# US 2021/0080437 A1 · Method for Evaluating Properties of Melt-Blown Plastic Resin

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0080437 A1
- Document ID: US20210080437A1
- Status: Published application
- Kind: A1
- Application number: 16/645,298
- Filed: 2018-09-11
- Published: 2021-03-18
- Earliest claimed: 2017-09-15
- Assignees: LG Chem, Ltd.
- Applicants: LG Chem, Ltd.
- Inventors: Hyunsup Lee; Seok Hwan Kim; Heekwang Park; Ki Soo Lee; SangJin Jeon; Myunghan Lee
- Web page: https://patentgrep.com/patent/US20210080437A1

## CPC

- G01N 30/88: Integrated analysis systems specially adapted therefor, not covered by a single one of the groups G01N30/04 - G01N30/86
- D01D 5/0985: {by means of a flowing gas (e.g. melt-blowing)}
- G01N 33/442: {Resins; Plastics}
- D01F 6/06: from polypropylene
- G01N 2030/027: {Liquid chromatography}
- G01N: INVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIR CHEMICAL OR PHYSICAL PROPERTIES (measuring or testing apparatus or processes other than immunoassay, involving enzymes or microorganisms C12M, C12Q)
- D01D: MECHANICAL METHODS OR APPARATUS IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS, THREADS, FIBRES, BRISTLES OR RIBBONS
- D01F: CHEMICAL FEATURES IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS, THREADS, FIBRES, BRISTLES OR RIBBONS; APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OF CARBON FILAMENTS

## Abstract

A method for evaluating physical properties of a melt-blown plastic resin, and, more specifically, a novel method for evaluating physical properties are provided. When a particular plastic resin is processed by a melt-blown process, a stretching diameter value after the process of the plastic resin can be accurately derived from a physical property value measured using a specimen of the resin.

## Claims

### Claim 1

A method for evaluating physical properties of a melt-blown plastic resin comprising:
measuring a molecular weight distribution for a plastic resin specimen;
deriving a peak molecular weight value from the molecular weight distribution;
deriving a molecular weight distribution value (Mw/Mn) from the molecular weight distribution; and
predicting a stretching diameter of the plastic resin specimen manufactured from a melt-blown process using the peak molecular weight value and the molecular weight distribution value.

### Claim 2 (depends on 1)

The method according to claim 1, wherein
when the molecular weight distribution of the plastic resin specimens is measured by GPC/SEC, the peak molecular weight value is a molecular weight value corresponding to a largest peak.

### Claim 3 (depends on 1)

The method according to claim 1, wherein
the melt-blown process is performed under the temperature condition of 150° C. to 250° C.

### Claim 4 (depends on 1)

The method according to claim 1, wherein
the melt-blown process is performed at a longitudinal stretch ratio of 100 times to 10,000 times.

### Claim 5 (depends on 1)

The method according to claim 1, wherein
predicting the stretching diameter comprises:
deriving a polymer characteristic factor using Mathematical Formula 1 below.
Polymer Characteristic Factor=a(MWD)b*(Mp)c [Mathematical Formula 1]
in Mathematical Formula 1,
MWD is the molecular weight distribution value (Mw/Mn),
Mp is the peak molecular weight value,
a is 0.01 to 0.02,
b is 0.8 to 1.0, and
c is 0.20 to 0.22.

### Claim 6 (depends on 5)

The method according to claim 5, wherein
predicting the stretching diameter comprises;
predicting a stretching diameter from the polymer characteristic factor using Mathematical Formula 2 below.
Predicted Stretching Diameter=d*(Polymer Characteristic Factor)−e [Mathematical Formula 2]
in Mathematical Formula 2,
d is 1.01 to 1.02, and
e is 0.005 to 0.007.

### Claim 7 (depends on 1)

The method according to claim 1, wherein
the peak molecular weight value is 10.000 g/mol to 150,000 g/mol.

### Claim 8 (depends on 1)

The method according to claim 1, wherein
the molecular weight distribution value is 4 or less.

### Claim 9 (depends on 1)

The method according to claim 1, wherein
the plastic resin has a number average molecular weight value (Mn) of 10,000 g/mol to 50,000 g/mol.

### Claim 10 (depends on 1)

The method according to claim 1, wherein
the plastic resin has a weight average molecular weight value (Mw) of 10,000 g/mol to 200,000 g/mol.

### Claim 11 (depends on 1)

The method according to claim 1, wherein
the plastic resin is a polypropylene resin.