# US 2021/0079256 A1 · High-durability antifogging coating film and coating composition

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0079256 A1
- Document ID: US20210079256A1
- Status: Published application
- Kind: A1
- Application number: 16/971,842
- Filed: 2019-02-21
- Published: 2021-03-18
- Earliest claimed: 2018-02-23
- Assignees: Asahi Kasei Kabushiki Kaisha
- Applicants: Asahi Kasei Kabushiki Kaisha
- Inventors: Kazuya ISEDA; Kentaro SHIRAISHI; Mifuyu NIWA
- Web page: https://patentgrep.com/patent/US20210079256A1

## CPC

- C08G 18/706: {the liquid medium being water}
- C09D 175/04: Polyurethanes
- B32B 17/10: of synthetic resin
- C03C 17/009: {Mixtures of organic and inorganic materials, e.g. ormosils and ormocers}
- C03C 17/30: with silicon-containing compounds
- C08G 18/022: {the polymeric products containing isocyanurate groups}
- C08G 18/1875: {containing ammonium salts or mixtures of secondary of tertiary amines and acids}
- C08G 18/246: {containing also tin-carbon bonds}
- C08G 18/283: {Compounds containing ether groups, e.g. oxyalkylated monohydroxy compounds}
- C08G 18/285: {Nitrogen containing compounds}
- C08G 18/4833: {Polyethers containing oxyethylene units}
- C08G 18/4883: {containing cyclic groups having at least one oxygen atom in the ring}
- C08G 18/5096: {containing silicon}
- C08G 18/718: {containing silicon}
- C08G 18/791: {containing isocyanurate groups}
- C08G 18/8064: {with monohydroxy compounds}
- C09D 5/00: Coating compositions, e.g. paints, varnishes or lacquers, characterised by their physical nature or the effects produced {(electrically insulating plastics, resins or waxes H01B3/30)}; Filling pastes
- C09D 5/024: {characterised by the additives}
- C09D 7/47: Levelling agents
- C09D 7/61: inorganic
- C09D 7/62: modified by treatment with other compounds
- C03C 2217/75: Hydrophilic and oleophilic coatings
- C08G 2290/00: Compositions for creating anti-fogging
- C08K 3/36: Silica
- C08K 9/06: with silicon-containing compounds
- C08K 9/08: Ingredients agglomerated by treatment with a binding agent
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)

## Abstract

The problem addressed by the present invention is to provide an antifogging coating film having excellent antifogging property, antifogging persistence, persistence of appearance, and elution resistance. The coating film according to the present invention contains a metal oxide (A) and a hydrophilic compound (B); the height of the eluate by a coating film surface elution test is 1.0 μm or less; this test is carried out by placing 10 μL of deionized water on the coating film, allowing the film to stand for 24 hours in a 23° C., 50% RH environment, measuring the eluate height of 20 locations selected randomly within a 10 cm2 range on the coating film surface, and determining the maximum height; and the water contact angle measured after subjecting the coating film to a moisture resistance test by exposure for 24 hours in an 85° C., 85% RH environment followed by standing for one hour in a 23° C., 50% RH environment, is less than 40°. Preferably, the elution level per coating film unit volume by a coating film total elution test is 40 mg/cm3 or less, and this test is carried out by immersing the coating film in 23° C. deionized water for 24 hours, then measuring the weight of the coating film eluate recovered from the deionized water.

## Claims

### Claim 1

A coating film comprising a metal oxide (A), and a hydrophilic compound (B), wherein a height of an eluate in a coating film surface elution test is 1.0 μm or less,
the coating film surface elution test is carried out by placing 10 μL of deionized water on the coating film, allowing the coating film to stand in a 23° C., 50% RH environment for 24 hours, measuring heights of the eluate at 20 locations selected randomly within a 10 cm2 range on a surface of the coating film, and determining a maximum height, and
a water contact angle measured after subjecting the coating film to a moisture resistance test, in which the coating film is exposed to an 85° C., 85% RH environment for 24 hours and then allowed to stand in a 23° C., 50% RH environment for 1 hour, is less than 40°.

### Claim 2 (depends on 1)

The coating film according to claim 1, wherein an elution level per coating film unit volume in a coating film total elution test is 40 mg/cm3 or less, and the coating film total elution test is carried out by immersing the coating film in deionized water at 23° C. for 24 hours and measuring a weight of an eluate of the coating film recovered from the deionized water.

### Claim 3 (depends on 1)

The coating film according to claim 1, wherein an elution level per coating film unit volume in a coating film total elution test is 40 mg/cm3 or less, and the coating film total elution test is carried out by immersing the coating film in deionized water at 80° C. for 24 hours and measuring a weight of an eluate of the coating film recovered from the deionized water.

### Claim 4 (depends on 1)

The coating film according to claim 1, wherein a value of a water contact angle is less than 40°.

### Claim 5 (depends on 1)

The coating film according to claim 1, wherein the metal oxide (A) has a hydroxy group.

### Claim 6 (depends on 1)

The coating film according to claim 1, wherein the metal oxide (A) is silica.

### Claim 7 (depends on 1)

The coating film according to claim 1, wherein the hydrophilic compound (B) is bonded to a surface of the metal oxide via a non-covalent bond and/or a covalent bond.

### Claim 8 (depends on 1)

The coating film according to claim 1, further comprising an isocyanate compound (C).

### Claim 9 (depends on 1)

The coating film according to claim 1, wherein the hydrophilic compound (B) is at least one selected from the group consisting of a nonionic compound, an anionic compound, and a zwitterionic compound.

### Claim 10 (depends on 1)

The coating film according to claim 1, wherein the hydrophilic compound (B) has a carbon-oxygen bond in the molecule.

### Claim 11 (depends on 1)

The coating film according to claim 1, wherein the hydrophilic compound (B) has an alkylene glycol moiety in the molecule.

### Claim 12 (depends on 1)

The coating film according to claim 1, wherein the hydrophilic compound (B) is bonded to each other via a urethane bond and/or a siloxane bond.

### Claim 13 (depends on 1)

The coating film according to claim 1, wherein the isocyanate compound (C) is a water-dispersible isocyanate compound.

### Claim 14 (depends on 1)

The coating film according to claim 1, wherein the isocyanate compound (C) has an alkoxysilane moiety and/or a siloxane moiety in the molecule.

### Claim 15 (depends on 1)

The coating film according to claim 1, wherein the isocyanate compound (C) is a blocked isocyanate.

### Claim 16 (depends on 1)

The coating film according to claim 1, further comprising polymer particles (D).

### Claim 17 (depends on 1)

The coating film according to claim 1, wherein ΔHAZE is less than 1.0, the ΔHAZE being a difference between a HAZE of the coating film after being subjected to a moisture resistance test in which the coating film is exposed to an environment of 85° C., 85% RH for 24 hours and then allowed to stand in an environment of 23° C., 50% RH for 1 hour, and a HAZE of the coating film before the moisture resistance test.

### Claim 18 (depends on 1)

A coating composition for producing the coating film according to claim 1, wherein the metal oxide (A) is constituted by an alkoxysilane and/or a hydrolysate or a condensate of alkoxysilane.

### Claim 19 (depends on 1)

A coating composition for producing the coating film according to claim 1, wherein the metal oxide (A) is silicone particles and/or acrylic silicone particles.

### Claim 20 (depends on 1)

A coating composition for producing the coating film according to claim 1, wherein the hydrophilic compound (B) contains an alkoxysilane and/or a silanol group in the molecule.

### Claim 21 (depends on 1)

A coating composition for producing the coating film according to claim 1, wherein the hydrophilic compound (B) has a polyalkylene oxide chain in the molecule and contains a primary aliphatic hydroxy group at one end of the polyalkylene oxide chain and an alkoxysilane and/or a silanol group at the other end.

### Claim 22 (depends on 1)

A coating composition for producing the coating film according to claim 1, the coating composition comprising a metal oxide (A), a hydrophilic compound (B), and optionally an isocyanate compound (C) and/or polymer particles (D) and/or water.

### Claim 23 (depends on 18)

The coating composition according to claim 18, wherein the hydrophilic compound (B) has three or more functional groups capable of reacting with an isocyanate group in the molecule.

### Claim 24 (depends on 18)

The coating composition according to claim 18, wherein an HLB value of the hydrophilic compound (B) determined by a Griffin method is 10 or more.

### Claim 25 (depends on 1)

A laminate comprising a resin substrate and/or a glass substrate, and the coating film according to claim 1.

### Claim 26 (depends on 1)

Use of the coating film according to claim 1 for imparting antifogging properties to a resin substrate and/or a glass substrate.

### Claim 27 (depends on 1)

The coating film according to claim 1, wherein the coating film is used as an antifogging coating film.

### Claim 28 (depends on 1)

The coating film according to claim 1, wherein the coating film is used as a coating film for an automotive exterior part.

### Claim 29 (depends on 1)

The coating film according to claim 1, wherein the coating film is used as a coating film for a lamp cover.