# US 2021/0079490 A1 · Process for Local Hardening

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0079490 A1
- Document ID: US20210079490A1
- Status: Published application
- Kind: A1
- Application number: 17/008,968
- Filed: 2020-09-01
- Published: 2021-03-18
- Earliest claimed: 2019-09-13
- Assignees: Robert Bosch GmbH
- Applicants: Robert Bosch GmbH
- Inventors: Hermann Autenrieth; Marcus Hansel; Michael Cesinger; Thomas Waldenmaier
- Web page: https://patentgrep.com/patent/US20210079490A1

## CPC

- C21D 5/00: Heat treatments of cast-iron
- C21D 1/18: Hardening (C21D1/02 takes precedence); Quenching with or without subsequent tempering (quenching devices C21D1/62)
- C21D 1/42: Induction heating
- C21D 2211/009: Pearlite
- C21D 2221/00: Treating localised areas of an article
- Y02P 10/25: Process efficiency
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A process for the local hardening of a workpiece by means of local induction hardening includes performing a local perlitization grain transformation on the workpiece after a local inductive diffusion heat treatment and before a local induction hardening on the workpiece.

## Claims

### Claim 1

A process for the local hardening of a workpiece comprising:
performing a local inductive diffusion heat treatment on the workpiece;
performing a local perlitization grain transformation on the workpiece after the local inductive diffusion heat treatment; and
performing a local induction hardening on the workpiece after preforming the local perlitization grain transformation on the workpiece.

### Claim 2 (depends on 1)

The process according to claim 1, wherein a duration of the local inductive diffusion heat treatment is brief compared to a duration of the local induction hardening.

### Claim 3 (depends on 2)

The process according to claim 2, wherein a duration of the local perlitization grain transformation is comparable to the duration of the local induction hardening.

### Claim 4 (depends on 3)

The process according to claim 3, wherein the local diffusion heat treatment is carried out at a temperature which is the same or slightly lower than a temperature at which the local induction hardening is carried out.

### Claim 4 (depends on 4)

The process according to claim 4, wherein the local perlitization grain transformation is carried out at a temperature which is significantly lower than the temperature at which the local induction hardening is carried out.

### Claim 6 (depends on 3)

The process according to claim 3, wherein the local perlitization grain transformation is carried out at a temperature which is significantly lower than a temperature at which the local induction hardening is carried out.

### Claim 7 (depends on 3)

The process according to claim 3, wherein
the local diffusion heat treatment is carried out at a temperature which is the same or slightly lower than a temperature at which the local induction hardening is carried out; and
the local perlitization grain transformation is carried out at a temperature which is significantly lower than the temperature at which the local induction hardening is carried out.

### Claim 8 (depends on 2)

The process according to claim 2, wherein the local perlitization grain transformation is carried out at a temperature which is significantly lower than a temperature at which the local induction hardening is carried out.

### Claim 9 (depends on 1)

The process according to claim 1, wherein a duration of the local perlitization grain transformation is comparable to the duration of the local induction hardening.

### Claim 10 (depends on 9)

The process according to claim 9, wherein the local diffusion heat treatment is carried out at a temperature which is the same or slightly lower than a temperature at which the local induction hardening is carried out.

### Claim 11 (depends on 10)

The process according to claim 10, wherein the local perlitization grain transformation is carried out at a temperature which is significantly lower than the temperature at which the local induction hardening is carried out.

### Claim 12 (depends on 9)

The process according to claim 9, wherein the local perlitization grain transformation is carried out at a temperature which is significantly lower than a temperature at which the local induction hardening is carried out.

### Claim 13 (depends on 1)

The process according to claim 1, wherein the local diffusion heat treatment is carried out at a temperature which is the same or slightly lower than a temperature at which the local induction hardening is carried out.

### Claim 14 (depends on 13)

The process according to claim 13, wherein the local perlitization grain transformation is carried out at a temperature which is significantly lower than the temperature at which the local induction hardening is carried out.

### Claim 15 (depends on 1)

The process according to claim 1, wherein the local perlitization grain transformation is carried out at a temperature which is significantly lower than a temperature at which the local induction hardening is carried out.

### Claim 16 (depends on 1)

The process according to claim 1, wherein the workpiece is a cast iron workpiece.

### Claim 17 (depends on 16)

The process according to claim 16, wherein a duration of the local inductive diffusion heat treatment is between 30 percent and 80 percent of a duration of the local induction hardening.

### Claim 18 (depends on 17)

The process according to claim 17, wherein a duration of the local perlitization grain transformation is between 80 percent and 120 percent the duration of the local induction hardening.

### Claim 19 (depends on 18)

The process according to claim 18, wherein:
the local diffusion heat treatment is carried out at a temperature between 900° C. and 1150° C.; and
the local perlitization grain transformation is carried out at a temperature of between 500° C. and 800° C.

### Claim 20 (depends on 19)

The process according to claim 19, wherein the local induction hardening is carried out at about 1050° C.