# US 2021/0078869 A1 · Method for preparing calcium oxide using a multistage suspension preheater kiln

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0078869 A1
- Document ID: US20210078869A1
- Status: Published application
- Kind: A1
- Application number: 16/993,279
- Filed: 2020-08-14
- Published: 2021-03-18
- Earliest claimed: 2019-09-12
- Assignees: Guangxi Siwei Materials Technology Co., Ltd.
- Applicants: Guangxi Siwei Materials Technology Co., Ltd.
- Inventors: Yan Zhuang; Licheng Zhuang; Qiancheng Zhuang
- Web page: https://patentgrep.com/patent/US20210078869A1

## CPC

- C01F 11/06: of carbonates
- B01J 3/006: {Processes utilising sub-atmospheric pressure; Apparatus therefor}
- B01J 6/001: {Calcining}
- B01J 6/002: {using rotating drums}
- B01J 6/004: {using hot gas streams in which the material is moved}
- B01J 8/14: moving in free vortex flow apparatus
- B01J 8/386: {internally, i.e. the particles rotate within the vessel}
- F27B 15/003: {Cyclones or chain of cyclones}
- F27B 15/08: Arrangements of devices for charging
- F27B 15/09: Arrangements of devices for discharging
- F27B 15/10: Arrangements of air or gas supply devices
- F27D 13/00: Apparatus for preheating charges; Arrangements for preheating charges
- F27D 15/02: Cooling
- C01P 2004/60: Particles characterised by their size
- C01P 2006/80: Compositional purity
- F27D 2013/007: {using a rotary furnace}
- Y02P 20/10: Process efficiency
- C01F: COMPOUNDS OF THE METALS BERYLLIUM, MAGNESIUM, ALUMINIUM, CALCIUM, STRONTIUM, BARIUM, RADIUM, THORIUM, OR OF THE RARE-EARTH METALS (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts of peroxyacids C01B15/00; sulfides or polysulfides of magnesium, calcium, strontium, or barium C01B17/42; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds other than ammonia or cyanogen containing nitrogen and non-metals and optionally metals C01B21/082; amides or imides of silicon C01B21/087}; metal {imides or} amides C01B21/092, {C01B21/0923}; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanic acid C01C3/14; salts of cyanamide C01C3/16; thiocyanates C01C3/20; {double sulfates of magnesium with sodium or potassium C01D5/12; with other alkali metals C01D15/00, C01D17/00})
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- F27B: FURNACES, KILNS, OVENS OR RETORTS IN GENERAL; OPEN SINTERING OR LIKE APPARATUS
- F27D: DETAILS OR ACCESSORIES OF FURNACES, KILNS, OVENS OR RETORTS, IN SO FAR AS THEY ARE OF KINDS OCCURRING IN MORE THAN ONE KIND OF FURNACE
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

The disclosure discloses a method for preparing calcium oxide using multistage suspension preheater kiln. The steps of the method are: (1) the limestone powder is fed to the multistage suspension preheater kiln for preheating to 800° C. to 900° C.; (2) A preheated material is fed to a decomposition furnace, and calcined at 900° C. to 1100° C. for 25 s to 35 s; (3) A calcined material is fed to a rotary kiln, and calcined at 1100° C. to 1300° C. for 25 to 35 minutes, and finally cooled to obtain calcium oxide.

## Claims

### Claim 1

A method for preparing calcium oxide using a multistage suspension preheater kiln, wherein the method comprises steps of:
(1) feeding limestone powder to the multistage suspension preheater kiln for preheating to 800° C. to 900° C.;
(2) feeding a preheated material to a decomposition furnace and calcining at 900° C. to 1100° C. for 25 s to 35 s;
(3) feeding a calcined material to a rotary kiln and calcining at 1100° C. to 1300° C. for 25 min to 35 min; cooling to obtain calcium oxide.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the multistage suspension preheater kiln comprises six-stage hot flue gas cyclones that are sequentially connected to a hot gas duct; the hot gas duct conveys hot flue gas upward; a first-stage hot flue gas cyclone on the hot gas duct is the topmost hot flue gas cyclone, and a material outlet of a fifth-stage hot flue gas cyclone connects to an inlet of a decomposition furnace.

### Claim 3 (depends on 2)

The method according to claim 2, wherein a gas temperature in the first-stage hot flue gas cyclone is lower than that in a second-stage hot flue gas cyclone;
the second-stage hot flue gas cyclone has a gas temperature of 400° C. to 500° C. and a negative pressure of −4 kPa to −5 kPa;
a third-stage hot flue gas cyclone has a gas temperature of 500° C. to 600° C. and a negative pressure of −3.5 kPa to −4.5 kPa;
a fourth-stage hot flue gas cyclone has a gas temperature of 600° C. to 700° C. and a negative pressure of −2.5 kPa to −3.5 kPa;
the fifth-stage hot flue gas cyclone has a gas temperature of 800° C. to 900° C. and a negative pressure of −1.5 kPa to −2.5 kPa.

### Claim 4 (depends on 1)

The method according to claim 1, wherein a negative pressure in the decomposition furnace is −0.9 kPa to −1.5 kPa.

### Claim 5 (depends on 2)

The method according to claim 2, wherein an end of the hot gas duct is provided with an exhaust device; a material outlet of the first-stage hot flue gas cyclone connects to a hot flue gas outlet duct of a third-stage hot flue gas cyclone, a material outlet of the third-stage hot flue gas cyclone connects to a hot flue gas outlet duct of the fifth-stage hot flue gas cyclone; a material outlet of a second-stage hot flue gas cyclone connects to a hot flue gas outlet duct of a fourth-stage hot flue gas cyclone, a material outlet of the fourth-stage hot flue gas cyclone connects to a hot flue gas outlet duct of a sixth-stage hot flue gas cyclone; a material at an outlet of the decomposition furnace connects to a feed pipe of the sixth-stage hot flue gas cyclone through a rising gas flow; a material outlet of the sixth-stage hot flue gas cyclone connects to a flue chamber of the rotary kiln; a powdered limestone raw material is fed through a hot gas duct between the first-stage hot flue gas cyclone and the second-stage hot flue gas cyclone.

### Claim 6 (depends on 1)

The method according to claim 1, wherein a particle size of the limestone powder is less than 70 mesh.

### Claim 7 (depends on 2)

The method according to claim 2, wherein the hot flue gas is a flue gas that is generated by the decomposition furnace and the rotary kiln.

### Claim 8 (depends on 1)

The method according to claim 1, wherein fuel used for calcination in the rotary kiln is petroleum coke.

### Claim 9 (depends on 1)

The method according to claim 1, wherein a wind pressure in the rotary kiln is 12 kPa and a rotating speed of the rotary kiln is 3.5 rpm.

### Claim 10 (depends on 5)

The method according to claim 5, wherein a gas temperature in the sixth-stage hot flue gas cyclone is 950° C. to 1130° C., a negative pressure in the sixth-stage hot flue gas cyclone is −1.0 kPa to −2.0 kPa.