# US 2021/0082732 A1 · Repulsion mesh and deposition methods

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0082732 A1
- Document ID: US20210082732A1
- Status: Published application
- Kind: A1
- Application number: 17/014,671
- Filed: 2020-09-08
- Published: 2021-03-18
- Earliest claimed: 2019-09-12
- Assignees: Applied Materials, Inc.
- Applicants: Applied Materials, Inc.
- Inventors: Madhu Santosh Kumar Mutyala; Sanjay Kamath; Deenesh Padhi
- Web page: https://patentgrep.com/patent/US20210082732A1

## CPC

- H10P 72/722: {Details of electrostatic chucks}
- C23C 16/401: {containing silicon}
- C23C 16/4408: {by purging residual gases from the reaction chamber or gas lines}
- H01J 37/32715: {Workpiece holder}
- H10P 14/6336: {in the presence of a plasma [PECVD]}
- H10P 14/6514: {by exposure to a plasma}
- H10P 14/6686: {the compound being a molecule comprising at least one silicon-oxygen bond and the compound having hydrogen or an organic group attached to the silicon or oxygen, e.g. a siloxane}
- H10P 14/69215: {the material being a silicon oxide, e.g. SiO2}
- H10P 50/283: {by chemical means}
- H01J 2237/3321: CVD [Chemical Vapor Deposition]
- H01J 2237/334: Etching
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H01J: ELECTRIC DISCHARGE TUBES OR DISCHARGE LAMPS (spark-gaps H01T; electric arc lamps H05B31/00; particle accelerators H05H)

## Abstract

Exemplary deposition methods may include electrostatically chucking a semiconductor substrate at a first voltage within a processing region of a semiconductor processing chamber. The methods may include performing a deposition process. The deposition process may include forming a plasma within the processing region of the semiconductor processing chamber. The methods may include halting formation of the plasma within the semiconductor processing chamber. The methods may include, simultaneously with the halting, increasing the first voltage of electrostatic chucking to a second voltage. The methods may include purging the processing region of the semiconductor processing chamber.

## Claims

### Claim 1

A deposition method comprising:
electrostatically chucking a semiconductor substrate at a first voltage within a processing region of a semiconductor processing chamber performing a deposition process, wherein the deposition process comprises forming a plasma within the processing region of the semiconductor processing chamber;
halting formation of the plasma within the semiconductor processing chamber;
simultaneously with the halting, increasing the first voltage of electrostatic chucking to a second voltage; and
purging the processing region of the semiconductor processing chamber.

### Claim 2 (depends on 1)

The deposition method of claim 1, wherein the first voltage is 200 V or less.

### Claim 3 (depends on 1)

The deposition method of claim 1, wherein the second voltage is 500 V or more.

### Claim 4 (depends on 1)

The deposition method of claim 1, wherein the semiconductor substrate is electrostatically chucked to a substrate support, wherein the semiconductor processing chamber comprises a showerhead, and wherein the deposition process occurs with the semiconductor substrate positioned at a first distance from the showerhead.

### Claim 5 (depends on 4)

The deposition method of claim 4, wherein the substrate support comprises a mesh disposed within the substrate support, and wherein the mesh is characterized by a first mesh density at an interior location of the mesh, and wherein the mesh is characterized by a second mesh density at an exterior location of the mesh surrounding the interior location of the mesh.

### Claim 6 (depends on 4)

The deposition method of claim 4, further comprising:
repositioning the semiconductor substrate to a second distance from the showerhead when the first voltage is increased to the second voltage, wherein the second distance is greater than the first distance.

### Claim 7 (depends on 6)

The deposition method of claim 6, wherein the second distance is more than 25% greater than the first distance.

### Claim 8 (depends on 1)

The deposition method of claim 1, wherein the deposition process comprises depositing silicon oxide using tetraethyl orthosilicate.

### Claim 9

A semiconductor processing chamber comprising:
a pedestal configured to support a semiconductor substrate; and
a conductive mesh incorporated within the pedestal, wherein the conductive mesh is characterized by a first mesh density at a central region of the conductive mesh, and wherein the conductive mesh is characterized by a second mesh density greater than the first mesh density at an exterior region of the conductive mesh.

### Claim 10 (depends on 9)

The semiconductor processing chamber of claim 9, wherein the exterior region of the conductive mesh is characterized by an annular shape encompassing the central region of the conductive mesh.

### Claim 11 (depends on 10)

The semiconductor processing chamber of claim 10, wherein the conductive mesh is characterized by a radius extending from a central axis through the conductive mesh, and wherein the exterior region extends up to about 30% of the radius from an exterior edge of the conductive mesh towards the central axis.

### Claim 12 (depends on 9)

The semiconductor processing chamber of claim 9, wherein the pedestal is configured to vertically translate the semiconductor substrate within the semiconductor processing chamber.

### Claim 13 (depends on 9)

The semiconductor processing chamber of claim 9, further comprising a showerhead configured to operate as a plasma-generating electrode within the semiconductor processing chamber.

### Claim 14

A deposition method comprising:
forming a plasma of an oxygen-containing precursor within a processing region of a semiconductor processing chamber, wherein the processing region houses a semiconductor substrate on a substrate support;
while maintaining the plasma of the oxygen-containing precursor, flowing a silicon-containing precursor into the processing region of the semiconductor processing chamber at a first flow rate;
ramping the first flow rate of the silicon-containing precursor over a period of time to a second flow rate greater than the first flow rate; and
performing a deposition at the second flow rate of the silicon-containing precursor.

### Claim 15 (depends on 14)

The deposition method of claim 14, wherein the silicon-containing precursor comprises tetraethyl orthosilicate.

### Claim 16 (depends on 14)

The deposition method of claim 14, wherein the period of time is less than or about 10 seconds.

### Claim 17 (depends on 14)

The deposition method of claim 14, wherein ramping the first flow rate occurs at a constant increase of from about 2 grams per second of the silicon-containing precursor to about 5 grams per second of the silicon-containing precursor.

### Claim 18 (depends on 14)

The deposition method of claim 14, wherein the deposition is performed at a temperature of less than or about 400° C.

### Claim 19 (depends on 14)

The deposition method of claim 14, wherein the processing region of the semiconductor processing chamber is maintained free of the silicon-containing precursor while forming the plasma of the oxygen-containing precursor.

### Claim 20 (depends on 14)

The deposition method of claim 14, wherein the semiconductor substrate comprises silicon, and wherein forming the plasma of the oxygen-containing precursor produces an oxygen-radicalized surface termination of the silicon of the semiconductor substrate.