# US 2021/0079263 A1 · High molecular weight polyvinyl pyrrolidone for low-k removal rate suppresion

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0079263 A1
- Document ID: US20210079263A1
- Status: Published application
- Kind: A1
- Application number: 16/987,632
- Filed: 2020-08-07
- Published: 2021-03-18
- Earliest claimed: 2019-09-17
- Assignees: Fujimi Incorporated
- Applicants: Fujimi Incorporated
- Inventors: Jimmy Erik GRANSTROM
- Web page: https://patentgrep.com/patent/US20210079263A1

## CPC

- C09G 1/02: containing abrasives or grinding agents {(abrasives as such C09K3/14; polishing of semi-conductors H10P52/40)}
- B24B 37/044: {characterised by the composition of the lapping agent}
- C09G: POLISHING COMPOSITIONS (French polish C09F11/00); SKI WAXES
- B24B: MACHINES, DEVICES, OR PROCESSES FOR GRINDING OR POLISHING (grinding of gear teeth B23F, of screw-threads B23G1/36; by electro-erosion B23H; abrasive or related blasting B24C; tools for grinding, buffing or sharpening B24D; polishing compositions C09G1/00; abrasives C09K3/14; electrolytic etching or polishing C25F3/00; grinding arrangements for use on assembled railway tracks E01B31/17); DRESSING OR CONDITIONING OF ABRADING SURFACES; FEEDING OF GRINDING, POLISHING, OR LAPPING AGENTS

## Abstract

Provided herein are compositions and methods for polishing surfaces comprising one or more low-k materials and optionally one or more additional materials (e.g., Cu, Ta, Co, Ni, etc.), e.g., in semiconductor device fabrication. Embodiments include a composition for chemical mechanical polishing of a surface comprising a low-k material (e.g., Black Diamond (BD)) the composition comprising an abrasive, a solvent, and a polymeric low-k suppressor.

## Claims

### Claim 1

A chemical mechanical polishing slurry, comprising
an abrasive;
a solvent; and
a polymeric low-k suppressor with Mw×C2>0.5 mg/mol, where Mw is weight average molecular weight and C is concentration,
wherein the Mw is greater than 4 kg/mol and the concentration of polymeric low-k suppressor is ≥0.01 wt-%.

### Claim 2 (depends on 1)

The chemical mechanical polishing slurry of claim 1, wherein the polymeric low-k suppressor has a Mw×C2>1.5 mg/mol.

### Claim 3 (depends on 1)

The chemical mechanical polishing slurry of claim 1, wherein the polymeric low-k suppressor has a Mw×C2>2.5 mg/mol.

### Claim 4 (depends on 1)

The chemical mechanical polishing slurry of claim 1, wherein the weight average molecular weight of polymeric low-k suppressor is greater than 6 kg/mol.

### Claim 5 (depends on 1)

The chemical mechanical polishing slurry of claim 1, wherein the weight average molecular weight of polymeric low-k suppressor is greater than 40 kg/mol.

### Claim 6 (depends on 1)

The chemical mechanical polishing slurry of claim 1, wherein the weight average molecular weight of the polymeric low-k suppressor is greater than 250 kg/mol.

### Claim 7 (depends on 1)

The chemical mechanical polishing slurry of claim 1, wherein the weight average molecular weight of the polymeric low-k suppressor is greater than 390 kg/mol.

### Claim 8 (depends on 1)

The chemical mechanical polishing slurry of claim 1, wherein the weight average molecular weight of polymeric low-k suppressor is equal to or less than 3,000 kg/mol.

### Claim 9 (depends on 1)

The chemical mechanical polishing slurry of claim 1, wherein the polymeric low-k suppressor contains one or more carbonyl group(s), and optionally also one or more ethoxylated unit(s).

### Claim 10 (depends on 1)

The chemical mechanical polishing slurry of claim 1, wherein the polymeric low-k suppressor is selected from the group consisting of polyvinyl pyrrolidone (PVP), aliphatic polyketones, poly (vinyl methyl ketone), poly (N-hydroxy propyl)methacrylamide, poly (N-vinyl acetamide), polylactic acid, poly(N-butyl methacrylate), poly(N-vinylpyrrolidone/vinyl acetate) and poly(ethylene oxide).

### Claim 11 (depends on 1)

The chemical mechanical polishing slurry of claim 1, wherein the slurry has a pH of 9-12.

### Claim 12 (depends on 1)

The chemical mechanical polishing slurry of claim 1, wherein the polymeric low-k suppressor in the slurry is capable of selectively suppressing removal of a low-k material.

### Claim 13 (depends on 1)

The chemical mechanical polishing slurry of claim 1, wherein the low-k material is selected from the group consisting of SiOC or SiOCH.

### Claim 14 (depends on 1)

A method of suppressing removal of a low-k material, comprising polishing a substrate comprising the low-k material, and an additional material with a chemical mechanical polishing slurry of claim 1, wherein the additional material is selectively removed at a higher rate than the low-k material.