# US 2021/0079272 A1 · Method for producing articles coated with adhesive

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0079272 A1
- Document ID: US20210079272A1
- Status: Published application
- Kind: A1
- Application number: 16/970,486
- Filed: 2019-02-15
- Published: 2021-03-18
- Earliest claimed: 2018-02-21
- Assignees: BASF SE
- Applicants: BASF SE
- Inventors: Christoph KIENER; Lars HECKHOFF; Peter PREISHUBER-PFLUEGL; Richard BOCIEK
- Web page: https://patentgrep.com/patent/US20210079272A1

## CPC

- C09J 7/385: {Acrylic polymers}
- C09J 179/00: Adhesives based on macromolecular compounds obtained by reactions forming in the main chain of the macromolecule a linkage containing nitrogen, with or without oxygen, or carbon only, not provided for in groups C09J161/00 - C09J177/00
- B32B 37/1284: {Application of adhesive}
- B32B 37/20: involving the assembly of continuous webs only
- C08L 39/06: Homopolymers or copolymers of N-vinyl-pyrrolidones
- C09J 133/02: Homopolymers or copolymers of acids; Metal or ammonium salts thereof
- C09J 139/06: Homopolymers or copolymers of N-vinyl-pyrrolidones
- C09J 175/04: Polyurethanes
- B05D 1/28: performed by transfer from the surfaces of elements carrying the liquid or other fluent material, e.g. brushes, pads, rollers
- B05D 5/10: to obtain an adhesive surface
- B05D 2201/04: Laminate
- B05D 2502/00: Acrylic polymers
- B32B 2309/14: Velocity, e.g. feed speeds
- C09J 2301/302: the adhesive being pressure-sensitive, i.e. tacky at temperatures inferior to 30°C
- C09J 2433/00: Presence of (meth)acrylic polymer
- C09J 2475/00: Presence of polyurethane
- C09J: ADHESIVES; NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL; ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE; USE OF MATERIALS AS ADHESIVES (preparation of glue or gelatine C09H)
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- B05D: PROCESSES FOR APPLYING FLUENT MATERIALS TO SURFACES, IN GENERAL (conveying articles or workpieces through baths of liquid B65G, e.g. B65G49/02)

## Abstract

Described is a process for producing adhesive-coated articles, wherein an aqueous dispersion adhesive composition comprising a dispersed adhesive polymer and a dissolved polyvinylpyrrolidone is applied at high web speed to a film substrate using a coating machine having at least one rotating roller and wherein the coated film substrate may optionally be bonded to a further substrate. Also described is the use of polyvinylpyrrolidone as a defoamer for aqueous dispersion adhesive compositions applied to a film substrate using a coating machine having a rapidly rotating roller.

## Claims

### Claim 1

A process for producing adhesive-coated articles, comprising:
applying an aqueous dispersion adhesive composition to a film substrate using a coating machine with at least one rotating roller,
wherein the aqueous dispersion adhesive composition comprises
at least one adhesive polymer dispersed in the aqueous phase and
at least one polyvinylpyrrolidone dissolved in the aqueous phase,
wherein the web speed of the film substrate is not less than 150 m/min, and
wherein the coated film substrate is optionally bonded to a further substrate.

### Claim 2 (depends on 1)

The process of claim 1, wherein the adhesive-coated articles are selected from the group consisting of laminates and pressure-sensitive adhesive articles.

### Claim 3 (depends on 1)

The process of claim 1, wherein the adhesive-coated articles are composite films, and
wherein at least two films are bonded to one another using the aqueous dispersion adhesive composition.

### Claim 4 (depends on 1)

The process of claim 1, wherein in the Billhöfer foam test measured at 250 m/min, the aqueous dispersion adhesive composition exhibits a value of greater than 120 minutes.

### Claim 5 (depends on 1)

The process of claim 1, wherein the at least one polyvinylpyrrolidone has a K value of 25 to 100 measured at 25° C. as a 1% solution in water.

### Claim 6 (depends on 1)

The process of claim 1, wherein the aqueous dispersion adhesive composition comprises
from 30% to 60% by weight of the at least one adhesive polymer and
from 0.02% to 2% by weight of the at least one polyvinylpyrrolidone, each relative to a total weight of the aqueous dispersion adhesive composition.

### Claim 7 (depends on 1)

The process of claim 1, wherein the at least one adhesive polymer has a glass transition temperature of −40° C. to +15° C., as measured by differential scanning calorimetry at a heating rate of 20° C./min.

### Claim 8 (depends on 1)

The process of claim 1,
wherein the at least one adhesive polymer is selected from the group consisting of polyurethanes and polymers producible by free-radical emulsion polymerization of ethylenically unsaturated, free-radically polymerizable monomers comprising
a) at least 60% by weight, based on the total amount of monomers, of at least one monomer selected from the group consisting of C1- to C20-alkyl acrylates, C1- to C20-alkyl methacrylates, vinyl esters of carboxylic acids comprising up to 20 carbon atoms, vinylaromatics having up to 20 carbon atoms, vinyl halides, vinyl ethers of alcohols comprising 1 to 10 carbon atoms, aliphatic hydrocarbons having 2 to 8 carbon atoms and one or two double bonds, and mixtures of these monomers,
b) at least 0.1% by weight, based on the total amount of monomers, of at least one monomer having at least one acid group; and
c) optionally at least one further monomer distinct from the monomers a) and b).

### Claim 9 (depends on 1)

The process of claim 1, wherein the at least one adhesive polymer is at least one polyurethane constructed from
a) at least one monomeric diisocyanate,
b) at least one diol, of which
b1) 10 to 100 mol %, based on the total amount of the diols (b), have a molecular weight of 500 to 5000 g/mol and
b2) 0 to 90 mol %, based on the total amount of the diols (b), have a molecular weight of 60 to 500 g/mol,
c) at least one monomer distinct from the monomers (a) and (b) having at least one isocyanate group or at least one isocyanate-reactive group which further bears at least one hydrophilic group or a potentially hydrophilic group, and
d) optionally at least one further compound distinct from the monomers (a) to (c) having at least two reactive groups selected from the group consisting of alcoholic hydroxyl groups, primary amino groups, secondary amino groups, and isocyanate groups, and
e) optionally at least one monofunctional compound distinct from the monomers (a) to (d) having a reactive group which is at least one selected from the group consisting of an alcoholic hydroxyl group, a primary or secondary amino group, and an isocyanate group.

### Claim 10 (depends on 9)

The process of claim 9, wherein:
the at least one monomeric diisocyanate a) is selected from diisocyanates of the formula X(NCO)2, wherein X represents at least one selected from the group consisting of an acyclic aliphatic hydrocarbon radical having 4 to 15 carbon atoms, a cycloaliphatic hydrocarbon radical having 6 to 15 carbon atoms, an aromatic hydrocarbon radical having 6 to 15 carbon atoms, and an araliphatic hydrocarbon radical having 7 to 15 carbon atoms;
the diols b1) are selected from the group consisting of polyester diols, polycarbonate diols, and polyether diols; and
the compound c) is selected from the group consisting of dihydroxycarboxylic acids, diaminocarboxylic acids, and diaminosulfonic acids.

### Claim 11 (depends on 9)

The process of claim 9, wherein the content of anionic or potentially anionic groups in the at least one polyurethane is 30 to 1000 mmol/kg of the at least one polyurethane.

### Claim 12 (depends on 1)

The process claim 1, wherein the at least one adhesive polymer is producible by free-radical emulsion polymerization of ethylenically unsaturated, free-radically polymerizable monomers comprising:
a) 60% to 99.9% by weight, based on the total amount of monomers, of at least one monomer selected from the group consisting of C1- to C20-alkyl acrylates, C1- to C20-alkyl methacrylates, and vinylaromatics having up to 20 carbon atoms; and
b) 0.1% to 5% by weight, based on the total amount of monomers, of at least one monomer having at least one acid group selected from acrylic acid, methacrylic acid, and itaconic acid; and
c) 0% to 10% by weight, based on the total amount of monomers, of further monomers distinct from the monomers a) to b), selected from the group consisting of acrylamide, methacrylamide, N-methylolacrylamide, N-methylolmethacrylamide, phenyloxyethylglycol mono(meth)acrylate, hydroxyl-comprising monomers, amino-comprising monomers, nitriles, alpha,beta-monoethylenically unsaturated C3-C8-carboxylic acids, bifunctional monomers which comprise not only an ethylenically unsaturated double bond but also at least one glycidyl group, bifunctional monomers which comprise not only an ethylenically unsaturated double bond but also at least one oxazoline group, bifunctional monomers which comprise not only an ethylenically unsaturated double bond but also at least one ureido group, bifunctional monomers which comprise not only an ethylenically unsaturated double bond but also at least one ureido-analogous group, and crosslinking monomers having more than one free-radically polymerizable group.

### Claim 13 (depends on 8)

The process of claim 8, wherein the monomers a) are at least one selected from the group consisting of C1- to C10-alkyl acrylates, C1- to C10-alkyl methacrylates, and styrene.

### Claim 14 (depends on 8)

The process of claim 8, wherein the monomers a) are employed in an amount of at least 80% by weight, based on the total amount of the monomers, and are at least one selected from the group consisting of C1- to C10-alkyl acrylates, C1- to C10-alkyl methacrylates, styrene, and a mixture thereof; and
wherein the monomers b) are employed in an amount of 0.5% to 5% by weight, based on the total amount of the monomers, and are at least one selected from the group consisting of acrylic acid, methacrylic acid, itaconic acid, and a mixture thereof.

### Claim 15 (depends on 1)

The process of claim 1, wherein the at least one adhesive polymer dispersed in the aqueous phase is a styrene/acrylate copolymer formed from a monomer mixture comprising styrene and at least one monomer selected from the group consisting of C1- to C20-alkyl acrylates and C1- to C20-alkyl methacrylates.

### Claim 16 (depends on 1)

The process of claim 1, wherein the aqueous dispersion adhesive composition comprises water-dispersed polymer particles having an average particle diameter of greater than 200 nm,
wherein the water-dispersed polymer particles have a monomodal particle size distribution and a uniform glass transition temperature,
wherein the water-dispersed polymer particles are produced by free-radical emulsion polymerization of a single monomer mixture comprising ethylenically unsaturated, free-radically polymerizable monomers and less than 0.8 parts by weight of emulsifier, based on 100 parts by weight of monomers,
wherein the water-dispersed polymer particles are produced using a polymer seed, without addition of protective colloids, and without formation of protective colloids in situ,
wherein the single monomer mixture comprises:
a) at least 60% by weight, based on the total amount of monomers, of at least one monomer selected from the group consisting of C1- to C20-alkyl acrylates, C1- to C20-alkyl methac-rylates, vinyl esters of carboxylic acids comprising up to 20 carbon atoms, vinylaromatics having up to 20 carbon atoms, vinyl halides, vinyl ethers of alcohols comprising 1 to 10 carbon atoms, aliphatic hydrocarbons having 2 to 8 carbon atoms and one or two double bonds, and mixtures of these monomers,
b) at least 0.1% by weight, based on the total amount of monomers, of at least one monomer having at least one acid group; and
c) optionally at least one further monomer distinct from the monomers a) and b);
wherein the feeding of the monomer mixture is carried out during the polymerization at a first feed rate and at least one second feed rate,
wherein the first feed rate is slower than the second feed rate,
wherein the acid groups of the monomers b) are fully or partially neutralized by feeding of a base during the emulsion polymerization, and
wherein the feeding of the base commences during the emulsion polymerization once at least 5% by weight of the total monomer mixture is present in the reaction vessel under polymerization conditions.

### Claim 17 (depends on 1)

The process of claim 1, wherein the aqueous dispersion adhesive composition further comprises at least one crosslinkable adhesive polymer dispersed in the aqueous phase and at least one reactive crosslinker.

### Claim 18 (depends on 17)

The process of claim 17, wherein the at least one reactive crosslinker is a polyisocyanate.

### Claim 19 (depends on 18)

The process of claim 18, wherein the film substrate comprises at least one selected from the group consisting of polyethylene, oriented polypropylene, unoriented polypropylene, polyamide, polyethylene terephthalate, polyacetate, cellophane, metallized films, and metal foils.

### Claim 20 (depends on 1)

The process of claim 1, wherein the aqueous dispersion adhesive composition is free from defoamers based on silicone and/or is free from defoamers based on organic oils.

### Claim 21

A method for producing films mechanically coated with an aqueous dispersion adhesive composition or for laminating rigid shaped articles with flexible decorative films mechanically coated with an aqueous dispersion adhesive composition, the method comprising:
applying the aqueous dispersion adhesive composition to a film substrate by means of a coating machine having at least one rotating roller,
wherein the web speed of the film substrate is at least 150 m/minute, and
wherein the aqueous dispersion adhesive composition comprises:
(a) at least one adhesive polymer dispersed in the aqueous phase and
(b) polyvinylpyrrolidone dissolved in the aqueous phase.

### Claim 22

A method of producing a coated film substrate, comprising:
applying an aqueous dispersion adhesive composition to a film substrate using a coating machine having at least one rotating roller,
wherein the web speed of the film substrate is at least 150 m/minute, and
wherein the aqueous dispersion adhesive composition comprises polyvinylpyrrolidone as a defoamer.