# US 2021/0082597 A1 · Conductive film manufacturing method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0082597 A1
- Document ID: US20210082597A1
- Status: Published application
- Kind: A1
- Application number: 16/954,268
- Filed: 2018-12-19
- Published: 2021-03-18
- Earliest claimed: 2017-12-22
- Assignees: Mitsui Mining & Smelting Co., Ltd.
- Applicants: Mitsui Mining & Smelting Co., Ltd.
- Inventors: Kei ANAI; Shun FUKUZATO
- Web page: https://patentgrep.com/patent/US20210082597A1

## CPC

- H01B 1/22: the conductive material comprising metals or alloys
- C09D 5/24: Electrically-conducting paints {(conductive materials H01B1/00)}
- C09D 201/00: Coating compositions based on unspecified macromolecular compounds
- C23C 26/00: Coating not provided for in groups C23C2/00 - C23C24/00
- H01B 13/00: Apparatus or processes specially adapted for manufacturing conductors or cables
- H01B: CABLES; CONDUCTORS; INSULATORS; SELECTION OF MATERIALS FOR THEIR CONDUCTIVE, INSULATING OR DIELECTRIC PROPERTIES (selection for magnetic properties H01F1/00; waveguides H01P {; printed circuits H05K})
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

Provided is a method for manufacturing a conductive film, including forming a coating of a composition that contains conductivity-imparting particles and photo-sintering the coating, wherein, prior to the photo-sintering of the coating, the coating is compressed in the thickness direction thereof. It is preferable that the coating be compressed at a temperature at which a binding agent contained in the composition shows a storage modulus of 100 MPa or less. It is also preferable that the coating be compressed so that the compression rate in the thickness direction is from 25% to 80%. It is preferable that, in the photo-sintering step, the light irradiation be performed through irradiation with pulsed light.

## Claims

### Claim 1

A method for manufacturing a conductive film, comprising:
forming a coating of a composition that contains conductivity-imparting particles; and
photo-sintering the coating,
wherein, prior to the photo-sintering of the coating, the coating is compressed in a thickness direction thereof.

### Claim 2 (depends on 1)

The method according to claim 1,
wherein the coating is compressed at a temperature at which a binding agent contained in the composition shows a storage modulus of 100 MPa or less.

### Claim 3 (depends on 1)

The method according to claim 1,
wherein the coating is compressed so that a compression rate in the thickness direction is from 25% to 80%.

### Claim 4 (depends on 2)

The method according to claim 2,
wherein the coating is compressed so that a compression rate in the thickness direction is from 25% to 80%.