# US 2021/0079209 A1 · Waterborne dispersions

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0079209 A1
- Document ID: US20210079209A1
- Status: Published application
- Kind: A1
- Application number: 16/772,994
- Filed: 2018-12-18
- Published: 2021-03-18
- Earliest claimed: 2017-12-19
- Assignees: Dsm IP Assets B.V.
- Applicants: Dsm IP Assets B.V.
- Inventors: Michael Arnoldus Jacobus SCHELLEKENS; Johannes Hendrikus DE BONT; John BARBOSA; Jon Andrew CRONIN; Charles SHEARER; Matthew Stewart GEBHARD; Gerardus Cornelis OVERBEEK
- Web page: https://patentgrep.com/patent/US20210079209A1

## CPC

- C08F 293/005: {using free radical "living" or "controlled" polymerisation, e.g. using a complexing agent}
- C08F 2/22: Emulsion polymerisation
- C08F 220/06: Acrylic acid; Methacrylic acid; Metal salts or ammonium salts thereof
- C08F 220/14: Methyl esters {, e.g. methyl (meth)acrylate}
- C08F 220/1804: {C4-(meth)acrylate, e.g. butyl (meth)acrylate, isobutyl (meth)acrylate or tert-butyl (meth)acrylate}
- C08F 220/56: Acrylamide; Methacrylamide
- C08F 287/00: Macromolecular compounds obtained by polymerising monomers on to block polymers
- C08J 7/0427: {with only one layer of a composition containing a polymer binder (with more layers C08J7/042)}
- C08J 7/043: Improving the adhesiveness of the coatings per se, e.g. forming primers (adhesives in the form of films or foils characterised by the primer layers between the polymer carriers and the adhesives C09J7/50)
- C08J 7/046: Forming abrasion-resistant coatings; Forming surface-hardening coatings
- C08J 7/056: Forming hydrophilic coatings
- C08K 3/22: of metals
- C08K 5/0025: {Crosslinking or vulcanising agents; including accelerators}
- C08K 5/25: Carboxylic acid hydrazides
- C08L 33/10: Homopolymers or copolymers of methacrylic acid esters
- C08L 53/00: Compositions of block copolymers containing at least one sequence of a polymer obtained by reactions only involving carbon-to-carbon unsaturated bonds; Compositions of derivatives of such polymers
- C09D 5/022: {Emulsions, e.g. oil in water}
- C09D 151/003: {grafted on to macromolecular compounds obtained by reactions only involving unsaturated carbon-to-carbon bonds (C09D151/04, C09D151/06 take precedence)}
- C09D 153/00: Coating compositions based on block copolymers containing at least one sequence of a polymer obtained by reactions only involving carbon-to-carbon unsaturated bonds; Coating compositions based on derivatives of such polymers
- C08F 2438/03: Use of a di- or tri-thiocarbonylthio compound, e.g. di- or tri-thioester, di- or tri-thiocarbamate, or a xanthate as chain transfer agent, e.g . Reversible Addition Fragmentation chain Transfer [RAFT] or Macromolecular Design via Interchange of Xanthates [MADIX]
- C08J 2327/06: Homopolymers or copolymers of vinyl chloride
- C08J 2433/10: Homopolymers or copolymers of methacrylic acid esters
- C08J 2453/00: Characterised by the use of block copolymers containing at least one sequence of a polymer obtained by reactions only involving carbon-to-carbon unsaturated bonds; Derivatives of such polymers
- C08K 2003/2241: {Titanium dioxide}
- C08L 2201/54: Aqueous solutions or dispersions
- C08L 2312/00: Crosslinking
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)

## Abstract

The present invention relates to a waterborne dispersion comprising (A) amphiphilic block copolymer obtained with a controlled radical polymerization process and comprising at least blocks [A] and [B], whereby block [A] comprises ethylenically unsaturated monomer(s) bearing water-soluble and/or water-dispersible functional groups (monomer(s) (i)), and block [B] comprises ethylenically unsaturated monomer(s) different from monomer(s) (i) (monomer(s) (ii)); and (B) polymer P comprising ethylenically unsaturated monomer(s) different from (i) (monomer(s) (ii)), characterized in that the amount of block copolymer is higher than 1 and lower than 30 wt. %, based on the total weight of monomers used to prepare the block copolymer and polymer P; the acid value of the composition consisting of block copolymer and polymer P is higher than 1 and at most 35 mg KOH per g of the block copolymer-polymer P composition; the block copolymer has a calculated glass transition temperature of higher than 10° C. and lower than 250° C.; and polymer P comprises at least 20 wt. % (relative to the total monomer composition to prepare the polymer P) of a polymer fraction with calculated glass transition temperature higher than 10° C. and lower than 100° C.

## Claims

### Claim 1

A waterborne dispersion comprising
(A) amphiphilic block copolymer obtained with a controlled radical polymerization process and comprising at least blocks [A] and [B], whereby block [A] comprises ethylenically unsaturated monomer(s) bearing water-soluble and/or water-dispersible functional groups (monomer(s) (i)), and block [B] comprises ethylenically unsaturated monomer(s) different from monomer(s) (i) (monomer(s) (ii)); and
(B) polymer P comprising ethylenically unsaturated monomer(s) different from (i) (monomer(s) (ii)), wherein
the amount of block copolymer is higher than 1 and lower than 30 wt. %, based on the total weight of monomers used to prepare the block copolymer and polymer P;
the acid value of the composition consisting of block copolymer and polymer P is higher than 1 and at most 35 mg KOH per g of the block copolymer-polymer P composition;
the block copolymer has a calculated glass transition temperature of higher than 10° C. and lower than 250° C.; and
polymer P comprises at least 20 wt. % (relative to the total monomer composition to prepare the polymer P) of a polymer fraction with a calculated glass transition temperature higher than 10° C. and lower than 100° C.

### Claim 2 (depends on 1)

The waterborne dispersion according to claim 1, wherein
the acid value of the block copolymer-polymer composition is from 1 to 25, more preferably from 1.5 to 20, more preferably from 2 to 18 mg KOH per g of the block copolymer-polymer P composition.

### Claim 3 (depends on 1)

The waterborne dispersion according to claim 1, wherein the amount of the block copolymer is from 2 to 25 wt. %, based on the total weight of monomers used to prepare the block copolymer and polymer P, more preferably from 3 to 20 wt. %, even more preferably from 4 to 15 wt. %.

### Claim 4 (depends on 1)

The waterborne dispersion according to claim 1, wherein the block copolymer has a calculated glass transition temperature from 20 to 200° C., more preferably from 30 to 150° C., more preferably from 40 to 130° C., even more preferably from 50 to 120° C.

### Claim 5 (depends on 1)

The waterborne dispersion according to claim 1, wherein polymer P comprises at least 30 wt. %, preferably at least 50 wt. %, more preferably at least 60 wt. % (relative to the total monomer composition to prepare the polymer P) of a polymer fraction with a calculated glass transition temperature higher than 10° C., preferably higher than 15° C. and with a calculated glass transition temperature lower than 100° C., preferably lower than 85° C., more preferably lower than 65° C. and even more preferably lower than 50° C.

### Claim 6 (depends on 1)

The waterborne dispersion according to claim 1, wherein block [A] has a Hansch parameter of less than 1.5 and block [B] has a Hansch parameter of at least 1.5.

### Claim 7 (depends on 1)

The waterborne dispersion according to claim 1, wherein the amount of ethylenically unsaturated monomer(s) (ii) in block [B] is at least 75 wt. %, more preferably at least 90 wt. %, most preferably at least 95 wt % relative to the total weight amount of monomers used to prepare block [B].

### Claim 8 (depends on 1)

The waterborne dispersion according to claim 1, wherein at least 90 wt. %, preferably at least 95 wt. % of the total amount of monomers (i) present in the block copolymer-polymer composition is present in block [A].

### Claim 9 (depends on 1)

The waterborne dispersion according to claim 1, wherein the water-soluble and/or water-dispersible functional groups are carboxylate groups.

### Claim 10 (depends on 1)

The waterborne dispersion according to claim 1, wherein the block copolymer is a diblock copolymer [A]x[B]y.

### Claim 11 (depends on 1)

The waterborne dispersion according to claim 1, wherein block [A] has an average degree of polymerization x where x is an integer from 3 to 200, preferably lower than 150, more preferably lower than 100 and most preferably lower than 50.

### Claim 12 (depends on 1)

The waterborne dispersion according to claim 1, wherein block [B] has an average degree of polymerization y where y is an integer >10, preferably >50, more preferably >100, and most preferably >150, where y>x.

### Claim 13 (depends on 1)

The waterborne dispersion according to claim 1, wherein the polymer P is obtained by an emulsion polymerization effected in the presence of the block copolymer.

### Claim 14 (depends on 1)

The waterborne dispersion according to claim 1, wherein the ethylenically unsaturated monomer(s) (ii) are selected from the group consisting of C1-12alkyl(meth)acrylate monomers, cyclohexyl (meth)acrylate, styrenic monomers and any mixture thereof, preferably the ethylenically unsaturated monomer(s) (ii) are selected from the group consisting of C1-12 alkyl(meth)acrylate monomers and any mixture thereof.

### Claim 15 (depends on 1)

The waterborne dispersion according to claim 1, wherein the weight average molecular weight of the block copolymer is in the range of from 2,000 to 100,000 g/mol, more preferably from 5,000 to 50,000 g/mol and even more preferably from 7,000 to 35,000 g/mol.

### Claim 16 (depends on 1)

The waterborne dispersion according to claim 1, wherein the weight average molecular weight of the block copolymer-polymer composition is higher than 100,000 g/mol, more preferably in the range of from 100,000 to 500,000 g/mol and even more preferably from 125,000 to 350,000 g/mol.

### Claim 17 (depends on 1)

The waterborne dispersion according to claim 1, wherein the block copolymer is obtained via reversible addition-fragmentation chain transfer (RAFT) polymerization in the presence of a control agent and a source of free radicals, preferably the RAFT polymerization is effected in solution.

### Claim 18 (depends on 1)

The waterborne dispersion according to claim 1, wherein the waterborne dispersion further comprises a crosslinker and is a one-pack system.

### Claim 19 (depends on 1)

A process for preparing a waterborne dispersion according to claim 1, whereby the process comprises at least the following steps:
(a) Preparing an amphiphilic block copolymer comprising at least blocks [A] and [B] in at least the following steps:
a. subjecting at least ethylenically unsaturated monomer(s) (i) bearing water-soluble and/or water-dispersible functional groups to a controlled radical polymerization to obtain block [A],
b. subjecting at least ethylenically unsaturated monomer(s) (ii) that is different from (i) to a controlled radical polymerization to obtain block [B],
wherein block [A] is prepared in the presence of block [B] or wherein block [B] is prepared in the presence of block [A],
(b) optionally converting at least part of the potentially ionic groups to ionic groups present in block [A] before, during or after preparation of block [B];
(c) conducting an emulsion polymerization process in water of at least an ethylenically unsaturated monomer(s) different from (i) (i.e. monomer(s) (ii)) in the presence of the block copolymer obtained in step (a) or step (b) (when present) to obtain the block copolymer-polymer P;
wherein the amount of the block copolymer is higher than 1 wt. % and lower than 30 wt. %, based on the total weight of monomers used to prepare the block copolymer-polymer composition;
the acid value of the block copolymer-polymer composition is higher than 1 and at most 35 mg KOH per g of the block copolymer-polymer P composition;
the block copolymer has a calculated glass transition temperature of higher than 10° C. and lower than 250° C.; and
polymer P comprises at least 20 wt. % (relative to the total monomer composition to prepare the polymer P) of a polymer fraction with a calculated glass transition temperature higher than 10° C. and lower than 100° C.

### Claim 20 (depends on 1)

A coating composition comprising the waterborne dispersion of claim 1.

### Claim 21 (depends on 20)

A coating composition according to claim 20, wherein the coating composition further comprises titanium dioxide in an amount of 15 to 40 volume-%, more preferably from 18 to 30 volume-%, relative to the volume of non-volatile material in the coating composition.

### Claim 22 (depends on 20)

A coating composition according to, claim 20, wherein the coating composition further comprises a crosslinker and is a one-pack system.

### Claim 23 (depends on 20)

A method of coating a substrate comprising the steps of (1) applying the coating composition from claim 20 to a substrate and (2) drying the coating composition.

### Claim 24 (depends on 23)

The method according to claim 23, wherein the substrate comprises a plastic, preferably a polyvinyl material, more preferably polyvinylchloride, more preferably the substrate is made of polyvinyl chloride.

### Claim 25 (depends on 23)

The method according to claim 23, wherein substrate is a profile for an architectural article, preferably the profile is a door frame, a window frame or door panel.

### Claim 26 (depends on 23)

The method according to claim 23, wherein the coating passes the detergent resistance test described in AAMA 614-17, section 7.7.4 and the detergent resistance test described in AAMA 615-17, section 7.7.4.

### Claim 27 (depends on 20)

An article having a coating deposited thereon, wherein the coating is obtained by depositing a coating composition according to claim 20 to a substrate and drying the coating composition.

### Claim 28 (depends on 27)

An article according to claim 27, wherein the article is a profile for an architectural article, preferably the profile is a door frame, a window frame or door panel.

### Claim 29 (depends on 27)

The article according to claim 27, wherein the profile comprises plastic material, preferably a polyvinyl material, more preferably polyvinyl chloride, more preferably the substrate is made of polyvinyl chloride.

### Claim 30 (depends on 27)

The article according to claim 27, wherein the coating passes the detergent resistance test described in AAMA 614-17, section 7.7.4 and the detergent resistance test described in AAMA 615-17, section 7.7.4.