# US 2021/0079532 A1 · Method for coating on surface of medical peek material, titanium having microporous structure

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0079532 A1
- Document ID: US20210079532A1
- Status: Published application
- Kind: A1
- Application number: 16/642,364
- Filed: 2018-07-19
- Published: 2021-03-18
- Earliest claimed: 2017-10-19
- Assignees: Osong Medical Innovation Foundation
- Applicants: Osong Medical Innovation Foundation
- Inventors: Tae Gon JUNG; Yong Hoon JEONG; Su Won LEE; Kwang Min PARK; Jae Woong YANG; Jae Young JUNG; Kwan Su KANG
- Web page: https://patentgrep.com/patent/US20210079532A1

## CPC

- C23C 14/20: on organic substrates
- C23C 14/351: {using a magnetic field in close vicinity to the substrate}
- A61L 27/18: obtained otherwise than by reactions only involving carbon-to-carbon unsaturated bonds
- A61L 27/306: {Other specific inorganic materials not covered by A61L27/303 - A61L27/32}
- B24B 31/10: involving other means for tumbling of work
- B24B 31/102: {using an alternating magnetic field}
- C23C 14/205: {by cathodic sputtering}
- C23C 14/35: by application of a magnetic field, e.g. magnetron sputtering {(C23C14/3457 takes precedence)}
- C23C 14/5853: {Oxidation}
- C23C 14/588: {by mechanical treatment}
- C23C 14/5886: {Mechanical treatment (involving removal of material C23C14/588)}
- C23C 28/322: {only coatings of metal elements only}
- C23C 28/3455: {with a refractory ceramic layer, e.g. refractory metal oxide, ZrO2, rare earth oxides or a thermal barrier system comprising at least one refractory oxide layer}
- C25D 11/26: of refractory metals or alloys based thereon
- C25D 11/34: of metals or alloys not provided for in groups C25D11/04 - C25D11/32
- A61L 2430/38: for reconstruction of the spine, vertebrae or intervertebral discs
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- A61L: METHODS OR APPARATUS FOR STERILISING MATERIALS OR OBJECTS IN GENERAL; DISINFECTION, STERILISATION OR DEODORISATION OF AIR; CHEMICAL ASPECTS OF BANDAGES, DRESSINGS, ABSORBENT PADS OR SURGICAL ARTICLES; MATERIALS FOR BANDAGES, DRESSINGS, ABSORBENT PADS OR SURGICAL ARTICLES (preservation of bodies or disinfecting characterised by the agents employed A01N; preserving, e.g. sterilising, food or foodstuffs A23; preparations for medical, dental or toiletry purposes A61K)
- B24B: MACHINES, DEVICES, OR PROCESSES FOR GRINDING OR POLISHING (grinding of gear teeth B23F, of screw-threads B23G1/36; by electro-erosion B23H; abrasive or related blasting B24C; tools for grinding, buffing or sharpening B24D; polishing compositions C09G1/00; abrasives C09K3/14; electrolytic etching or polishing C25F3/00; grinding arrangements for use on assembled railway tracks E01B31/17); DRESSING OR CONDITIONING OF ABRADING SURFACES; FEEDING OF GRINDING, POLISHING, OR LAPPING AGENTS
- C25D: PROCESSES FOR THE ELECTROLYTIC OR ELECTROPHORETIC PRODUCTION OF COATINGS; ELECTROFORMING; APPARATUS THEREFOR

## Abstract

In a method for coating on a surface of a medical PEEK material with titanium to have a microporous structure, titanium is coated on a surface of polyether ether ketone (PEEK) via magnetron sputtering. The surface of the titanium coated on the surface of PEEK is polished via an electromagnetic polishing apparatus. A thin-film with titanium dioxide (TiO2) having a microporous structure is formed on the polished surface of the titanium via an anodic oxidation treatment.

## Claims

### Claim 1

A method for coating with titanium, comprising:
coating titanium on a surface of polyether ether ketone (PEEK) via magnetron sputtering;
polishing the surface of the titanium coated on the surface of PEEK via an electromagnetic polishing apparatus; and
forming a thin-film with titanium dioxide (TiO2) having a microporous structure on the polished surface of the titanium via an anodic oxidation treatment.

### Claim 2 (depends on 1)

The method of claim 1, wherein in the coating titanium,
disposing a titanium target inside of a chamber of a magnetron sputtering apparatus;
injecting an unalive gas into the chamber; and
applying a predetermined voltage to the titanium target with predetermined temperature and pressure conditions, to coat the titanium on the surface of PEEK.

### Claim 3 (depends on 2)

The method of claim 2, wherein in the coating titanium on the surface of PEEK,
the pressure is about 5×10−3 torr, the temperature is between about 100° C. and about 150° C., and the power is between about 2 kW and about 3 kW.

### Claim 4 (depends on 1)

The method of claim 1, wherein a thickness coated on the surface of PEEK is between about 2.5 μm and about 3.0 μm.

### Claim 5 (depends on 2)

The method of claim 2, wherein in the coating titanium on the surface of PEEK,
a titanium plasma is generated by the voltage applied between the titanium target and the PEEK with rotating the PEEK, and a magnetic field generated by an electrode reaches the PEEK, so that titanium plasma ions generated around a surface of the titanium target are coated on the surface of PEEK.

### Claim 6 (depends on 1)

The method of claim 1, wherein the electromagnetic polishing apparatus comprises:
a magnetic field generator having a permanent magnet generating an N pole magnetic field and a permanent generating an S pole magnetic field;
a magnetic field converter rotating the magnetic field generator, to covert the positions of the N pole magnetic field and the S pole magnetic field repeatedly by a relatively short period;
a polishing receiver configured into which the PEEK having the surface coated with titanium and a polishing material having magnetism are provided, into which the magnetic field generated by the magnetic field generator is supplied; and
a receiving plate disposed over the magnetic field converter and receiving the polishing receiver.

### Claim 7 (depends on 1)

The method of claim 1, wherein in the polishing,
a liquid and a polishing material are provided into a polishing receiver having a predetermined volume;
the PEEK having the surface coated with titanium is disposed and fixed into the polishing receiver;
a magnetic force is generated to the polishing receiver via a magnetic field generator; and
the polishing material moves along a predetermined direction with respect to the PEEK having the surface coated with titanium due to the generated magnetic force, so that the titanium coated on the surface of the PEEK is polished to be planarized.

### Claim 8 (depends on 7)

The method of claim 7, wherein the polishing material is SUS 304.

### Claim 9 (depends on 1)

The method of claim 1, wherein in forming the thin-film with titanium dioxide,
the PEEK coated with the polished titanium and platinum (Pt) are dipped into an electrolyte of an anodic oxidation apparatus;
an anode of a direct current power is electrically connected to the PEEK coated with the polished titanium, and a cathode thereof is electrically connected to platinum; and
a predetermined voltage and a predetermined current are applied to the anode and the cathode in a predetermined temperature for the anodic oxidation of the surface of the polished titanium, so that the thin-film with titanium dioxide having the microporous structure is formed.

### Claim 10 (depends on 9)

The method of claim 9, wherein the electrolyte comprises 3.75 mole NaOH.

### Claim 11 (depends on 9)

The method of claim 9, wherein in forming the thin-film with titanium dioxide,
the temperature is about 18° C., the voltage is between about 10V and about 15V, and the current is between about 0.5 A and about 1 A.