# US 2021/0079512 A1 · Molybdenum containing targets

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0079512 A1
- Document ID: US20210079512A1
- Status: Published application
- Kind: A1
- Application number: 17/038,325
- Filed: 2020-09-30
- Published: 2021-03-18
- Earliest claimed: 2010-06-30
- Assignees: H.C. Starck GmbH
- Applicants: H.C. Starck, Inc.
- Inventors: Gary Alan Rozak; Mark E. Gaydos; Patrick Alan Hogan; Shuwei Sun
- Web page: https://patentgrep.com/patent/US20210079512A1

## CPC

- C23C 14/185: {by cathodic sputtering}
- C22C 27/04: Alloys based on tungsten or molybdenum
- C23C 14/3407: {Cathode assembly for sputtering apparatus, e.g. Target}
- C23C 14/3414: {Metallurgical or chemical aspects of target preparation, e.g. casting, powder metallurgy}
- C23C 14/5873: {Removal of material}
- G06F 3/041: Digitisers, e.g. for touch screens or touch pads, characterised by the transducing means
- B22F 2998/10: Processes characterised by the sequence of their steps
- G06F 2203/04103: Manufacturing, i.e. details related to manufacturing processes specially suited for touch sensitive devices
- Y10T 428/12743: Next to refractory [Group IVB, VB, or VIB] metal-base component
- Y10T 428/12826: Group VIB metal-base component
- Y10T 428/265: 1 mil or less
- Y10T 428/31678: Of metal
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- G06F: ELECTRIC DIGITAL DATA PROCESSING (computer systems based on specific computational models G06N)
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

The invention is directed at sputter targets including 50 atomic % or more molybdenum, a second metal element of niobium or vanadium, and a third metal element selected from the group consisting of titanium, chromium, niobium, vanadium, and tantalum, wherein the third metal element is different from the second metal element, and deposited films prepared by the sputter targets. In a preferred aspect of the invention, the sputter target includes a phase that is rich in molybdenum, a phase that is rich in the second metal element, and a phase that is rich in the third metal element.

## Claims

### Claim at position 1

-24. (canceled)

### Claim 25

A sputter target that is sputterable to form a film comprising an alloy, the sputter target comprising molybdenum, titanium, vanadium, chromium, tantalum, and niobium,
wherein a total concentration of molybdenum, titanium, vanadium, chromium, tantalum, and niobium in the sputter target is 60 atomic percent or more, based on the total number of atoms in the sputter target.

### Claim 26 (depends on 25)

The sputter target of claim 25, wherein the total concentration of molybdenum, titanium, vanadium, chromium, tantalum, and niobium in the sputter target is 80 atomic percent or more, based on the total number of atoms in the sputter target.

### Claim 27 (depends on 25)

The sputter target of claim 25, wherein the total concentration of molybdenum, titanium, vanadium, chromium, tantalum, and niobium in the sputter target is 95 atomic percent or more, based on the total number of atoms in the sputter target.

### Claim 28 (depends on 25)

The sputter target of claim 25, wherein the total concentration of molybdenum, titanium, vanadium, chromium, tantalum, and niobium in the sputter target is 99 atomic percent or more, based on the total number of atoms in the sputter target.

### Claim 29 (depends on 25)

The sputter target of claim 25, wherein the total concentration of molybdenum, titanium, vanadium, chromium, tantalum, and niobium in the sputter target is 99.5 atomic percent or more, based on the total number of atoms in the sputter target.

### Claim 30 (depends on 25)

The sputter target of claim 25, wherein the sputter target contains at least 50 atomic percent molybdenum.

### Claim 31 (depends on 25)

The sputter target of claim 25, wherein the sputter target contains at least 65 atomic percent molybdenum.

### Claim 32 (depends on 25)

The sputter target of claim 25, wherein the sputter target contains no more than 95 atomic percent molybdenum.

### Claim 33 (depends on 25)

The sputter target of claim 25, wherein the sputter target contains no more than 85 atomic percent molybdenum.

### Claim 34 (depends on 25)

The sputter target of claim 25, wherein the sputter target contains no more than 81 atomic percent molybdenum.

### Claim 35 (depends on 25)

The sputter target of claim 25, wherein the sputter target comprises a plurality of phases.

### Claim 36 (depends on 35)

The sputter target of claim 35, wherein the plurality of phases comprises one or more first phases, each first phase (I) comprising at least 50 atomic percent molybdenum and (ii) being a continuous phase.

### Claim 37 (depends on 36)

The sputter target of claim 36, wherein the plurality of phases comprises one or more discrete phases dispersed within at least one of the first phases.

### Claim 38

A method for manufacturing a touch screen device, the method comprising:
depositing a molybdenum alloy layer over a substrate; and
depositing a conductive layer over the molybdenum alloy layer,
wherein (i) the molybdenum alloy layer is deposited by sputtering a sputter target comprising molybdenum, titanium, vanadium, chromium, tantalum, and niobium, and (ii) a total concentration of molybdenum, titanium, vanadium, chromium, tantalum, and niobium in the sputter target is 60 atomic percent or more, based on the total number of atoms in the sputter target.

### Claim 39 (depends on 38)

The method of claim 38, further comprising etching the molybdenum alloy layer before depositing the conductive layer.

### Claim 40 (depends on 38)

The method of claim 38, wherein the conductive layer comprises at least one of Cu, Al, Ag, or Au.

### Claim 41 (depends on 38)

The method of claim 38, further comprising, before depositing the molybdenum alloy layer, at least one of (i) removing an oxide from the sputter target or (ii) removing an oxide from the substrate.

### Claim 42 (depends on 38)

The method of claim 38, wherein the substrate comprises glass.

### Claim 43 (depends on 38)

The method of claim 38, wherein the substrate comprises silicon.

### Claim 44 (depends on 38)

The method of claim 38, wherein a thickness of the molybdenum alloy layer is less than 200 nm.