- Number: US 2021/0079547 A1
- Document ID: US20210079547A1
- Status: Published application
- Kind: A1
- Application number: 16/982,421
- Filed: 2019-03-15
- Published: 2021-03-18
- Earliest claimed: 2018-03-20
- Assignees: aveni
- Applicants: Aveni
- Inventors: Vincent MEVELLEC; Dominique SUHR; Mikailou THIAM; Louis CAILLARD
- Web page: https://patentgrep.com/patent/US20210079547A1

## CPC

- C25D 3/12: of nickel or cobalt
- C25D 5/50: by heat-treatment
- C25D 7/123: {Semiconductors first coated with a seed layer or a conductive layer}
- H10P 14/47: Electrolytic deposition, i.e. electroplating; Electroless plating
- H10P 14/69215: {the material being a silicon oxide, e.g. SiO2}
- H10W 20/056: {by filling conductive material into holes, grooves or trenches}
- H10W 20/057: {by selectively depositing, e.g. by using selective CVD or plating}
- H10W 20/4437: {the principal metal being a transition metal}
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

The present invention relates to a process for the fabrication of cobalt interconnections and to an electrolyte which enables the implementation thereof. The electrolyte which has a pH below 4.0 comprises cobalt ions, chloride ions and at most two organic additives of low molecular weight. One of these additives may be an alpha-hydroxy carboxylic acid or a compound having a pKa value ranging from 1.8 to 3.5.

## Claims

### Claim 1

Electrolyte for the electrodeposition of cobalt, characterized in that the electrolyte is an aqueous solution comprising from 1 to 5 g/l of cobalt II ions, from 1 to 10 g/l of chloride ions, an acid in an amount sufficient to obtain a pH of between 1.8 and 4.0, and at most two organic additives, said organic additives not being polymers.

### Claim 2 (depends on 1)

Electrolyte according to claim 1, characterized in that the organic additive(s) have a molecular weight of less than 250 g/mol and greater than 50 g/mol.

### Claim 3 (depends on 1)

Electrolyte according to claim 1, characterized in that it comprises at most one organic additive.

### Claim 4 (depends on 1)

Electrolyte according to claim 1, characterized in that the organic additive(s) are chosen from alpha-hydroxy carboxylic acids.

### Claim 5 (depends on 1)

Electrolyte according to claim 1, characterized in that the acid is hydrochloric acid and that at least one of the organic additives is chosen from organic compounds which have at least 1 pKa ranging from 1.8 to 3.5.

### Claim 6 (depends on 5)

Electrolyte according to claim 5, characterized in that at least one of the organic additives is chosen from citric acid, tartaric acid, malic acid, mandelic acid, maleic acid, fumaric acid, glyceric acid, orotic acid, malonic acid, L-alanine, acetylsalicylic acid and salicylic acid.

### Claim 7 (depends on 1)

Electrolyte according to claim 1, characterized in that the cobalt II ions are in free form, that is to say not complexed with the organic additive(s).

### Claim 8 (depends on 1)

Electrolyte according to claim 1, characterized in that its pH is between 2.0 and 3.5.

### Claim 9 (depends on 1)

Electrolyte according to claim 1, characterized in that the concentration of the additive or the sum of the concentrations of the two additives is between 5 and 200 mg/l.

### Claim 10 (depends on 1)

Electrochemical process for filling cavities, said process comprising:
a step of bringing a conductive surface of said cavities into contact with an electrolyte in accordance with claim 1,
a step of polarizing the conductive surface for a period of time sufficient to carry out the conformal and complete filling of the cavities by deposition of the cobalt, and
a step of annealing the cobalt deposit obtained at the end of the polarization step.

### Claim 11 (depends on 10)

Process according to claim 10, characterized in that the cavities are obtained by carrying out the following steps:
a step of etching structures in a silicon substrate,
a step of forming a layer of silicon oxide on a silicon surface of the structures so as to obtain a silicon oxide surface,
a step of depositing a layer of metal on said silicon oxide surface or on said layer of metal alloy so as to obtain the conductive surface of the cavities.

### Claim 12 (depends on 11)

Process according to claim 11, characterized in that the layer of metal comprises at least one compound chosen from the group consisting of cobalt, copper, tungsten, titanium, tantalum, ruthenium, nickel, titanium nitride and tantalum nitride.

### Claim 13 (depends on 10)

Process according to claim 10, characterized in that the cavities have a width or a diameter at the opening of less than 40 nm, preferably of between 15 nm and 30 nm, and a depth of between 50 nm and 250 nm.

### Claim 14 (depends on 10)

Process according to claim 10, characterized in that the cobalt deposit has a content of impurities of less than 1000 ppm atomic and that it comprises an average void percentage of less than 10% by volume or by surface area, measured by electron microscopy.

### Claim 15 (depends on 10)

Process according to claim 10, characterized in that the cobalt deposition speed is between 0.1 and 3.0 nm/s.

### Claim 16

Electrochemical process for the deposition of cobalt on a substrate comprising a conductive surface inside cavities hollowed out in the substrate and a conductive surface outside the cavities, said process comprising:
a step of bringing said conductive surfaces into contact with an electrolyte in the form of an aqueous solution with a pH of between 2.0 and 4.0 comprising cobalt II ions, chloride ions, and just one or at most two organic additives, said organic additives not being polymers,
a step of polarizing said conductive surfaces for a period of time sufficient to carry out the filling of the cavities with cobalt, and also to deposit a layer of cobalt at least 50 nm thick on the conductive surface outside the cavities,
a step of annealing the cobalt obtained at the end of the polarization step.