- Inventors: Deok Hwan Kim; Yeon Keun Lee; Jung Doo Kim; Jun Haeng Lee
- Web page: https://patentgrep.com/patent/US20210080768A1

## CPC

- G02F 1/1375: {using dynamic scattering}
- C09K 19/02: characterised by optical, electrical or physical properties of the components, in general
- G02F 1/1337: Surface-induced orientation of the liquid crystal molecules, e.g. by alignment layers
- G02F 1/13725: {based on guest-host interaction (G02F1/13762, G02F1/13737, take precedence)}
- G02F 1/133742: {for homeotropic alignment}
- G02F 1/13712: {the liquid crystal having negative dielectric anisotropy}
- G02F 2202/06: dopant
- G02F: OPTICAL DEVICES OR ARRANGEMENTS FOR THE CONTROL OF LIGHT BY MODIFICATION OF THE OPTICAL PROPERTIES OF THE MEDIA OF THE ELEMENTS INVOLVED THEREIN; NON-LINEAR OPTICS; FREQUENCY-CHANGING OF LIGHT; OPTICAL LOGIC ELEMENTS; OPTICAL ANALOGUE/DIGITAL CONVERTERS
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE

## Abstract

A liquid crystal cell and a manufacturing method thereof and a use thereof are provided in the present disclosure. The liquid crystal cell is in a normally transparent mode, and has excellent transmittance-variable characteristics in a transparent mode and a scattering mode and excellent haze characteristics in the scattering mode. Such liquid crystal cell may be applied to various light modulation devices such as a smart window, a window protective film, a flexible display element, a light shielding plate for transparent displays, an active retarder for 3D image displays or a viewing angle control film.

## Claims

### Claim 1

A liquid crystal cell comprising:
two substrates disposed opposite to each other; and
a liquid crystal layer present between the two substrates, wherein upon measuring current densities over time, a current density peak appears after 2 ms, wherein the current densities are measured during a positive half cycle after a fifth cycle and the current densities are measured by applying an alternating-current voltage at a first voltage of 40 V and a frequency of 20 Hz to 120 Hz to the liquid crystal cell, and the current density peak is a maximum value of the current densities appeared after 0.5 ms).

### Claim 2 (depends on 1)

The liquid crystal cell according to claim 1, wherein the liquid crystal layer comprises non-reactive liquid crystals and a conductivity control agent.

### Claim 3 (depends on 2)

The liquid crystal cell according to claim 2, wherein the non-reactive liquid crystals have negative dielectric constant anisotropy.

### Claim 4 (depends on 2)

The liquid crystal cell according to claim 2, wherein the conductivity control agent comprises one or more selected from an anisotropic dye, reactive liquid crystals or an ionic compound.

### Claim 5 (depends on 2)

The liquid crystal cell according to claim 2, wherein the conductivity control agent is included in a ratio of 0.1 parts by weight to 30 parts by weight relative to 100 parts by weight of the non-reactive liquid crystals.

### Claim 6 (depends on 1)

The liquid crystal cell according to claim 1, wherein the liquid crystal layer has a transparent mode in an initial state and a scattering mode at the time of applying a second voltage.

### Claim 7 (depends on 6)

The liquid crystal cell according to claim 6, wherein the liquid crystal layer has a difference of 40% or more between transmittance in the initial state and transmittance at the time of applying the second voltage of 60 V.

### Claim 8 (depends on 6)

The liquid crystal cell according to claim 6, wherein the liquid crystal layer has haze of 90% or more at the time of applying the second voltage of 60 V.

### Claim 9 (depends on 1)

The liquid crystal cell according to claim 1, wherein the two substrates each comprise an electrode layer and a vertical alignment film.

### Claim 10

A method for manufacturing a liquid crystal cell comprising two substrates disposed opposite to each other and a liquid crystal layer present between the two substrates, wherein the method comprises:
adjusting the liquid crystal layer so that upon measuring current densities of the liquid crystal layer over time, the current density peak appears after 2 ms, wherein the current densities are measured during a positive half cycle after a fifth cycle and the current densities are measured by applying an alternating-current voltage at a voltage of 40 V and a frequency of 20 Hz to 120 Hz to the liquid crystal cell, and the current density peak is a maximum value of the current densities appeared after 0.5 ms.

### Claim 11 (depends on 10)

The method for manufacturing a liquid crystal cell according to claim 10, wherein the liquid crystal cell is manufactured by injecting a heated liquid crystal composition between the two substrates and sealing the edges of the heated liquid crystal composition injected between the substrates.

### Claim 12 (depends on 11)

The method for manufacturing a liquid crystal cell according to claim 11, wherein the liquid crystal composition comprises non-reactive liquid crystals and a conductivity control agent, wherein the conductivity control agent comprises an anisotropic dye and reactive liquid crystals, wherein the liquid crystal composition is heated a temperature of 100° C. to 120° C. for 25 hours to 30 hours.

### Claim 13 (depends on 11)

The method for manufacturing a liquid crystal cell according to claim 11, wherein the liquid crystal composition comprises:
non-reactive liquid crystals; and
a conductivity control agent, wherein the conductivity control agent comprise an anisotropic dye, reactive liquid crystals and an ionic compound, and when the reactive liquid crystals are included in an amount of 2.5 wt % to 7.5 wt % in the liquid crystal composition, and the liquid crystal composition is heated at a temperature of 100° C. to 120° C. for 30 minutes to 15 hours.

### Claim 14 (depends on 11)

The method for manufacturing a liquid crystal cell according to claim 11, wherein the liquid crystal composition comprises:
non-reactive liquid crystals and
a conductivity control agent comprising an anisotropic dye, reactive liquid crystals and an ionic compound, and when the reactive liquid crystals are included in an amount of 7.5 wt % to 12.5 wt % in the liquid crystal composition, the liquid crystal composition is heated at a temperature of 100° C. to 120° C. for 30 minutes to 4 hours.

### Claim 15 (depends on 1)

An optical modulation device comprising the liquid crystal cell of claim 1.