# US 2021/0079552 A1 · Methods for electropolishing and coating aluminum on air and/or moisture sensitive substrates

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0079552 A1
- Document ID: US20210079552A1
- Status: Published application
- Kind: A1
- Application number: 16/572,810
- Filed: 2019-09-17
- Published: 2021-03-18
- Earliest claimed: 2019-09-17
- Assignees: Consolidated Nuclear Security, LLC
- Applicants: Consolidated Nuclear Security, LLC
- Inventors: John W. FREIDERICH; Tasha L. BOYD
- Web page: https://patentgrep.com/patent/US20210079552A1

## CPC

- C23C 18/1848: {by electrochemical pretreatment}
- C23C 18/1653: {Two or more layers with at least one layer obtained by electroless plating and one layer obtained by electroplating}
- C23C 18/31: Coating with metals
- C25D 3/44: Aluminium
- C25D 3/56: of alloys
- C25D 3/665: {from ionic liquids}
- C25D 5/18: Electroplating using modulated, pulsed or reversing current
- C25D 5/34: Pretreatment of metallic surfaces to be electroplated
- C25D 5/50: by heat-treatment
- C25F 3/16: Polishing
- C25F 3/20: of aluminium
- C25F 3/22: of heavy metals
- C25F 3/26: of refractory metals
- C25F 3/28: of actinides
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR
- C25F: PROCESSES FOR THE ELECTROLYTIC REMOVAL OF MATERIALS FROM OBJECTS; APPARATUS THEREFOR

## Abstract

Methods for electropolishing and coating aluminum on a surface of an air and/or moisture sensitive substrate, including: in a vessel, submerging the substrate in a first molten salt bath and applying an anodizing current to the substrate at a first temperature to electropolish the surface of the substrate; wherein the first molten salt bath includes one of a first organic salt bath and first inorganic salt bath; wherein, when used, the first organic salt bath includes one of (a) aluminum halide and ionic liquid, (b) a combination of an aluminum halide and halogenatedmethylphenylsulfone (C6(H5−y,Xy)SO2CX3, where y is a number from 0-5), (c) a combination of an aluminum halide, an ionic liquid, and halogenatedmethylphenylsulfone (C6(H5−y,Xy)SO2CX3), and (d) AlF3-organofluoride-hydrofluoric acid adduct; wherein, when used, the first inorganic salt bath includes aluminum halide and alkali metal halide; and wherein the anodizing current is 10-30 mA/cm2.

## Claims

### Claim 1

A method for electropolishing a surface of an air and/or moisture sensitive substrate, the method comprising:
in a vessel, submerging the substrate in a first molten salt bath at a first temperature and applying an anodizing current to the substrate to electropolish the surface of the substrate;
wherein the first molten salt bath comprises one of a first organic salt bath and first inorganic salt bath;
wherein, when used, the first organic salt bath comprises one of (a) aluminum halide and ionic liquid (e.g., trihexyltetradecylphosphonium chloride (P((CH2)5CH3)3(CH2)13CH3Cl)), (b) a combination of an aluminum halide and halogenatedmethylphenylsulfone (C6(H5−y,Xy)SO2CX3, where y is a number from 0-5), (c) a combination of an aluminum halide, an ionic liquid (e.g., trihexyltetradecylphosphonium chloride (P((CH2)5CH3)3(CH2)13CH3Cl)), and halogenatedmethylphenylsulfone (C6(H5−y,Xy)SO2CX3, where y is a number from 0-5), and (d) AlF3-organofluoride-hydrofluoric acid adduct;
wherein, when used, the first inorganic salt bath comprises aluminum halide and alkali metal halide; and
wherein the anodizing current is 10-30 mA/cm2 applied using one of a reverse bias from a power supply coupled to the first molten salt bath and by swapping working and auxiliary electrode leads coupled to the first molten salt bath.

### Claim 2 (depends on 1)

The method of claim 1, wherein the halogenatedmethylphenylsulfone comprises fluorinatedmethylphenylsulfone (C6(H5−y,Fy)SO2CF3).

### Claim 3 (depends on 1)

The method of claim 1, wherein, when used, the first organic salt bath comprises (a) 55-67 wt % AlCl3 and 33-45 wt % ionic liquid.

### Claim 4 (depends on 1)

The method of claim 1, wherein, when used, the first organic salt bath comprises (b) 55-67 wt % AlCl3 and 33-45 wt % halogenatedmethylphenylsulfone.

### Claim 5 (depends on 1)

The method of claim 1, wherein, when used, the first organic salt bath comprises (c) 55-67 wt % AlCl3, 0.1-10 wt % ionic liquid, and 27-44.9 wt % halogenatedmethylphenylsulfone.

### Claim 6 (depends on 1)

The method of claim 1, wherein, when used, the first organic salt bath comprises (d) 60-70 wt % aluminum fluoride, 23-29 wt % 1-ethyl-3-methylimidazolium fluoride, and 8-10 wt % hydrofluoric acid.

### Claim 7 (depends on 1)

The method of claim 1, wherein the first temperature of the first organic salt bath is less than the flash point of the first organic salt bath.

### Claim 8 (depends on 1)

The method of claim 1, wherein the first temperature of the first organic salt bath is 20-70 degrees C.

### Claim 9 (depends on 1)

The method of claim 1, wherein, when used, the first inorganic salt bath comprises 68-100 wt % AlCl3, 0-19 wt % NaCl, and 0-13 wt % KCl.

### Claim 10 (depends on 9)

The method of claim 9, wherein, when used, the first inorganic salt bath comprises 82 wt % AlCl3, 11 wt % NaCl, and 7 wt % KCl.

### Claim 11 (depends on 1)

The method of claim 1, wherein, when used, the first inorganic salt bath comprises 75-100 wt % AlBr3, 0-15.4 wt % NaBr, and 0-9.6 wt % KBr.

### Claim 12 (depends on 1)

The method of claim 1, wherein, when used, the first inorganic salt bath comprises 76-100 wt % AlI3, 0-15 wt % NaI, and 0-9 wt % KI at a first temperature of 110-250 degrees C.

### Claim 13 (depends on 1)

The method of claim 1, wherein the first temperature of the inorganic salt bath is 95-250 degrees C.

### Claim 14 (depends on 1)

The method of claim 1, further comprising, subsequent to electropolishing the surface of the substrate, coating the electropolished surface of the substrate with aluminum.

### Claim 15 (depends on 14)

The method of claim 14, wherein coating the electropolished surface of the substrate with aluminum comprises:
discontinuing the anodizing current and allowing the electropolished substrate to dwell in the first molten salt bath such that the electropolished surface of the substrate is coated with aluminum.

### Claim 16 (depends on 14)

The method of claim 14, wherein coating the electropolished surface of the substrate with aluminum comprises:
one or more of heating the first molten salt bath and evaporating the first molten salt bath under vacuum to remove the first molten salt bath from the vessel, physically pumping the first molten salt bath from the vessel, and draining the first molten salt bath from the vessel; and
in the vessel, submerging the electropolished substrate in a second molten salt bath at a second temperature such that the electropolished surface of the substrate is coated with aluminum;
wherein the second molten salt bath comprises one of a second organic salt bath and second inorganic salt bath;
wherein, when used, the second organic salt bath comprises one of (a) aluminum halide and ionic liquid (e.g., trihexyltetradecylphosphonium chloride (P((CH2)5CH3)3(CH2)13CH3Cl)), (b) a combination of an aluminum halide and halogenatedmethylphenylsulfone (C6(H5−y,Xy)SO2CX3, where y is a number from 0-5), (c) a combination of an aluminum halide, an ionic liquid (e.g., trihexyltetradecylphosphonium chloride (P((CH2)5CH3)3(CH2)13CH3Cl)), and halogenatedmethylphenylsulfone (C6(H5−y,Xy)SO2CX3, where y is a number from 0-5), and (d) AlF3-organofluoride-hydrofluoric acid adduct; and
wherein, when used, the second inorganic salt bath comprises aluminum halide and alkali metal halide.

### Claim 17 (depends on 16)

The method of claim 16, wherein, the halogenatedmethylphenylsulfone comprises fluorinatedmethylphenylsulfone (C6(H5−y,Fy)SO2CF3).

### Claim 18 (depends on 16)

The method of claim 16, further comprising purging the vessel with an inert gas after the first molten salt bath is removed from the vessel.

### Claim 19 (depends on 16)

The method of claim 16, wherein the second temperature is below a flash point of the second organic salt bath, when used, and 95-250 degrees C. for the second inorganic salt bath, when used.

### Claim 20 (depends on 16)

The method of claim 16, wherein the second inorganic salt bath comprises 68-100 wt % AlCl3, 0-19 wt % NaCl, and 0-13 wt % KCl.

### Claim 21 (depends on 14)

The method of claim 14, wherein coating the electropolished surface of the substrate with aluminum further comprises:
applying a reducing current to the electropolished substrate to coat the surface of the electropolished substrate with aluminum derived from the first molten salt bath.

### Claim 22 (depends on 21)

The method of claim 21, wherein the reducing current is no more than 7 mA/cm2, is alternating-current frequency modulated, and is applied using a working electrode coupled to the first molten salt bath.

### Claim 23 (depends on 14)

The method of claim 14, wherein coating the electropolished surface of the substrate with aluminum further comprises:
applying a reducing current to the electropolished substrate to coat the surface of the electropolished substrate with aluminum derived from the second molten salt bath.

### Claim 24 (depends on 23)

The method of claim 23, wherein the reducing current is no more than 7 mA/cm2, is alternating-current frequency modulated, and is applied in the second molten salt bath.

### Claim 25 (depends on 14)

The method of claim 14, further comprising adding a transition metal halide to the second molten salt bath to cause an aluminum alloy to be coated on the surface of the electropolished substrate.

### Claim 26 (depends on 25)

The method of claim 25, wherein the transition metal halide comprises one or more of Mn, Cr, and Ni.

### Claim 27 (depends on 14)

The method of claim 14, further comprising annealing a resulting aluminum coating.

### Claim 28 (depends on 14)

The method of claim 14, wherein coating the electropolished surface of the substrate with aluminum comprises:
in the vessel, submerging the substrate in a molten pool of aluminum to coat the surface of the substrate with aluminum or the surface of an aluminum-coated substrate with additional aluminum.

### Claim 29

A method for coating aluminum on a surface of an air and/or moisture sensitive substrate, the method comprising:
in a vessel, submerging the substrate in a molten salt bath with a temperature of at least 95 degrees C.;
applying an anodizing current to the substrate to electropolish the surface of the substrate; and
coating the electropolished surface of the substrate with aluminum by one of submerging the substrate in a molten pool of aluminum, discontinuing the anodizing current and allowing the electropolished substrate to dwell in the molten salt bath at a temperature of at least 95 degrees C. such that the electropolished surface of the substrate is electrolessly coated with aluminum, and applying a reducing current to the electropolished substrate to electroplate the surface of the electropolished substrate with aluminum derived from the molten salt bath, wherein the reducing current is no more than 7 mA/cm2;
wherein the molten salt bath comprises aluminum halide and alkali metal halide.

### Claim 30 (depends on 29)

The method of claim 29, wherein the substrate comprises one or more of zirconium, hafnium, thorium, uranium, plutonium, manganese, a rare earth metal (La—Lu), yttrium, magnesium, lithium, and their alloys.

### Claim 31 (depends on 29)

The method of claim 29, wherein the vessel is sealed and contains an inert cover gas.

### Claim 32 (depends on 29)

The method of claim 29, wherein the substrate electrolessly coated with aluminum is submerged in a molten pool of aluminum.

### Claim 33 (depends on 29)

The method of claim 29, wherein the substrate electroplated with aluminum is submerged in a molten pool of aluminum.