# US 2021/0080846 A1 · Toner

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0080846 A1
- Document ID: US20210080846A1
- Status: Published application
- Kind: A1
- Application number: 17/012,889
- Filed: 2020-09-04
- Published: 2021-03-18
- Earliest claimed: 2019-09-13
- Assignees: Canon Kabushiki Kaisha
- Applicants: Canon Kabushiki Kaisha
- Inventors: Takuya Mizuguchi; Yoshitaka Suzumura; Hiroyuki Tomono; Osamu Matsushita; Shuntaro Watanabe; Hiroki Akiyama; Hiroki Kagawa
- Web page: https://patentgrep.com/patent/US20210080846A1

## CPC

- G03G 9/08755: {Polyesters}
- G03G 9/08711: {with esters of acrylic or methacrylic acid}
- G03G 9/08782: {Waxes}
- G03G 9/08793: {Crosslinked polymers}
- G03G 9/08795: {characterised by their chemical properties, e.g. acidity, molecular weight, sensitivity to reactants}
- G03G 9/08797: {characterised by their physical properties, e.g. viscosity, solubility, melting temperature, softening temperature, glass transition temperature}
- G03G: ELECTROGRAPHY; ELECTROPHOTOGRAPHY; MAGNETOGRAPHY

## Abstract

A toner comprising a toner particle including a binder resin, wherein in a temperature T (° C.)-storage elastic modulus G′ (Pa) curve obtained by measuring the toner with a rheometer, a storage elastic modulus G′ (80° C.) at 80° C. is from 2.0×103 Pa to 2.0×105 Pa; and a local minimum value of a change amount (dG′/dT) of a storage elastic modulus G′ in a range of 60° C. to 80° C. with respect to a temperature T is −1.0×106 or less, and when the temperature of the toner is raised, where a projected area of the toner at 80° C. is S1 (μm2), a radius of the projected area of the toner at 80° C. is R1 (μm), and a projected area of the toner at 120° C. is S2 (μm2), the S1, R1 and S2 satisfy a following formula (1): S2/S1×1/R1≤0.22. (1)

## Claims

### Claim 1

A toner comprising a toner particle including a binder resin, wherein in a temperature T (° C.)-storage elastic modulus G′ (Pa) curve obtained at a temperature rise rate of 2.0° C./min by measuring the toner with a rotating plate rheometer,
(i) a storage elastic modulus G′ (80° C.) at 80° C. is from 2.0×103 Pa to 2.0×105 Pa; and
(ii) a local minimum value of a change amount (dG′/dT) of a storage elastic modulus G′ in a range of 60° C. to 80° C. with respect to a temperature T is −1.0×106 or less, and
when the temperature of the toner is raised from 25° C. to 120° C. at a temperature rise rate of 10° C./min, where a projected area of the toner at 80° C. is S1 (μm2), a radius of the projected area of the toner at 80° C. is R1 (μm), and a projected area of the toner at 120° C. is S2 (μm2),
the S1, R1 and S2 satisfy a following formula (1):
S2/S1×1/R1≤0.22. (1)

### Claim 2 (depends on 1)

The toner according to claim 1, wherein in the temperature T (° C.)-storage elastic modulus G′ (Pa) curve,
a storage elastic modulus G′ (120° C.) at 120° C. is from 2.0×103 Pa to 2.0×104 Pa.

### Claim 3 (depends on 1)

The toner according to claim 1, wherein when the toner is extracted by Soxhlet extraction using tetrahydrofuran for 18 hours, the toner includes a tetrahydrofuran-insoluble matter, and
a storage elastic modulus G′ (120° C.) at 120° C. measured at a temperature rise rate of 2.0° C./min by measuring the tetrahydrofuran-insoluble matter with a rotating plate rheometer is from 1.0×105 Pa to 1.0×107 Pa.

### Claim 4 (depends on 1)

The toner according to claim 1, wherein
where an amount of an ethyl acetate-insoluble matter of the toner, when the toner is extracted for 18 hours by Soxhlet extraction using ethyl acetate, is α (% by mass), and
an amount of a tetrahydrofuran-insoluble matter of the toner, when the toner is extracted for 18 hours by Soxhlet extraction using tetrahydrofuran, is β (% by mass),
the α and the β satisfy following formulas (2) and (3):
5.0≤≤β≤30.0 (2)
10.0≤(α-β)≤40.0. (3)

### Claim 5 (depends on 1)

The toner according to claim 1, wherein the binder resin includes a hybrid resin having a vinyl polymer segment and an amorphous polyester segment.

### Claim 6 (depends on 5)

The toner according to claim 5, wherein
the vinyl polymer segment has a structure in which at least one selected from the group consisting of an acrylic acid ester and a methacrylic acid ester is polymerized, and
a total amount of the structure in which at least one selected from the group consisting of an acrylic acid ester and a methacrylic acid ester is polymerized in the vinyl polymer segment is from 50% by mass to 98% by mass.

### Claim 7 (depends on 5)

The toner according to claim 5, wherein the amount of the amorphous polyester segment in the hybrid resin is from 50% by mass to 98% by mass.

### Claim 8 (depends on 5)

The toner according to claim 5, wherein the amorphous polyester segment has a structure crosslinked by at least one selected from the group consisting of a trihydric or higher polyhydric alcohol and a trivalent or higher polycarboxylic acid.

### Claim 9 (depends on 1)

The toner according to claim 1, wherein
the toner particle includes a crystalline polyester,
the crystalline polyester is a polycondensation product of an alcohol component including an aliphatic diol and an acid component including an aliphatic dicarboxylic acid, and
when a carbon number of the aliphatic diol is C1, and a carbon number of the aliphatic dicarboxylic acid is C2, a sum of C1 and C2 is from 10 to 16.

### Claim 10 (depends on 1)

The toner according to claim 1, wherein
in the differential scanning calorimeter (DSC) measurement of the toner, when
(i) the number of cold crystallization peaks in a range of from 40° C. to 120° C. at a time of lowering temperature is X, and
(ii) the number of endothermic peaks in a range of from 40° C. to 120° C. at a time of a second temperature rise is Y,
X and Y satisfy following formulas (7) and (8):
X≥1 (7)
Y≥X+1. (8)

### Claim 11 (depends on 1)

The toner according to claim 1, wherein
the toner particle includes a crystalline polyester resin, and
in differential scanning calorimetry of the toner,
a temperature is raised from 25° C. to 120° C. at a rate of 1000° C./sec,
the temperature is held at 120° C. for 100 msec and then cooling is performed to 25° C. at a rate of 1000° C./sec, and then
the temperature is raised to 120° C. at a rate of 1000° C./sec, and
when a glass transition temperature at a first temperature rise is Tg1 (° C.), and a glass transition temperature at a second temperature rise is Tg2 (° C.),
following formulas (9) and (10) are satisfied:
65° C.≤Tg1≤85° C. (9)
7° C.≤Tg1-Tg2≤30° C. (10)

### Claim 12 (depends on 1)

The toner according to claim 1, wherein
in the temperature T (° C.)-storage elastic modulus G′ (Pa) curve, a temperature at which the storage elastic modulus is 1.0×103 Pa is T1 (° C.),
in a DSC curve obtained by differential scanning calorimetry of the toner, an endothermic peak exists in a range of from 30° C. to 120° C., and
when a peak temperature of a peak present on a lowest temperature side of the endothermic peak is T2 (° C.),
a following formula (11) is satisfied:
T1-T2≥40. (11)