# US 2021/0079495 A1 · Process for the recovery of cobalt, lithium, and other metals from spent lithium-based batteries and other feeds

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0079495 A1
- Document ID: US20210079495A1
- Status: Published application
- Kind: A1
- Application number: 16/620,191
- Filed: 2018-06-08
- Published: 2021-03-18
- Earliest claimed: 2017-06-08
- Assignees: Urban Mining Pty Ltd; NMR 360 Inc
- Applicants: Urban Mining Pty Ltd; NMR 360 Inc
- Inventors: Bryn Harris; Carl White
- Web page: https://patentgrep.com/patent/US20210079495A1

## CPC

- C22B 7/007: {by acid leaching}
- C22B 3/08: Sulfuric acid {, other sulfurated acids or salts thereof}
- C22B 3/22: by physical processes, e.g. by filtration, by magnetic means {, or by thermal decomposition} (treatment or purification of solutions by liquid-liquid extraction C22B3/26)
- C22B 3/42: by ion-exchange extraction
- C22B 3/46: by substitution, e.g. by cementation
- C22B 7/005: {Separation by a physical processing technique only, e.g. by mechanical breaking}
- C22B 23/043: {Sulfurated acids or salts thereof}
- C22B 23/0461: {by chemical methods}
- C22B 23/0484: {in acidic type solutions}
- C22B 26/12: Obtaining lithium
- H01M 10/54: Reclaiming serviceable parts of waste accumulators
- Y02P 10/20: Recycling
- Y02W 30/84: Recycling of batteries or fuel cells
- C22B: PRODUCTION AND REFINING OF METALS (electrolytic C25); PRETREATMENT OF RAW MATERIALS
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS
- Y02W: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATER TREATMENT OR WASTE MANAGEMENT

## Abstract

A processes is disclosed for the recovery of cobalt, lithium and associated metals from lithium-ion batteries, comprising (i) shredding and pulverising the batteries under an inert atmosphere, (ii) leaching the batteries with sulphuric acid and sulphur dioxide under reducing conditions with a sub-stoichiometric amount of acid, (iii) recovery of copper by cementation, (iv) purification of the leach filtrate to precipitate iron and aluminium, along with some of the manganese and nickel if they are at low levels in the feed battery, (v) ion exchange to remove residual copper, nickel and manganese, (vi) precipitation of the purified solution with soda ash to recover all of the cobalt, and (vii) recovery of lithium as carbonate.

## Claims

### Claim 1

A method for recovering metals from waste lithium and cobalt containing feeds, including:
subjecting shredded and/or pulverised Li-battery waste to a sulphuric acid leach and sparging with SO2 gas to form a slurry including a leachate of soluble metal salts and a solid residue, wherein the soluble metal salts are a mixture of Co- and Li-salts and other metal salts in the form of metal sulphites and metal sulphates;
separating the leachate and the solid residue;
treating the leachate with an air sparge to oxidise and/or convert at least some of the soluble metal salts to insoluble metal salts, and form a Co- and Li-containing leachate and a precipitate of insoluble metal salts;
separating the Co- and Li-containing leachate and the precipitate of insoluble metal salts;
treating the Co- and Li-containing leachate with a precipitant to form an Li-containing leachate and a Co-containing precipitate; and
separating the Co-containing precipitate from the Li-containing leachate.

### Claim 2 (depends on 1)

The method of claim 1, wherein the sulphuric acid leach and sparging with SO2 are conducted under anoxic conditions.

### Claim 3 (depends on 1)

The method of claim 1, wherein sufficient sulphuric acid solution is added during the leach to provide a cobalt concentration of about 40 g/L to about 100 g/L.

### Claim 4 (depends on 1)

The method of claim 1, wherein a sub-stoichiometric amount of sulphuric acid is used in the sulphuric acid leach, based on an amount of metals in the Li-battery waste.

### Claim 5 (depends on 4)

The method of claim 4, wherein the sub-stoichiometric amount of sulphuric acid is from about 50 to about 90% of the stoichiometric amount of sulphuric acid.

### Claim 6 (depends on 1)

The method of claim 1, wherein a pH of the slurry is maintained at a value of from about 0 to about 4 during the sulphuric acid leach.

### Claim 7 (depends on 1)

The method of claim 1, wherein the sulphuric acid leach includes at least two stages:
a first stage of adding from about 10 to about 30% of the total sulphuric acid; and
a second stage of adding a remainder of the total sulphuric acid while sparging with SO2 gas.

### Claim 8 (depends on 7)

The method of claim 7, wherein during the first stage, the temperature is maintained at or below 75° C.

### Claim 9 (depends on 1)

The method of claim 1, wherein the other metal salts include one or more metal salts selected from the group consisting of: Mn, Fe, Ni, Cu, and Al.

### Claim 10 (depends on 1)

The method of claim 1, wherein the other metal salts include at least iron in the form of iron sulphite, and wherein the step of treating the leachate with the air sparge oxidises and/or converts the iron sulphite to one or more insoluble iron salts.

### Claim 11 (depends on 1)

The method of claim 1, wherein the other metal salts include at least Mn;
wherein when Mn is present in an amount of less than 2 g/L, the step of treating the leachate with the air sparge further includes adjusting the pH to a value of from about 4 to about 5 with a hydroxide to convert the Mn to one or more insoluble Mn salts; or
wherein when Mn is present in an amount of from about 2 g/L to about 5 g/L, the Co- and Li-containing leachate further includes Mn, and prior to the step of treating the Co- and Li-containing leachate with the precipitant, the method further includes:
contacting the leachate with an ion exchange resin to adsorb the Mn from the Co- and Li-containing leachate to a surface of the resin to form an Mn-loaded resin.

### Claim 12 (depends on 11)

The method of claim 11, wherein the method further includes recovering Mn from the Mn-loaded resin.

### Claim 13 (depends on 1)

The method of claim 1, wherein the other metal salts include at least Ni;
wherein when Ni is present in an amount of less than 2 g/L, the step of treating the leachate with the air sparge further includes adjusting the pH to a value of from about 4.5 to about 5 to convert the Ni to one or more insoluble Ni salts; or
wherein when Ni is present in an amount of from about 2 g/L to about 5 g/L], the Co- and Li-containing leachate further includes Ni, and prior to the step of treating the Co- and Li-containing leachate with the precipitant, the method further includes:
contacting the leachate with an ion exchange resin to adsorb the Ni from the Co- and Li-containing leachate to a surface of the resin to form an Ni-loaded resin.

### Claim 14 (depends on 13)

The method of claim 13, wherein the method further includes recovering Ni from the Ni-loaded resin.

### Claim 15 (depends on 1)

The method of claim 1, wherein the other metal salts include at least Cu;
wherein when Cu is present in an amount of greater than 1 g/L, prior to the step of treating the leachate with the air sparge, the method further includes a copper cementation step to produce metallic Cu, and a separation step of removing metallic Cu from the leachate; or
wherein when Cu is present in an amount of 1 g/L or less, the Co- and Li-containing leachate further includes Cu, and prior to the step of treating the Co- and Li-containing leachate with the precipitant, the method further includes:
contacting the leachate with an ion exchange resin to adsorb the Cu from the Co- and Li-containing leachate to a surface of the resin to form an Cu-loaded resin.

### Claim 16 (depends on 15)

The method of claim 15, wherein the method further includes recovering Cu from the Cu-loaded resin.

### Claim 17 (depends on 1)

The method of claim 1, wherein after the step of separating the leachate and the solid residue, and prior to the step of treating the leachate with the air sparge, the method further includes treating the leachate with activated carbon to remove dissolved organic compounds.

### Claim 18 (depends on 1)

The method of claim 1, wherein the step of treating the Co- and Li-containing leachate with the precipitant to form the Li-containing leachate and the Co-containing precipitate further includes:
a preliminary precipitation step including:
treating the Co- and Li-containing leachate with sufficient precipitant to form an amount of a preliminary Co-containing precipitate corresponding to about 5 to about 20 wt % of the total Co originally in the Co- and Li-containing leachate; and
separating the preliminary Co-containing precipitate from the Co- and Li-containing leachate; and
recycling the preliminary Co-containing precipitate to the leachate.

### Claim 19 (depends on 1)

The method of claim 1, wherein the Co-containing precipitate is substantially free of other metals.

### Claim 20 (depends on 1)

The method of claim 1, wherein the method further includes treating the Li-containing leachate with a precipitant to form an Li-containing precipitate substantially free of other metals.