# US 2021/0079508 A1 · Magnesium-based wrought alloy material and manufacturing method therefor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0079508 A1
- Document ID: US20210079508A1
- Status: Published application
- Kind: A1
- Application number: 16/629,906
- Filed: 2018-07-10
- Published: 2021-03-18
- Earliest claimed: 2017-07-10
- Assignees: National Institute for Materials Science
- Applicants: National Institute for Materials Science
- Inventors: Hidetoshi Somekawa; Yoshiaki Osawa
- Web page: https://patentgrep.com/patent/US20210079508A1

## CPC

- C22F 1/00: Changing the physical structure of non-ferrous metals or alloys by heat treatment or by hot or cold working (apparatus for mechanical working of metal B21, B23, B24)
- C22F 1/06: of magnesium or alloys based thereon
- C22C 23/00: Alloys based on magnesium
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

Adding multiple solute elements could create fracture origin through formation of intermetallic compound due to bonding of added elements. While maintaining microstructure for activating non-basal dislocation movement, additive elements not to create fracture origin, but to promote grain boundary sliding are preferably found from among inexpensive and versatile elements. Provided is Mg-based wrought alloy material including two or more among group consisting of Mn, Zr, Bi, and Sn; and Mg and unavoidable constituents, having excellent room-temperature ductility and characterized by having finer crystal grain size in Mg parent phase during room-temperature deformation and in that mean grain size in matrix thereof is 20 μm or smaller; rate of (σmax−σbk)/σmax (maximum load stress (σmax), breaking stress (σbk)) in stress-strain curve obtained by tension-compression test of the wrought material is 0.2 or higher; and resistance against breakage shows 200 kJ or higher.

## Claims

### Claim 1

A Mg-based alloy wrought material comprising: Mg-A mol % X-B mol % Z wherein a remainder comprises Mg and unavoidable impurities,
wherein X is any one kind of element from Mn, Bi, and Sn,
wherein Z is one or more kinds of elements from Mn, Bi, Sn, and Zr, but does not overlap the element of X,
wherein a value of A is at least 0.03 mol % and not exceeding 1 mol %,
wherein, with respect to a relationship of A and B, A≥B and an upper limit of B is not exceeding 1.0 times as large as an upper limit of A and a lower limit of B is at least 0.03 mol %, and
wherein an average crystal grain size of the Mg-based alloy wrought material is not exceeding 20 micrometer.

### Claim 2 (depends on 1)

The Mg-based alloy wrought material according to claim 1, wherein intermetallic compound particles constituted of Mg and an added element and having an average diameter of not exceeding 0.5 micrometer exist in Mg mother phase and/or crystal grain boundaries of a metallographic structure of the Mg-based alloy wrought material.

### Claim 3 (depends on 1)

The Mg-based alloy wrought material according to claim 1, wherein a value of a formula of (σmax−σbk)/σmax is at least 0.2 when a maximum applied stress is defined as (σmax) and a stress at break is defined as (σbk) in a stress-strain diagram obtained by a room temperature tensile test with an initial strain rate: not exceeding 1×10−3 s−1.

### Claim 4 (depends on 1)

The Mg-based alloy wrought material according to claim 1, wherein the Mg-based alloy wrought material does not break even if a nominal strain of at least 0.2 is applied in a room temperature tensile test or compression test with an initial strain rate: not exceeding 1×10−3 s−1.

### Claim 5 (depends on 1)

The Mg-based alloy wrought material according to claim 1, wherein an area enclosed by a nominal stress-and-nominal strain curve in a stress-strain diagram obtained by a room temperature compression test with an initial strain rate: at least 1×10−3 s−1 exhibits at least 200 kJ with respect to the Mg-based alloy wrought material.

### Claim 6 (depends on 1)

A method of manufacturing a Mg-based alloy wrought material as described in claim 1, the method comprising:
performing the solution treatment of a Mg-based alloy cast material having been melted and cast at a temperature of at least 400 degree Celsius and not exceeding 650 degree Celsius for at least 0.5 hours and not exceeding 48 hours and,
performing a hot plastic working for the treated material at a temperature of at least 50 degree Celsius and not exceeding 550 degree Celsius with at least 70% of cross-section reduction rate as a process of applying plastic strain.

### Claim 7 (depends on 6)

The method of manufacturing the Mg-based alloy wrought material according to claim 6, wherein the process of applying plastic strain comprises any one of extrusion, forging, rolling, and drawing.

### Claim 8 (depends on 2)

The Mg-based alloy wrought material according to claim 2, wherein a value of a formula of (σmax−σbk)/σmax is at least 0.2 when a maximum applied stress is defined as (σmax) and a stress at break is defined as (σbk) in a stress-strain diagram obtained by a room temperature tensile test with an initial strain rate: not exceeding 1×10−3 s−1.

### Claim 9 (depends on 2)

The Mg-based alloy wrought material according to claim 2, wherein the Mg-based alloy wrought material does not break even if a nominal strain of at least 0.2 is applied in a room temperature tensile test or compression test with an initial strain rate: not exceeding 1×10−3 s−1.

### Claim 10 (depends on 3)

The Mg-based alloy wrought material according to claim 3, wherein the Mg-based alloy wrought material does not break even if a nominal strain of at least 0.2 is applied in a room temperature tensile test or compression test with an initial strain rate: not exceeding 1×10−3 s−1.

### Claim 11 (depends on 8)

The Mg-based alloy wrought material according to claim 8, wherein the Mg-based alloy wrought material does not break even if a nominal strain of at least 0.2 is applied in a room temperature tensile test or compression test with an initial strain rate: not exceeding 1×10−3 s−1.

### Claim 12 (depends on 2)

The Mg-based alloy wrought material according to claim 2, wherein an area enclosed by a nominal stress-and-nominal strain curve in a stress-strain diagram obtained by a room temperature compression test with an initial strain rate: at least 1×10−3 s−1 exhibits at least 200 kJ with respect to the Mg-based alloy wrought material.

### Claim 13 (depends on 3)

The Mg-based alloy wrought material according to claim 3, wherein an area enclosed by a nominal stress-and-nominal strain curve in a stress-strain diagram obtained by a room temperature compression test with an initial strain rate: at least 1×10−3 s−1 exhibits at least 200 kJ with respect to the Mg-based alloy wrought material.

### Claim 14 (depends on 4)

The Mg-based alloy wrought material according to claim 4, wherein an area enclosed by a nominal stress-and-nominal strain curve in a stress-strain diagram obtained by a room temperature compression test with an initial strain rate: at least 1×10−3 s−1 exhibits at least 200 kJ with respect to the Mg-based alloy wrought material.

### Claim 15 (depends on 8)

The Mg-based alloy wrought material according to claim 8, wherein an area enclosed by a nominal stress-and-nominal strain curve in a stress-strain diagram obtained by a room temperature compression test with an initial strain rate: at least 1×10−3 s−1 exhibits at least 200 kJ with respect to the Mg-based alloy wrought material.

### Claim 16 (depends on 9)

The Mg-based alloy wrought material according to claim 9, wherein an area enclosed by a nominal stress-and-nominal strain curve in a stress-strain diagram obtained by a room temperature compression test with an initial strain rate: at least 1×10−3 s−1 exhibits at least 200 kJ with respect to the Mg-based alloy wrought material.

### Claim 17 (depends on 10)

The Mg-based alloy wrought material according to claim 10, wherein an area enclosed by a nominal stress-and-nominal strain curve in a stress-strain diagram obtained by a room temperature compression test with an initial strain rate: at least 1×10−3 s−1 exhibits at least 200 kJ with respect to the Mg-based alloy wrought material.

### Claim 18 (depends on 11)

The Mg-based alloy wrought material according to claim 11, wherein an area enclosed by a nominal stress-and-nominal strain curve in a stress-strain diagram obtained by a room temperature compression test with an initial strain rate: at least 1×10−3 s−1 exhibits at least 200 kJ with respect to the Mg-based alloy wrought material.

### Claim 19 (depends on 2)

A method of manufacturing a Mg-based alloy wrought material as described in claim 2, the method comprising:
performing the solution treatment of a Mg-based alloy cast material having been melted and cast at a temperature of at least 400 degree Celsius and not exceeding 650 degree Celsius for at least 0.5 hours and not exceeding 48 hours and,
performing a hot plastic working for the treated material at a temperature of at least 50 degree Celsius and not exceeding 550 degree Celsius with at least 70% of cross-section reduction rate as a process of applying plastic strain.

### Claim 20 (depends on 19)

The method of manufacturing the Mg-based alloy wrought material according to claim 19, wherein the process of applying plastic strain comprises any one of extrusion, forging, rolling, and drawing.