# US 2021/0079554 A1 · Methods for growing a nitrogen doped single crystal silicon ingot using continuous czochralski method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0079554 A1
- Document ID: US20210079554A1
- Status: Published application
- Kind: A1
- Application number: 16/569,949
- Filed: 2019-09-13
- Published: 2021-03-18
- Earliest claimed: 2019-09-13
- Assignees: GlobalWafers Co., Ltd.
- Applicants: GlobalWafers Co., Ltd.
- Inventors: Carissima Marie Hudson; Jae-Woo Ryu
- Web page: https://patentgrep.com/patent/US20210079554A1

## CPC

- C30B 15/04: adding doping materials, e.g. for n-p-junction
- C30B 15/305: {Stirring of the melt}
- C30B 15/002: {Continuous growth}
- C30B 15/14: Heating of the melt or the crystallised materials
- C30B 15/203: {the relationship of pull rate (v) to axial thermal gradient (G)}
- C30B 29/06: Silicon
- H10P 36/20: Intrinsic gettering, i.e. thermally inducing defects by using oxygen present in the silicon body
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A method for growing a single crystal silicon ingot by the continuous Czochralski method is disclosed. The melt depth and thermal conditions are constant during growth because the silicon melt is continuously replenished as it is consumed, and the crucible location is fixed. The critical v/G is determined by the hot zone configuration, and the continuous replenishment of silicon to the melt during growth enables growth of the ingot at a constant pull rate consistent with the critical v/G during growth of a substantial portion of the main body of the ingot. The continuous replenishment of silicon is accompanied by periodic or continuous nitrogen addition to the melt to result in a nitrogen doped ingot.

## Claims

### Claim 1

A method of preparing a single crystal silicon ingot by the Continuous Czochralski method, the method comprising:
adding an initial charge of polycrystalline silicon to a crucible, the initial charge further comprising a source of nitrogen;
heating the crucible comprising the initial charge of polycrystalline silicon and the source of nitrogen to cause a silicon melt to form in the crucible, the silicon melt comprising an initial volume of molten silicon and having an initial melt elevation level;
contacting a silicon seed crystal with a silicon melt;
withdrawing the silicon seed crystal to grow a neck portion, wherein the silicon seed crystal is withdrawn at a neck portion pull rate during growth of the neck portion, and further wherein the neck portion has a neck portion nitrogen concentration of at least about 1×1013 atoms/cm3;
withdrawing the silicon seed crystal to grow an outwardly flaring seed-cone adjacent the neck portion, wherein the silicon seed crystal is withdrawn at a seed-cone pull rate during growth of the outwardly flaring seed-cone, and further wherein the outwardly flaring seed-cone has an outwardly flaring seed-cone nitrogen concentration of at least about 1×1013 atoms/cm3; and
withdrawing the silicon seed crystal to grow a main body of the single crystal silicon ingot adjacent the outwardly flaring seed-cone, wherein the silicon melt comprises a volume of molten silicon and a melt elevation level during growth of the main body of the single crystal silicon ingot, and further wherein the main body of the single crystal silicon has a main body nitrogen concentration of at least about 1×1013 atoms/cm3;
wherein the main body of the single crystal silicon ingot is grown at an initial variable main body pull rate and a constant main body pull rate, wherein the main body of the single crystal silicon ingot is grown at the initial variable main body pull rate for less than about 20% of a length of the main body of the single crystal silicon ingot and grown at the constant main body pull rate during growth for at least about 30% of the length of the main body of the single crystal silicon ingot; and
further wherein polycrystalline is continuously fed or periodically feed to the crucible to thereby replenish a volume of molten silicon and to thereby maintain a melt elevation level in the crucible during growth of the main body of the single crystal silicon ingot and the source of nitrogen is continuously fed or periodically fed to the crucible to thereby replenish an amount of nitrogen.

### Claim 2 (depends on 1)

The method of claim 1 wherein the source of nitrogen is a solid source of nitrogen.

### Claim 3 (depends on 1)

The method of claim 1 wherein the source of nitrogen is silicon nitride powder.

### Claim 4 (depends on 1)

The method of claim 1 wherein the source of nitrogen is a silicon wafer having a silicon nitride film on a surface thereof, wherein the silicon wafer is optionally crushed.

### Claim 5 (depends on 1)

The method of claim 1 wherein the source of nitrogen is silicon oxynitride glass.

### Claim 6 (depends on 1)

The method of claim 1 wherein the source of nitrogen is nitrogen gas.

### Claim 7 (depends on 1)

The method of claim 1 wherein the neck portion nitrogen concentration is between about 1×1013 atoms/cm3 and about 1×1015 atoms/cm3, or between about 1×1013 atoms/cm3 and about 1.5×1014 atoms/cm3, or between about 5×1013 atoms/cm3 and about 1×1014 atoms/cm3.

### Claim 8 (depends on 1)

The method of claim 1 wherein the outwardly flaring seed-cone nitrogen concentration is between about 1×1013 atoms/cm3 and about 1×1015 atoms/cm3, or between about 1×1013 atoms/cm3 and about 1.5×1014 atoms/cm3, or between about 5×1013 atoms/cm3 and about 1×1014 atoms/cm3.

### Claim 9 (depends on 1)

The method of claim 1 wherein the source of nitrogen is continuously fed or periodically fed to the crucible in an amount between about 1 milligram nitrogen and about 100 milligrams nitrogen per 50 mm of axial length of the main body of the single crystal silicon ingot, or between about 1 milligram nitrogen and about 25 milligrams nitrogen per 50 mm of axial length of the main body of the single crystal silicon ingot, or between about 2 milligrams nitrogen and about 15 milligrams nitrogen per 50 mm of axial length of the main body of the single crystal silicon ingot.

### Claim 10 (depends on 1)

The method of claim 1 wherein silicon nitride is continuously fed or periodically fed to the crucible during growth of the main body of the single crystal silicon ingot in an amount between about 2.5 milligrams silicon nitride and 250 milligrams silicon nitride per 50 mm of axial length of the main body of the single crystal silicon ingot, or between about 5 milligrams silicon nitride and 100 milligrams silicon nitride per 50 mm of axial length of the main body of the single crystal silicon ingot, or between about 10 milligrams silicon nitride and 50 milligrams silicon nitride per 50 mm of axial length of the main body of the single crystal silicon ingot.

### Claim 11 (depends on 1)

The method of claim 1 wherein the main body nitrogen concentration is between about 1×1013 atoms/cm3 and about 1×1015 atoms/cm3, or between about 1×1013 atoms/cm3 and about 1.5×1014 atoms/cm3, or between about 5×1013 atoms/cm3 and about 1×1014 atoms/cm3.

### Claim 12 (depends on 1)

The method of claim 1 wherein the main body nitrogen concentration is between about 5×1013 atoms/cm3 and about 1×1014 atoms/cm3, over at least 40% of axial length of the main body of the single crystal silicon ingot, at least 50% of axial length of the main body of the single crystal silicon ingot, at least 60% of axial length of the main body of the single crystal silicon ingot, at least 70% of axial length of the main body of the single crystal silicon ingot, or at least 80% of axial length of the main body of the single crystal silicon ingot.

### Claim 13 (depends on 1)

The method of claim 1 wherein the main body nitrogen concentration is between about 1×1013 atoms/cm3 and about 1.5×1014 atoms/cm3, or between about 5×1013 atoms/cm3 and about 1×1014 atoms/cm3 and further wherein the main body nitrogen concentration varies by no more than 20% above and no less than 20% below an average main body nitrogen concentration over at least 40% of axial length of the main body of the single crystal silicon ingot, at least 50% of axial length of the main body of the single crystal silicon ingot, at least 60% of axial length of the main body of the single crystal silicon ingot, at least 70% of axial length of the main body of the single crystal silicon ingot, or at least 80% of axial length of the main body of the single crystal silicon ingot.

### Claim 14 (depends on 1)

The method of claim 1 wherein the main body nitrogen concentration is between about 5×1013 atoms/cm3 and about 1×1014 atoms/cm3 and further wherein the main body nitrogen concentration varies by no more than 20% above and no less than 20% below an average main body nitrogen concentration over at least 40% of axial length of the main body of the single crystal silicon ingot, at least 50% of axial length of the main body of the single crystal silicon ingot, at least 60% of axial length of the main body of the single crystal silicon ingot, at least 70% of axial length of the main body of the single crystal silicon ingot, or at least 80% of axial length of the main body of the single crystal silicon ingot.

### Claim 15 (depends on 1)

The method of claim 1 wherein a magnetic field is applied to the silicon melt during growth of the main body of the single crystal silicon ingot.

### Claim 16 (depends on 15)

The method of claim 15 wherein a horizontal magnetic field is applied to the silicon melt during growth of the main body of the single crystal silicon ingot.

### Claim 17 (depends on 15)

The method of claim 15 wherein a cusp magnetic field is applied to the silicon melt during growth of the main body of the single crystal silicon ingot.

### Claim 18 (depends on 15)

The method of claim 15 wherein the applied magnetic field maintains a substantially constant melt/solid interface profile during at least about 70% of the growth of the main body of the single crystal silicon ingot.

### Claim 19 (depends on 15)

The method of claim 15 wherein the applied magnetic field maintains a substantially constant melt/solid interface profile during between about 70% and about 90% of the growth of the main body of the single crystal silicon ingot.

### Claim 20 (depends on 1)

The method of claim 1 wherein the main body of the single crystal silicon ingot is at least about 1000 millimeters long, such as at least 1400 millimeters long, such as at least 1500 millimeters long, or at least 2000 millimeters long, or at least 2200 millimeters, such as 2200 millimeters, or at least about 3000 millimeters long, or at least about 4000 millimeters long.

### Claim 21 (depends on 1)

The method of claim 1 wherein the main body of the single crystal silicon ingot has a diameter of at least about 150 millimeters, such as at least about 200 millimeters, at least about 300 millimeters, or at least about 450 millimeters.

### Claim 22 (depends on 1)

The method of claim 1 wherein the constant main body pull rate is between about 0.4 mm/min and about 0.8 mm/min, between about 0.4 mm/min and about 0.7 mm/min, or between about 0.4 mm/min and about 0.65 mm/min.

### Claim 23 (depends on 1)

The method of claim 1 wherein the main body of the single crystal silicon ingot is grown at the initial variable main body pull rate for between about 5% and about 20% of the length of the main body of the single crystal silicon ingot.

### Claim 24 (depends on 1)

The method of claim 1 wherein the main body of the single crystal silicon ingot is grown at the constant main body pull rate during growth for at least about 50% of the length of the main body of the single crystal silicon ingot.

### Claim 25 (depends on 1)

The method of claim 1 wherein the main body of the single crystal silicon ingot is grown at the constant main body pull rate during growth for at least about 70% of the length of the main body of the single crystal silicon ingot.

### Claim 26 (depends on 1)

The method of claim 1 wherein the main body of the single crystal silicon ingot is grown at the constant main body pull rate during growth for at least about 80% of the length of the main body of the single crystal silicon ingot.

### Claim 27 (depends on 1)

The method of claim 1 wherein the main body of the single crystal silicon ingot is grown at the constant main body pull rate during growth for at least about 90% of the length of the main body of the single crystal silicon ingot.

### Claim 28 (depends on 1)

The method of claim 1 wherein the main body pull rate is a constant critical pull rate sufficient to avoid agglomerated point defects over at least 70% of the length of the main body of the single crystal silicon ingot.

### Claim 29 (depends on 1)

The method of claim 1 wherein the main body pull rate is a constant critical pull rate sufficient to avoid agglomerated point defects over at least 90% of the length of the main body of the single crystal silicon ingot.

### Claim 30 (depends on 1)

The method of claim 1 wherein the volume of molten silicon varies by no more than about 1.0 volume % during growth of at least about 90% the main body of the single crystal silicon ingot.

### Claim 31 (depends on 1)

The method of claim 1 wherein the volume of molten silicon varies by no more than about 0.5 volume % during growth of at least about 90% the main body of the single crystal silicon ingot.

### Claim 32 (depends on 1)

The method of claim 1 wherein the volume of molten silicon varies by no more than about 0.1 volume % during growth of at least about 90% the main body of the single crystal silicon ingot.

### Claim 33 (depends on 1)

The method of claim 1 wherein the melt elevation level varies by less than about +/−0.5 millimeter during growth of at least about 90% the main body of the single crystal silicon ingot.

### Claim 34 (depends on 1)

The method of claim 1 wherein the main body of the single crystal silicon ingot comprises perfect silicon over at least about 70% of the length of the main body of the single crystal silicon ingot.

### Claim 35 (depends on 1)

The method of claim 1 wherein the main body of the single crystal silicon ingot comprises perfect silicon over at least about 80% of the length of the main body of the single crystal silicon ingot.

### Claim 36 (depends on 1)

The method of claim 1 wherein the main body of the single crystal silicon ingot comprises perfect silicon over at least about 90% of the length of the main body of the single crystal silicon ingot.

### Claim at position 37

-56. (canceled)