# US 2021/0079159 A1 · Homogeneous poly(alkylene) guanidines and method for the production thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0079159 A1
- Document ID: US20210079159A1
- Status: Published application
- Kind: A1
- Application number: 16/499,292
- Filed: 2018-03-27
- Published: 2021-03-18
- Earliest claimed: 2017-03-28
- Assignees: Thomas FLECHSIG
- Inventors: Thomas FLECHSIG; Frank FLECHSIG
- Web page: https://patentgrep.com/patent/US20210079159A1

## CPC

- C08G 73/02: Polyamines
- C08G 73/0213: {Preparatory process}
- C08G 73/0206: {Polyalkylene(poly)amines}
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS

## Abstract

The invention relates to a method for producing poly(alkylene) guanidines, comprising at least the following steps: a) providing an alkylene diamine of the formula NH2—(CH2)m-NH2 with m=4-12, in particular 6-10, in a reaction vessel and heating the alkylene diamine to a temperature greater than or equal to the melting temperature of the alkylene diamine in question, typically to a temperature in a range of 25° C. to 115° C., preferably 55° C. to 110° C., whereby a melt of the alkylene diamine is produced; b) adding a guanidinium salt, in particular guanidinium HCl, in portions and reacting same with the alkylene diamine until the formation of alkylene(guanidine) monomers is completed; c) reacting the monomers formed in step b), at at least the minimum temperature at which the polymerization to form the desired poly(alkylene) guanidine begins, until the formation of the poly(alkylene) guanidine is completed; wherein steps a) and b) for forming alkylene(guanidine) monomers are carried out at a temperature below the minimum polymerization temperature and the mixture is stirred during all method steps. The invention further relates to the homogeneous poly(alkylene) guanidines obtainable by means of the method described above, said poly(alkylene) guanidines having a content of at least 85 wt %, in particular at least 90% or 97%, of a desired linear poly(alkylene) guanidine having 3-14, preferably 4-10, alkylene monomer units in the molecule as a main product and a content of by-products, in particular branched isomers of said poly(alkylene) guanidine, of at most 15%, 10%, 5% or 3%.

## Claims

### Claim 1

A method for the production of poly(alkylene) guanidines, comprising at least the following steps:
a) providing an alkylene diamine of the formula NH2—(CH2)m—NH2 where m=4-12, in a reaction vessel and heating of the alkylene diamine to a temperature equal to or above a melting temperature of the alkylene diamine, as a result of which a melt of the alkylene diamine is formed;
b) portion-wise adding of a guanidinium salt and reacting with the alkylene diamine until the formation of alkylene(guanidine) monomers is concluded;
c) reacting the monomers formed in step b) at at least a minimum polymerization temperature at which a polymerization to a desired poly(alkylene) guanidine begins until a formation of the poly(alkylene) guanidine is concluded;
wherein steps a) and b) for the formation of alkylene(guanidine) monomers are performed at a temperature below the minimum polymerization temperature and all of the steps are carried out while stirring.

### Claim at position 2

2-13. (canceled)

### Claim 14 (depends on 1)

The method according to claim 1, wherein step b) is performed at a temperature in a range from 20° C. to 115° C. for a period of time of 15 min to 20 h, and/or wherein step c) is performed for a period of time of 30 min to 25 h.

### Claim 15 (depends on 1)

The method according to claim 1, wherein step (b) is conducted while stirring at a temperature in a range from 41° C. to 110° C., for a period of time of 15 min to 25 h, until the formation of alkylene(guanidine) monomers is concluded, and wherein step (c) comprises the following steps:
c1) heating the monomers formed in step b) while stirring to the minimum temperature at which the polymerization to the desired poly(alkylene) guanidine begins;
c2) keeping the reaction mixture at this temperature for a predetermined period of time;
c3) slowly increasing the reaction temperature in steps, and after each increasing step keeping the reaction mixture at the respective increased temperature for a predetermined period of time;
c4) keeping the reaction mixture at a predetermined maximum temperature for a predetermined period of time;
c5) reducing the temperature of the reaction mixture to a predetermined value below the maximum temperature, but above the minimum temperature for polymerization and keeping the reaction mixture at this temperature for a predetermined period of time; and
c6) cooling the reaction mixture to a temperature below the minimum polymerization temperature for the termination of polymerization, as a result of which the desired homogeneous poly(alkyene) guanidine is directly obtained.

### Claim 16 (depends on 1)

The method according to claim 1, wherein the alkylene diamine is tetramethylenediamine, the monomer formation is performed in step b) at a temperature in a range from 25° C. to 110° C., and the minimum polymerization temperature is 120° C.

### Claim 17 (depends on 1)

The method according to claim 1, wherein the alkylene diamine is hexamethylenediamine, octamethylenediamine or decamethylendiamine, the monomer formation is performed in step b) at a temperature in the range from 55° C. to 110° C., and the minimum polymerization temperature is 120° C.

### Claim 18 (depends on 17)

The method according to claim 17, wherein the temperature at which monomer formation in step (b) is performed is 60° C. to 80° C. when the alkylene diamine is hexamethylenediamine, 70° C. to 90° C. when the alkylene diamine is octamethylenediamine, and 75° C. to 90° C. when the alkylene diamine is decamethylenediamine.

### Claim 19 (depends on 1)

The method according to claim 1, wherein the conclusion of the monomer formation in step b) is ascertained by a cessation of foaming as a result of NH3 release and optionally a vacuum is generated in the reaction vessel for a predetermined period of time in order to promote foaming.

### Claim 20 (depends on 19)

The method according to claim 19, wherein a pressure is present in a range from 2 mbar to 4000 mbar, in step b) in the reaction vessel for a period of time in a range from 10 to 240 min.

### Claim 21 (depends on 1)

The method according to claim 1, wherein, in step b), unreacted alkylene diamine is distilled off prior to step c).

### Claim 22 (depends on 1)

The method according to claim 1, wherein a molar ratio of alkylene diamine to guanidinium salt is from 1.2:1 to 1:1.

### Claim 23 (depends on 22)

The method according to claim 22, wherein the molar ratio of alkylene diamine to guanidinium salt is from 1.1:1 to 1:1.

### Claim 24 (depends on 22)

The method according to claim 22, wherein the molar ratio of alkylene diamine to guanidinium salt is about 1:1.

### Claim 25 (depends on 1)

The method according to claim 1, wherein in step a) the temperature to which the alkylene diamine is heated is from 25° C. to 115° C.

### Claim 26 (depends on 1)

A poly(alkylene) guanidine, obtainable with the method according to claim 1, which has a content of at least 85% by weight of a desired linear poly(alkylene) guanidine with 3-14 alkylene monomer units therein as a main product and a content of branched isomer byproducts of the poly(alkylene) guanidine of at most 15%.

### Claim 27 (depends on 26)

The poly(alkylene) guanidine according to claim 26, which contains at least 90% or 97% by weight of the desired linear poly(alkylene) guanidine with 3-14 alkylene monomer units as the main product and contains at most 10% of the branched isomer byproducts of the poly(alkylene) guanidine.

### Claim 28 (depends on 26)

The poly(alkylene) guanidine according to claim 26, wherein the content of the branched isomer byproducts of the poly(alkylene) guanidine is not more than 3%.

### Claim 29 (depends on 26)

The poly(alkylene) guanidine according to claim 26, which has a molecular weight average in a range from 500 to 15,000 Dalton, wherein at most 15% of the polymer molecules have a molecular weight outside the molecular weight average.

### Claim 30 (depends on 29)

The poly(alkylene) guanidine according to claim 29, wherein the molecular weight average is from 500 to 5000 Dalton.