# US 2021/0082706 A1 · Methods for Doping High-K Metal Gates for Tuning Threshold Voltages

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0082706 A1
- Document ID: US20210082706A1
- Status: Published application
- Kind: A1
- Application number: 16/572,820
- Filed: 2019-09-17
- Published: 2021-03-18
- Earliest claimed: 2019-09-17
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Applicants: Taiwan Semiconductor Manufacturing Company, Ltd.
- Inventors: Kuo-Feng Yu; Chun Hsiung Tsai; Jian-Hao Chen; Hoong Shing Wong; Chih-Yu Hsu
- Web page: https://patentgrep.com/patent/US20210082706A1

## CPC

- H10D 64/01338: {with a treatment, e.g. annealing, after the formation of the conductor}
- H10D 30/024: {of fin field-effect transistors [FinFET]}
- H10D 64/0134: {with a treatment, e.g. annealing, after the formation of the insulator and before the formation of the conductor}
- H10D 64/017: {using dummy gates in processes wherein at least parts of the final gates are self-aligned to the dummy gates, i.e. replacement gate processes}
- H10D 84/0144: {Manufacturing their gate insulating layers}
- H10D 84/0158: {the components including FinFETs}
- H10D 84/0167: {Manufacturing their channels}
- H10D 84/0193: {the components including FinFETs}
- H10D 84/038: {using silicon technology, e.g. SiGe}
- H10D 84/853: {comprising FinFETs}
- H10P 50/73: {using masks for insulating materials}
- H10P 76/405: {characterised by their composition, e.g. multilayer masks}
- H10P 76/4085: {characterised by the processes involved to create the masks}
- H10D 84/0177: {the gate conductors having different materials or different implants}
- H10D 84/0181: {Manufacturing their gate insulating layers}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A method includes forming a first gate dielectric and a second gate dielectric over a first semiconductor region and a second semiconductor region, respectively, depositing a lanthanum-containing layer including a first portion and a second portion overlapping the first gate dielectric and the second gate dielectric, respectively, and depositing a hard mask including a first portion and a second portion overlapping the first portion and the second portion of the lanthanum-containing layer, respectively. The hard mask is free from both of titanium and tantalum. The method further includes forming a patterned etching mask to cover the first portion of the hard mask, with the second portion of the hard mask being exposed, removing the second portion of the hard mask and the second portion of the lanthanum-containing layer, and performing an anneal to drive lanthanum in the first portion of the lanthanum-containing layer into the first gate dielectric.

## Claims

### Claim 1

A method comprising:
forming a first gate dielectric and a second gate dielectric over a first semiconductor region and a second semiconductor region, respectively;
depositing a lanthanum-containing layer comprising a first portion and a second portion overlapping the first gate dielectric and the second gate dielectric, respectively;
depositing a hard mask comprising a first portion and a second portion overlapping the first portion and the second portion of the lanthanum-containing layer, respectively, wherein the hard mask is free from both of titanium and tantalum;
forming a patterned etching mask to cover the first portion of the hard mask, with the second portion of the hard mask being exposed;
removing the second portion of the hard mask and the second portion of the lanthanum-containing layer; and
performing an anneal to drive lanthanum in the first portion of the lanthanum-containing layer into the first gate dielectric.

### Claim 2 (depends on 1)

The method of claim 1 further comprising:
before the anneal, removing the patterned etching mask; and
removing the first portion of the hard mask.

### Claim 3 (depends on 1)

The method of claim 1, wherein the hard mask is a single-layer hard mask.

### Claim 4 (depends on 1)

The method of claim 1 further comprising, before the forming the patterned etching mask, performing a plasma treatment on the hard mask.

### Claim 5 (depends on 1)

The method of claim 1, wherein the hard mask is a dual-layer hard mask comprising:
a first sub-layer comprising aluminum nitride, aluminum oxide, or zirconium oxide; and
a second sub-layer over the first sub-layer, wherein the second sub-layer comprises tungsten.

### Claim 6 (depends on 1)

The method of claim 1 further comprising forming a non-metal-containing adhesion layer over and contacting the hard mask.

### Claim 7 (depends on 1)

The method of claim 1 further comprising:
after the anneal, removing the first portion of the lanthanum-containing layer.

### Claim 8 (depends on 7)

The method of claim 7 further comprising:
forming a titanium nitride comprising layer comprising a first portion and a second portion over and contacting the first gate dielectric and the second gate dielectric, respectively.

### Claim 9 (depends on 1)

The method of claim 1 further comprising:
removing dummy gate stacks to form a first trench between first gate spacers and a second trench between second gate spacers, wherein the first gate dielectric and the second gate dielectric extend into the first trench and the second trench, respectively.

### Claim 10 (depends on 1)

The method of claim 1, wherein the depositing the lanthanum-containing layer comprises depositing a lanthanum oxide layer.

### Claim 11

A method comprising:
depositing a doping-metal-containing layer comprising a first portion over a first gate dielectric;
depositing a hard mask comprising a first portion over and contacting the first portion of the doping-metal-containing layer, wherein an entirety of the hard mask is formed of a homogenous material;
forming an etching mask comprising a first portion over and contacting the first portion of the hard mask;
performing an anneal process to drive a dopant in the doping-metal-containing layer into the first gate dielectric; and
removing the doping-metal-containing layer.

### Claim 12 (depends on 11)

The method of claim 11, wherein the forming the etching mask comprises dispensing a photo resist over and contacting the hard mask, with a contact angle between the photo resist and the hard mask being smaller than about 10 degrees.

### Claim 13 (depends on 11)

The method of claim 11 further comprising removing the etching mask before the anneal process.

### Claim 14 (depends on 11)

The method of claim 11 further comprising removing the hard mask before the anneal process.

### Claim 15 (depends on 11)

The method of claim 11, wherein the doping-metal-containing layer further comprises a second portion over a second gate dielectric, the hard mask further comprises a second portion over the second portion of the doping-metal-containing layer, and the method further comprises:
before the anneal process, removing the second portion of the hard mask; and
before the anneal process, removing the second portion of the doping-metal-containing layer.

### Claim 16 (depends on 11)

The method of claim 11, wherein the depositing the hard mask comprises depositing an aluminum oxide layer.

### Claim 17

A method comprising:
removing a dummy gate stack to form a trench between gate spacers;
forming a high-k dielectric layer extending into the trench;
depositing a lanthanum oxide layer over the high-k dielectric layer;
depositing a hard mask over the lanthanum oxide layer, wherein the hard mask is a single-layer hard mask;
forming a patterned photo resist over and contacting the hard mask;
patterning the hard mask and the lanthanum oxide layer;
removing the hard mask;
removing the lanthanum oxide layer; and
forming a gate electrode over and contacting the high-k dielectric layer.

### Claim 18 (depends on 17)

The method of claim 17 further comprising, after the removing the hard mask and before the removing the lanthanum oxide layer, performing an anneal process to drive lanthanum into the high-k dielectric layer.

### Claim 19 (depends on 18)

The method of claim 18, wherein the anneal process comprises a spike anneal process performed at a temperature in a range between about 570° C. and about 750° C.

### Claim 20 (depends on 17)