# US 2021/0079501 A1 · Low cost high ductility cast aluminum alloy

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0079501 A1
- Document ID: US20210079501A1
- Status: Published application
- Kind: A1
- Application number: 17/079,818
- Filed: 2020-10-26
- Published: 2021-03-18
- Earliest claimed: 2015-03-17
- Applicants: Magna International Inc.
- Inventors: Juergen WUEST; Xiaoping NIU; Randy BEALS
- Web page: https://patentgrep.com/patent/US20210079501A1

## CPC

- C22C 21/02: with silicon as the next major constituent
- B22D 21/007: {with low melting point, e.g. Al 659 degrees C, Mg 650 degrees C}
- C22C 1/02: by melting {(C22C1/1036 takes precedence)}
- C22C 1/026: {Alloys based on aluminium}
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- B22D: CASTING OF METALS; CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES (shaping of plastics or substances in a plastic state B29C; metallurgical processing, selection of substances to be added to metal C21, C22)

## Abstract

An aluminum alloy for casting into a component, such as a vehicle component, is provided. The aluminum alloy includes 2 to 5 wt. % silicon, which is a lower amount of silicon compared to other aluminum alloys used for casting. The aluminum alloy further includes 1.0 to 2.0 wt. % zinc, less than 0.5 wt. % iron, and not greater than 0.6 wt. % manganese, based on the total weight of the aluminum alloy. The aluminum alloy can further include 0.01 to 0.07 wt. % strontium, 0.05 to 0.6 wt. % magnesium, not greater than 0.2 wt. % titanium, and less than 0.02 wt. % copper, based on the total weight of the aluminum alloy. After the casting step, the cast aluminum alloy has a yield strength of at least 110 MPa, ultimate tensile strength (UTS) of 220 to 230 MPa, and an elongation of 10 to 20%.

## Claims

### Claim 1

An aluminum alloy, comprising:
at least 80 weight percent (wt. %) aluminum, 2 to 5 wt. % silicon, 1.0 to 2.0 wt. % zinc, less than 0.5 wt. % iron, and not greater than 0.6 wt. % manganese, based on the total weight of the aluminum alloy.

### Claim 2 (depends on 1)

The aluminum alloy of claim 1 including 0.01 to 0.07 wt. % strontium, 0.05 to 0.6 wt. % magnesium, not greater than 0.2 wt. % titanium, and less than 0.02 wt. % copper, based on the total weight of the aluminum alloy.

### Claim 3 (depends on 1)

The aluminum alloy of claim 1, wherein the total amount of manganese and iron is 0.6 to 0.8 wt. %, based on the total weight of the aluminum alloy.

### Claim 4 (depends on 1)

The aluminum alloy of claim 1, wherein the alloy is cast and has a yield strength of at least 110 MPa, ultimate tensile strength (UTS) of 220 to 230 MPa, and an elongation of 10 to 20%.

### Claim 5 (depends on 1)

The aluminum alloy of claim 1 including at least 0.16 wt. % iron and at least 0.3 wt. % manganese, based on the total weight of the aluminum alloy.

### Claim 6 (depends on 2)

The aluminum alloy of claim 2 including at least 0.05 wt. % titanium and at least 0.006 wt. % copper, based on the total weight of the aluminum alloy.

### Claim 7 (depends on 1)

The aluminum alloy of claim 1, wherein the aluminum alloy is cast and formed into a component for a vehicle.

### Claim 8

A method of manufacturing a component, comprising the steps of:
casting an aluminum alloy, the aluminum alloy including at least 80 weight percent (wt. %) aluminum, 2 to 5 wt. % silicon, 1.0 to 2.0 wt. % zinc, less than 0.5 wt. % iron, and not greater than 0.6 wt. % manganese, based on the total weight of the aluminum alloy.

### Claim 9 (depends on 8)

The method of claim 8, wherein the aluminum alloy includes 0.01 to 0.07 wt. % strontium, 0.05 to 0.6 wt. % magnesium, not greater than 0.2 wt. % titanium, and less than 0.02 wt. % copper, based on the total weight of the aluminum alloy.

### Claim 10 (depends on 8)

The method of claim 8, wherein the aluminum alloy has a yield strength of at least 110 MPa, ultimate tensile strength (UTS) of 220 to 230 MPa, and an elongation of 10 to 20% after the casting step.

### Claim 11 (depends on 8)

The method of claim 8, wherein the aluminum alloy includes at least 0.16 wt. % iron and at least 0.3 wt. % manganese, based on the total weight of the aluminum alloy.

### Claim 12 (depends on 9)

The method of claim 9, wherein the aluminum alloy includes at least 0.05 wt. % titanium and at least 0.006 wt. % copper, based on the total weight of the aluminum alloy.

### Claim 13

A method of manufacturing an aluminum alloy, comprising the steps of:
melting a 300 series aluminum alloy; and
adding silicon to the melted 300 series aluminum alloy to form an improved aluminum alloy and so that the total amount of silicon present in the improved aluminum alloy is 2 to 5 wt. %, based on the total weight of the improved aluminum alloy, and the improved aluminum alloy further includes at least 80 weight percent (wt. %) aluminum, 1.0 to 2.0 wt. % zinc, less than 0.5 wt. % iron, and not greater than 0.6 wt. % manganese, based on the total weight of the improved aluminum alloy.

### Claim 14 (depends on 13)

The method of claim 13, wherein the improved aluminum alloy includes 0.01 to 0.07 wt. % strontium, 0.05 to 0.6 wt. % magnesium, not greater than 0.2 wt. % titanium, and less than 0.02 wt. % copper, based on the total weight of the improved aluminum alloy.

### Claim 15 (depends on 13)

The method of claim 13, wherein the improved aluminum alloy includes a total amount of manganese and iron of 0.6 to 0.8 wt. %, based on the total weight of the improved aluminum alloy.

### Claim 16 (depends on 13)

The method of claim 13 including casting the improved aluminum alloy, wherein the improved aluminum alloy has a yield strength of at least 110 MPa, ultimate tensile strength (UTS) of 220 to 230 MPa, and an elongation of 10 to 20% after the casting step.

### Claim 17 (depends on 16)

The method of claim 16, wherein the casting step includes forming the aluminum alloy into a component for a vehicle.

### Claim 18 (depends on 13)

The method of claim 13, wherein the improved aluminum alloy includes at least 0.16 wt. % iron and at least 0.3 wt. % manganese, at least 0.05 wt. % titanium, and at least 0.006 wt. % copper, based on the total weight of the improved aluminum alloy.

### Claim 19 (depends on 13)

The method of claim 13, wherein the 300 series aluminum alloy includes 91.3-93.2 wt. % aluminum, not greater than 0.10 wt. % copper, not greater than 0.12 wt. % iron, 0.30 to 0.45 wt. % magnesium, not greater than 0.05 wt. % manganese, 6.5 to 7.5 wt. % silicon, not greater than 0.20 wt. % titanium, not greater than 0.05 wt. % zinc, other elements each in an amount of not greater than 0.05 wt. %, and other elements in a total amount of not greater than 0.15 wt. %, based on the total weight of the improved aluminum alloy.

### Claim 20 (depends on 13)

The method of claim 13, wherein the 300 series aluminum alloy is obtained from recycled road wheels.