# US 2021/0079149 A1 · Porous membranes including triblock copolymers

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0079149 A1
- Document ID: US20210079149A1
- Status: Published application
- Kind: A1
- Application number: 16/982,258
- Filed: 2019-05-29
- Published: 2021-03-18
- Earliest claimed: 2018-06-01
- Assignees: 3M Innovative Properties Company
- Applicants: 3M Innovative Properties Company
- Inventors: Michelle M. MOK; Lucas D. MCINTOSH; Carl A. LASKOWSKI; Timothy M GILLARD
- Web page: https://patentgrep.com/patent/US20210079149A1

## CPC

- C08F 297/046: {polymerising vinyl aromatic monomers and isoprene, optionally with other conjugated dienes}
- B01D 67/0013: {Casting processes}
- B01D 69/02: characterised by their properties
- B01D 71/24: Rubbers
- B01D 71/261: {Polyethylene}
- B01D 71/28: Polymers of vinyl aromatic compounds
- B01D 71/281: {Polystyrene}
- B01D 71/5211: {Polyethylene glycol or polyethyleneoxide}
- B01D 71/80: Block polymers
- C08F 8/04: Reduction, e.g. hydrogenation
- C08F 8/12: Hydrolysis
- C08F 297/048: {polymerising vinyl aromatic monomers, conjugated dienes and polar monomers}
- C08G 63/08: Lactones or lactides
- C08L 53/025: {modified}
- B01D 2325/022: Asymmetric membranes
- B01D 2325/04: Characteristic thickness
- B01D 2325/20: Specific permeability or cut-off range
- C08F 2800/20: as weight or mass percentages
- C08F 2810/40: taking place solely at one end or both ends of the polymer backbone, i.e. not in the side or lateral chains
- C08F 2810/50: wherein the polymer is a copolymer and the modification is taking place only on one or more of the monomers present in minority
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- B01D: SEPARATION (separating solids from solids by wet methods B03B, B03D; by pneumatic jigs or tables B03B; by other dry methods B07; magnetic or electrostatic separation of solid materials from solid materials or fluids, separation by high-voltage electric fields B03C; centrifuges, vortex apparatus B04; presses per se for squeezing-out liquid from liquid-containing material B30B9/02; treatment of water C02F, e.g. softening by ion-exchange C02F1/42; {arrangements of air intake cleaners in gas turbine plants F02C7/05} ; arrangements or mounting of filters in air-conditioning, air-humidification or ventilation F24F13/28)
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)

## Abstract

A porous membrane includes a triblock copolymer of the formula ABC. B is a hydrogenated vinyl aromatic block present in a range from 30 to 90 weight percent, based on the total weight of the copolymer and has a Tg of ≥110° C. C is a rubbery block present in a range from 10 to 70 weight percent, based on the total weight of the copolymer and has a Tg≤25° C. A is substantially incompatible with both the B and C blocks and is derived from ring-opening polymerization. B+C is present in a range from 70 to 95 weight percent, based on the total weight of the copolymer.

## Claims

### Claim 1

A porous membrane comprising a triblock copolymer of the formula ABC wherein:
B is a hydrogenated vinyl aromatic block present in a range from 30 to 90 weight percent, based on the total weight of the copolymer and having a Tg of ≥110° C.;
C is a rubbery block present in a range from 10 to 70 weight percent, based on the total weight of the copolymer and having a Tg≤25° C.; and
A is substantially incompatible with both the B and C blocks and is derived from ring-opening polymerization,
wherein B+C is present in a range from 70 to 95 weight percent, based on the total weight of the copolymer.

### Claim 2 (depends on 1)

The porous membrane of claim 1, wherein the porous membrane is an integral asymmetric membrane.

### Claim 3 (depends on 1)

The porous membrane of claim 1, wherein the B block has a residual unsaturation of not greater than 55 mol %.

### Claim 4 (depends on 1)

The porous membrane of claim 1, wherein the B block has a residual unsaturation of not greater than 10 mol %

### Claim 5 (depends on 1)

The porous membrane of claim 1, wherein A is present in a range from 5 to 30 weight percent, based on the total weight of the copolymer.

### Claim 6 (depends on 1)

The porous membrane of claim 1, wherein the B block is present in a range from 60 to 90 weight percent, based on the total weight of the copolymer.

### Claim 7 (depends on 1)

The porous membrane of claim 1, wherein the C block is present in a range from 10 to 40 weight percent, based on the total weight of the copolymer.

### Claim 8 (depends on 1)

The porous membrane of claim 1,
wherein the B block is selected from at least partially hydrogenated styrene, α-methyl styrene, 4-methyl styrene, 3-methyl styrene, 4-ethyl styrene, 3,4-dimethyl styrene, 2,4,6-trimethylstyrene, 3-tert-butyl-styrene, 4-tert-butylstyrene, 4-methoxystyrene, 4-trimethylsilylstyrene, 2,6-dichlorostyrene, vinyl naphthalene, 4-chlorostyrene, 3-chlorostyrene, 4-fluorostyrene, 4-bromostyrene, vinyl toluene, ethylstyrene, diethyl styrene, di-n-butylstyrene, isopropylstyrene, other alkylated-styrenes, styrene analogs, vinyl naphthalene, and vinyl anthracene;
wherein the C block is selected from hydrogenated butadiene, isoprene, ethylbutadiene, phenylbutadiene, piperylene, pentadiene, hexadiene, ethylhexadiene, and dimethylbutadiene 1,3-cyclodiene monomers;
wherein the A block are polyethers selected from poly(ethylene oxide), poly(propylene oxide), poly(ethoxyethyl-glycidylether), poly(vinylglycidylether), poly(methylglycidylether), poly(ethylglycidylether), poly(propylglycidylether), poly(butylglycidylether), glycidol, and copolymers thereof derived from ring-opening polymerization of cyclic ethers; or
any combination thereof.

### Claim 9 (depends on 1)

The porous membrane of claim 1, wherein the Mn is 60-500 kDa.

### Claim 10 (depends on 1)

The porous membrane of claim 1, wherein the porous membrane has a dry thickness in a range from 0.5 to 500 micrometers.

### Claim 11 (depends on 1)

A shaped article comprising the porous membrane of claim 1 that is a free-standing flat sheet, a supported flat sheet, or a hollow fiber.

### Claim 12 (depends on 1)

A filter comprising the porous membrane of claim 1.

### Claim 13 (depends on 1)

A kit comprising:
a filter comprising the porous membrane of claim 1; and
a package for containing the filter.

### Claim 14 (depends on 13)

The kit of claim 13, wherein the package comprises information related to the filter or a use thereof.

### Claim 15 (depends on 13)

The kit of claim 13, further comprising a filter support.

### Claim 16 (depends on 13)

The kit of claim 13, further comprising a receptacle.

### Claim 17

A method of preparing a porous membrane, the method comprising:
dissolving a triblock copolymer of the formula ABC in a solvent system to form a triblock copolymer solution wherein:
B is a hydrogenated vinyl aromatic block present in a range from 30 to 90 weight percent, based on the total weight of the copolymer and having a Tg of ≥110° C.;
C is a rubbery block present in a range from 10 to 70 weight percent, based on the total weight of the copolymer and having a Tg≤25° C.; and
A is substantially incompatible with both the B and C blocks and is derived from ring-opening polymerization,
wherein B+C is present in a range from 70 to 95 weight percent, based on the total weight of the copolymer;
forming a precursor article from the triblock copolymer solution;
removing at least a portion of the solvent system from the precursor article to form a partially dried precursor article; and
contacting the partially dried precursor article with a nonsolvent, thereby forming the porous membrane.

### Claim 18 (depends on 17)

The method of claim 17, wherein the triblock copolymer solution has triblock copolymer in a range from 9 to 15 weight percent, based on the total weight of the triblock copolymer solution.

### Claim 19 (depends on 17)

The method of claim 17, wherein the film is formed using a notch bar coater, knife coater, or a spin coater.

### Claim 20 (depends on 17)

The method of claim 17, wherein the triblock copolymer solution is cast onto a substrate using a notch bar coater having a coating gap in a range from 1 to 15 mils (25 to 375 micrometers).