization process, a top surface of the dielectric fin is substantially level with top surfaces of the first semiconductor fin, the second semiconductor fin and the third semiconductor fin.

### Claim 8

A method for forming a semiconductor structure, comprising:
patterning a semiconductor substrate to form a first semiconductor fin and a second semiconductor fin adjacent to the first semiconductor fin;
conformally forming a first dielectric material on the first semiconductor fin and the second semiconductor fin on the semiconductor substrate;
conformally forming a silicon-containing material on the first dielectric material;
heating the silicon-containing material to cause at least a portion of the silicon-containing material to flow to a bottom region of a first trench between the first semiconductor fin and the second semiconductor fin;
forming a second dielectric material on the silicon-containing material, wherein the first trench is filled with a portion of the second dielectric material and the portion of the semiconductor material; and
performing an annealing process to react the first dielectric material, the second dielectric material, and the silicon-containing material to form a first isolation structure surrounding the first semiconductor fin and the second semiconductor fin.

### Claim 9 (depends on 8)

The method for forming a semiconductor structure as claimed in claim 8, wherein a silicon-containing structure surrounded by the first isolation structure is formed after the annealing process is performed, a first carbon content of the silicon-containing structure is lower than a second carbon content of the first isolation structure, and a first nitrogen content of the silicon-containing structure is lower than a second nitrogen content of the first isolation structure.

### Claim 10 (depends on 9)

The method for forming a semiconductor structure as claimed in claim 9, wherein the first carbon content of the silicon-containing structure is in a range from about 0.1 w.t. % to about 1 w.t. %, and the first nitrogen content of the silicon-containing structure is in a range from about w.t. % 0.1 to about w.t. % 1.

### Claim 11 (depends on 8)

The method for forming a semiconductor structure as claimed in claim 8, wherein the annealing process is performed with an annealing temperature in a range from about 500° C. to about 700° C.

### Claim 12 (depends on 8)

The method for forming a semiconductor structure as claimed in claim 8, wherein the annealing process is performed with an annealing time in a range from about 1800 seconds to about 7200 seconds.

### Claim 13 (depends on 8)

The method for forming a semiconductor structure as claimed in claim 8, further comprising:
forming a first gate stack and a second gate stack adjacent to the first gate stack on the semiconductor substrate, wherein the first gate stack and the second gate stack are across the first semiconductor fin and the second semiconductor fin, the first dielectric material is also conformally formed on the first gate stack and the second gate stack, there is a second trench between the first gate stack and the second gate stack, a first width of the first trench is smaller than a second width of the second trench, and the first isolation structure is conformally formed on the first gate stack and the second gate stack.

### Claim 14 (depends on 13)

The method for forming a semiconductor structure as claimed in claim 13, further comprising:
forming a shallow trench isolation structure between the first semiconductor fin and the second semiconductor fin before the formation of the first isolation structure; and
anisotropically etching the first isolation structure to form gate sidewall spacers on sidewalls of the first gate stack and sidewalls of the second gate stack, wherein the first isolation structure covers the shallow trench isolation structure during the anisotropic etching of the first isolation structure.

### Claim 15 (depends on 14)

The method for forming a semiconductor structure as claimed in claim 14, further comprising:
forming a source/drain structure on the first semiconductor fin adjacent to the first gate stack;
forming a dielectric layer on the semiconductor substrate, wherein the dielectric layer surrounds the first gate stack and the source/drain structure; and
replacing the first gate stack with a third gate stack that includes a first gate dielectric layer and a first metal gate electrode layer on the first gate dielectric layer.

### Claim 16 (depends on 8)

The method for forming a semiconductor structure as claimed in claim 8, wherein the annealing process is performed in an oxygen-containing atmosphere.

### Claim 17 (depends on 8)

The method for forming a semiconductor structure as claimed in claim 8, wherein the first dielectric material comprises silicon, nitrogen, carbon and oxygen, and the second dielectric material comprises silicon, nitrogen, carbon and oxygen.

### Claim 18

A semiconductor structure, comprising:
a first semiconductor fin and a second semiconductor fin protruding from a semiconductor substrate;
a first isolation structure on the semiconductor substrate between the first semiconductor fin and the second semiconductor fin;
a gate stack on the semiconductor substrate and across the first semiconductor fin and the second semiconductor fin;
source/drain structures on the first semiconductor fin and the second semiconductor fin at opposite sides of the gate stack; and
a silicon-containing structure in the first isolation structure between the first semiconductor fin and the second semiconductor fin, wherein a first carbon content of the silicon-containing structure is lower than a second carbon content of the first isolation structure, and a first nitrogen content of the silicon-containing structure is lower than a second nitrogen content of the first isolation structure.

### Claim 19 (depends on 18)

The semiconductor structure as claimed in claim 18, wherein the first carbon content of the silicon-containing structure is in a range from about 0.1 w.t. % to about 1 w.t. %, and the first nitrogen content of the silicon-containing structure is in a range from about 0.1 w.t. % to about 1 w.t. %.

### Claim 20 (depends on 18)

The semiconductor structure as claimed in claim 18, further comprising:
a second isolation structure between the first isolation structure and the semiconductor substrate.