# US 2021/0079940 A1 · Method of gluing metal parts

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0079940 A1
- Document ID: US20210079940A1
- Status: Published application
- Kind: A1
- Application number: 17/017,327
- Filed: 2020-09-10
- Published: 2021-03-18
- Earliest claimed: 2019-09-12
- Assignees: Braun GmbH
- Applicants: Braun GmbH
- Inventors: Dieter Groß; Marcel Denis Knorr; Arne Schmidt
- Web page: https://patentgrep.com/patent/US20210079940A1

## CPC

- F16B 11/006: {by gluing (gluing of plastics material B29C65/48)}
- B23K 26/0624: {using ultrashort pulses, i.e. pulses of 1 ns or less}
- B23K 26/36: Removing material (B23K26/55, B23K26/57 take precedence)
- C09J 5/02: involving pretreatment of the surfaces to be joined
- A61C 17/22: with brushes, cushions, cups, or the like (brush bodies, e.g. arrangements of the bristles A46B)
- B23K 2101/20: Tools
- B23K 2103/04: Steel {or steel} alloys
- C09J 2301/416: use of irradiation
- C09J 2400/163: in the substrate
- C09J 2400/166: in the pretreated surface to be joined
- C09J 2463/00: Presence of epoxy resin
- F16B: DEVICES FOR FASTENING OR SECURING CONSTRUCTIONAL ELEMENTS OR MACHINE PARTS TOGETHER, e.g. NAILS, BOLTS, CIRCLIPS, CLAMPS, CLIPS OR WEDGES; JOINTS OR JOINTING (couplings for transmitting rotation F16D)
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- C09J: ADHESIVES; NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL; ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE; USE OF MATERIALS AS ADHESIVES (preparation of glue or gelatine C09H)
- A61C: DENTISTRY; APPARATUS OR METHODS FOR ORAL OR DENTAL HYGIENE (non-driven toothbrushes A46B; {tongue scrapers A61B17/24;} preparations for dentistry A61K6/00; preparations for cleaning the teeth or mouth A61K8/00, A61Q11/00)

## Abstract

A method of gluing a metal part to another part for use in a personal care device such as an electric toothbrush. The method includes steps of providing a metal, such as steel, part, and another, metal, part; treating a surface portion of the metal part with ultra-fast laser pulses having a pulse length in the femtosecond range, e.g., from about 1 femtosecond to about 990 femtoseconds, so that a surface layer of the metal surface is removed; applying an adhesive to the treated surface of the metal part or to a surface of the other part; and gluing the metal part and the other part together.

## Claims

### Claim 1

A method of gluing a metal part to another part, the metal part and the other part being structured and configured for use in an electric toothbrush, the method comprising the steps of:
providing a first metal part and a second part;
treating a surface portion of the first metal part with ultra-fast laser pulses having a pulse length in the femtosecond range of from 1 femtosecond to 990 femtoseconds, so that a surface layer of the metal surface is removed;
applying an adhesive to the treated surface of the first metal part or to a surface of the second part; and
gluing the first metal part and the second part together.

### Claim 2 (depends on 1)

The method of claim 1, wherein the step of applying an adhesive includes applying an epoxide adhesive comprising a two-component, room-temperature-curing epoxide adhesive.

### Claim 3 (depends on 1)

The method of claim 1, wherein the second part is another metal part, and the method includes the step of treating a surface portion of the second part that is intended for being glued to the first metal part with laser pulses comprising ultra-fast or fast laser pulses having a pulse length in the femtosecond or picosecond or nanosecond range.

### Claim 4 (depends on 1)

The method of claim 1, wherein the first metal part is at least partially cylindrical and wherein the method includes rotating the first metal part while applying the ultra-fast laser pulses.

### Claim 5 (depends on 1)

The method of claim 1, wherein the step of treating the surface with ultra-fast laser pulses includes forming laser-induced quasi-periodic or periodic surface structures.

### Claim 6 (depends on 5)

The method of claim 5, wherein the step of forming laser-induced periodic surface structures includes applying the laser pulses along a sand-clock type path.

### Claim 7 (depends on 1)

The method of claim 1, comprising the step of treating a portion of the surface of the first metal part that comprises the portion of the surface intended for being treated with ultra-short laser pulses and that comprises a portion of the surface adjoining the portion of the surface intended for being treated with ultra-short laser pulses with a plasma to at least immobilize layers of volatile organic compounds on the treated metal surface, wherein the plasma is an atmospheric-pressure plasma.

### Claim 8 (depends on 1)

The method of claim 1, wherein the laser light fluence on the laser-treated surface portion is in a range selected from the group consisting of a range of between 1 J/cm2 and 10 J/cm2 and a range of between 5 J/cm2 and 8 J/cm2.

### Claim 9 (depends on 1)

The method of claim 1, wherein an energy per pulse is in a range selected from the group consisting of an energy of between 20 μJ and 100 μJ and an energy of between 30 μJ and 80 μJ.

### Claim 10 (depends on 1)

The method of claim 1, wherein a frequency at which the ultra-fast laser pulses are applied is in a range selected from the group consisting of a frequency of between 100 kHz and 800 kHz, a frequency of between 300 kHz and 500 kHz, and a frequency of about 400 kHz.

### Claim 11 (depends on 1)

The method of claim 1, wherein a wavelength of the laser is in a range selected from the group consisting of a wavelength of between 930 nm and 1064 nm and a wavelength of about 1030 nm.

### Claim 12 (depends on 1)

The method of claim 1, wherein the ultra-fast laser pulses have a spot diameter of from 30 μm to 80 μm.

### Claim 13 (depends on 1)

The method of claim 1, wherein the laser pulses applied onto the surface portion overlap one another by about 70%.

### Claim 14

A method of manufacturing a personal care device comprising the step of gluing a steel shaft into a metal cup, the method comprising the steps of:
providing the steel shaft and the metal cap sized to receive at least a tip region of the steel shaft;
treating a surface portion of the steel shaft intended for being glued to the other part with ultra-fast laser pulses having a pulse length in the femtosecond range comprising the range of from 1 femtosecond to 990 femtoseconds, so that a surface layer from the metal surface is removed;
treating at least a portion of an inner surface of the metal cap intended for being bonded with the respective surface portion of the steel shaft with fast or ultra-fast laser pulses;
applying an adhesive to the treated surface portion of at least one of the steel shaft or the metal cap; and
fitting the metal cap onto the steel shaft and curing of the adhesive.

### Claim 15 (depends on 14)

The method of claim 14, further comprising a step of treating a portion of the surface of the metal part that comprises the portion of the surface intended for being treated with ultra-short laser pulses and that comprises a portion of the surface adjoining the portion of the surface intended for being treated with ultra-short laser pulses with a plasma to at least immobilize layers of volatile organic compounds on the treated metal surface, wherein the plasma is an atmospheric-pressure plasma.

### Claim 16 (depends on 12)

The method of claim 12, wherein the ultra-fast laser pulses have a spot diameter of around 50 μm.
