# US 2021/0082598 A1 · Conductive High Strength Extrudable Ultra High Molecular Weight Polymer Graphene Oxide Composite

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0082598 A1
- Document ID: US20210082598A1
- Status: Published application
- Kind: A1
- Application number: 17/012,913
- Filed: 2020-09-04
- Published: 2021-03-18
- Earliest claimed: 2019-09-12
- Assignees: Braskem Research Center
- Applicants: Garmor Inc.
- Inventors: David Restrepo; Alessandro Bernardi; Kevin Herrington; Matthew McInnis; Jeff Bullington
- Web page: https://patentgrep.com/patent/US20210082598A1

## CPC

- H01B 1/24: the conductive material comprising carbon-silicon compounds, carbon or silicon
- B29B 7/002: {Methods (chemical aspects C08J3/00)}
- B29B 7/7461: {Combinations of dissimilar mixers}
- B29B 7/90: Fillers or reinforcements {, e.g. fibres}
- B29B 9/06: in the form of filamentary material, e.g. combined with extrusion
- B29B 9/12: characterised by structure or composition
- B29B 9/16: Auxiliary treatment of granules
- C08J 3/203: {Solid polymers with solid and/or liquid additives}
- C08K 3/04: Carbon
- C08K 3/042: {Graphene or derivatives, e.g. graphene oxides}
- C08L 23/04: Homopolymers or copolymers of ethene
- B29B 7/10: rotary
- B29B 7/42: with screw or helix
- B29B 2009/163: {Coating, i.e. applying a layer of liquid or solid material on the granule}
- B29K 2023/0683: {UHMWPE, i.e. ultra high molecular weight polyethylene}
- B29K 2023/12: {PP, i.e. polypropylene}
- B29K 2105/16: Fillers
- B29K 2509/00: Use of inorganic materials not provided for in groups {B29K2503/00 - B29K2507/00,} as filler
- C08J 2323/06: Polyethene
- C08J 2423/12: Polypropene
- C08K 2201/001: Conductive additives
- C08K 2201/005: Additives being defined by their particle size in general
- C08K 2201/011: Nanostructured additives
- C08K 2201/016: Additives defined by their aspect ratio
- H01B: CABLES; CONDUCTORS; INSULATORS; SELECTION OF MATERIALS FOR THEIR CONDUCTIVE, INSULATING OR DIELECTRIC PROPERTIES (selection for magnetic properties H01F1/00; waveguides H01P {; printed circuits H05K})
- B29B: PREPARATION OR PRETREATMENT OF THE MATERIAL TO BE SHAPED; MAKING GRANULES OR PREFORMS; RECOVERY OF PLASTICS OR OTHER CONSTITUENTS OF WASTE MATERIAL CONTAINING PLASTICS
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS

## Abstract

The present invention includes an injection moldable/extrudable composite that preserves at least 80% or enhances the primary physical properties of compression molded polymer, the composite comprising, e.g., an Ultra High Molecular Weight Polyethylene (UHMWPE) and graphene/graphite oxide or graphene oxide, with or without polypropylene.

## Claims

### Claim 1

An injection moldable/extrudable composite that preserves at least 80% or enhances the primary physical properties of compression molded polymer, the composite comprising a non-extrudable or poorly-extrudable polymer and graphene/graphite oxide or graphene oxide.

### Claim 2 (depends on 1)

The composite of claim 1, wherein the non-extrudable or poorly-extrudable polymer is selected from olefin fibers, Ultra High Molecular Weight Polyethylene (UHMWPE), cross-linked polyethylene (PEX), high-density polyethylene (HDPE), polypropylene, linear low-density polyethylene (LLDPE), low-density polyethylene (LDPE), medium-density polyethylene (MDPE), para-aramid fibers, and/or polyoxazole fibers.

### Claim 3 (depends on 2)

The composite of claim 2, wherein the physical properties of a compression molded UHMWPE, and a resistivity less than 1011 Ohm-cm.

### Claim 4 (depends on 2)

The composite of claim 2, wherein the UHMWPE has a molecular weight between 500,000 and 16,000,000 Daltons or between 2,000,000 and 8,000,000 Daltons.

### Claim 5 (depends on 1)

The composite of claim 1, wherein the composite has a graphene oxide is 0.1 wt %, 0.5 wt %, 1.0 wt %, 1.25 wt %, 1.5 wt %, 1.75 wt %, 2.0 wt %, 2.25 w %, 2.5 w %, 2.75 wt %, 3.0 wt %, 3.25 wt %, 3.5 wt %, 3.75 wt %, 4.0 wt %, 4.25 wt %, 4.5 wt %, 4.75 wt %, 5.0 wt %, 6.0 wt %, 7.0 wt %, 8.0 wt %, 9.0 wt %, 10 wt %, 11 wt %, 12 wt %, 13 wt %, 14 wt %, 15 wt %, 16 wt %, 17 wt %, 18 wt %, 19 wt %, or 20 wt % relative to UHMWPE; or
the composite has a polypropylene loading is 0.1 wt %, 0.5 wt %, 1.0 wt %, 1.25 wt %, 1.5 wt %, 1.75 wt %, 2.0 wt %, 2.25 w %, 2.5 w %, 2.75 wt %, 3.0 wt %, 3.25 wt %, 3.5 wt %, 3.75 wt %, 4.0 wt %, 4.25 wt %, 4.5 wt %, 4.75 wt %, 5.0 wt %, 6.0 wt %, 7.0 wt %, 8.0 wt %, 9.0 wt %, 10 wt %, 11 wt %, 12 wt %, 13 wt %, 14 wt %, 15 wt %, 16 wt %, 17 wt %, 18 wt %, 19 wt %, or 20 wt % relative to UHMWPE.

### Claim 6 (depends on 1)

The composite of claim 1, wherein the graphene/graphite oxide are graphene/graphite oxide flakes with a surface area to thickness ratio greater than 300 Angstroms, and thickness of less than 160 Angstroms, wherein the graphene flakes have no significant physical surface distortions, no significant epoxy functionalization, and have an oxidation level greater than 0.5% by mass.

### Claim 7 (depends on 1)

The composite of claim 1, wherein at least one of: a mechanical, an electrical, or a thermal physical property of the polymer is enhanced or sustained with the addition of the graphene/graphite oxide or graphene oxide when compared to the polymer without the graphene/graphite oxide or graphene oxide.

### Claim 8 (depends on 1)

The composite of claim 1, wherein at least one of: 95% of the graphene/graphite oxide are flakes with a thickness of about 0.8 to 20 nanometers; the polymer is a UHMWPE in a powder with a particle size between 15 μm and 1,000 μm; or the polymer is a polypropylene in a powder with a particle size between 100 μm and 2,500 μm.

### Claim 9

A method of making a non-extrudable or poorly-extrudable polymer/graphene (G) and/or graphene oxide (GO) composite that is extrudable and injection moldable and preserves or enhances at least one mechanical, electrical, or thermal physical property relative to a compression molded version of non-extrudable or poorly-extrudable polymer/GO composite comprising:
mixing a powder or pellets of the non-extrudable or poorly-extrudable polymer with between 0.01 wt % and 20 wt % graphene and/or graphene oxide under conditions in which the polymer powder or pellets and the graphene and/or graphene oxide are substantially mixed.

### Claim 10 (depends on 9)

The method of claim 9, wherein the non-extrudable or poorly-extrudable polymer is selected from olefin fibers, Ultra High Molecular Weight Polyethylene (UHMWPE), cross-linked polyethylene (PEX), high-density polyethylene (HDPE), polypropylene, linear low-density polyethylene (LLDPE), low-density polyethylene (LDPE), medium-density polyethylene (MDPE), para-aramid fibers, and/or polyoxazole fibers.

### Claim 11 (depends on 9)

The method of claim 9, wherein the physical properties of a compression molded non-extrudable or poorly-extrudable polymer comprises a resistivity less than 1011 Ohm-cm.

### Claim 12 (depends on 9)

The method of claim 9, wherein the non-extrudable or poorly-extrudable polymer is UHMWPE with a molecular weight between 500,000 and 16,000,000 Daltons or between 2,000,000 and 8,000,000 Daltons.

### Claim 13 (depends on 9)

The method of claim 9, wherein the composite has a graphene oxide is 0.1 wt %, 0.5 wt %, 1.0 wt %, 1.25 wt %, 1.5 wt %, 1.75 wt %, 2.0 wt %, 2.25 w %, 2.5 w %, 2.75 wt %, 3.0 wt %, 3.25 wt %, 3.5 wt %, 3.75 wt %, 4.0 wt %, 4.25 wt %, 4.5 wt %, 4.75 wt %, 5.0 wt %, 6.0 wt %, 7.0 wt %, 8.0 wt %, 9.0 wt %, 10 wt %, 11 wt %, 12 wt %, 13 wt %, 14 wt %, 15 wt %, 16 wt %, 17 wt %, 18 wt %, 19 wt %, or 20 wt % relative to UHMWPE;
the composite has a polypropylene loading is 0.1 wt %, 0.5 wt %, 1.0 wt %, 1.25 wt %, 1.5 wt %, 1.75 wt %, 2.0 wt %, 2.25 w %, 2.5 w %, 2.75 wt %, 3.0 wt %, 3.25 wt %, 3.5 wt %, 3.75 wt %, 4.0 wt %, 4.25 wt %, 4.5 wt %, 4.75 wt %, 5.0 wt %, 6.0 wt %, 7.0 wt %, 8.0 wt %, 9.0 wt %, 10 wt %, 11 wt %, 12 wt %, 13 wt %, 14 wt %, 15 wt %, 16 wt %, 17 wt %, 18 wt %, 19 wt %, or 20 wt % relative to UHMWPE; or the polypropylene is a powder and has a particle size between 100 μm and 2,500 μm.

### Claim 14 (depends on 9)

The method of claim 9, wherein the graphene/graphite oxide are graphene/graphite oxide flakes with a surface area to thickness ratio greater than 300 Angstroms, and thickness of less than 160 Angstroms, wherein the graphene flakes have no significant physical surface distortions, no significant epoxy functionalization, and have an oxidation level greater than 0.5% by mass.

### Claim 15 (depends on 9)

The method of claim 9, wherein at least 95% of the graphene/graphite oxide are flakes with a thickness of about 0.8 to 20 nanometers; or the polymer is a UHMWPE in a powder with a particle size between 15 μm and 1,000 μm.

### Claim 16 (depends on 9)

The method of claim 9, further comprising at least one of:
heating a UHMWPE/GO/PP composite during the mixing step;
coating a UHMWPE powder with graphene or graphite oxide by combining the UHMWPE powder and the graphene or graphite oxide powder in a high shear mixer for more than 1 minutes and less than 60 minutes;
adding a polypropylene powder to a graphene or graphite oxide coated UHMWPE powder and combining in a high shear mixer for more than 1 minutes and less than 60 minutes;
placing a UHMWPE/GO/PP powder mix into an extruder to produce pellets for use in injection molding;
obtaining graphene/graphite oxide flakes formed in a stirred media mill, and the stirred media mill is an Attrition mill or ball mill; or
extruding the composite in a cylinder at a temperature between 200° C. to 250° C.; with a melt temperature between 180° C. and 400° C. preferable 200° C. and 240° C.; and a screw speed between 60 to 300 rpm.

### Claim 17 (depends on 9)

The method of claim 9, wherein at least one of a mechanical, electrical, or thermal physical property of the cementitious composite is enhanced with the addition of the graphene/graphite oxide.

### Claim 18 (depends on 9)

The method of claim 9, wherein at least 95% of the graphene/graphite oxide flakes have a surface area to thickness ratio of a minimum of 300 Angstroms; or wherein the graphene/graphite oxide flake has primarily edge oxidation.

### Claim 19 (depends on 9)

The method of claim 9, wherein the non-extrudable or poorly-extrudable polymer/graphene (G) and/or graphene oxide (GO) composite comprises:
mixing a powder or pellets of the non-extrudable or poorly-extrudable polymer with between 0.01 wt % and 20 wt % graphene and/or graphene oxide under conditions in which the polymer powder or pellets and the graphene and/or graphene oxide are substantially mixed; and
extruding or injection molding the composite into a shape, wherein the extrudable and injection moldable and preserves or enhances at least one mechanical, electrical, or thermal physical property relative to a compression molded version of non-extrudable or poorly-extrudable polymer/GO composite.

### Claim 20

An injection moldable/extrudable composite that preserves at least 80% or enhances the primary physical properties of compression molded polymer, the composite comprising an Ultra High Molecular Weight Polyethylene (UHMWPE) and graphene/graphite oxide or graphene oxide.