# US 2021/0078103 A1 · Method for Laser Beam Welding of One or More Steel Sheets Made of Press-Hardenable Manganese-Boron Steel

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0078103 A1
- Document ID: US20210078103A1
- Status: Published application
- Kind: A1
- Application number: 16/642,267
- Filed: 2018-08-09
- Published: 2021-03-18
- Earliest claimed: 2017-08-31
- Assignees: Baosteel Tailored Blanks GmbH
- Applicants: Baosteel Tailored Blanks GmbH
- Inventors: Jana von der Heydt; Christian Both; Michael Kessler
- Web page: https://patentgrep.com/patent/US20210078103A1

## CPC

- B23K 26/211: with interposition of special material to facilitate connection of the parts
- B23K 26/032: {using optical means}
- B23K 26/082: Scanning systems, i.e. devices involving movement of the laser beam relative to the laser head
- B23K 26/24: Seam welding
- B23K 26/322: involving coated metal parts (using absorbing layers on the workpiece B23K26/18)
- B23K 2101/18: Sheet panels
- B23K 2101/34: Coated articles {; Surface treated articles}
- B23K 2103/04: Steel {or steel} alloys
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM

## Abstract

A method for laser beam welding of one or more steel sheets made of press-hardenable manganese-boron steel is disclosed. At least one of the steel sheets has a coating of aluminium. The laser beam welding takes place by feeding an additional wire into a melt bath generated by of a laser beam. The additional wire contains at least one austenite-stabilising alloy element. The weld seam after hot forming (press hardening) has a strength that is comparable to the base material. The laser beam is put into oscillation such that it oscillates transverse to the welding direction, wherein the oscillation frequency of the laser beam is at least 200 Hz, preferably at least 500 Hz. The method dispenses with removing the aluminum coating at the edge of the sheet-metal edges to be welded.

## Claims

### Claim 1

A method for laser beam welding of one or more steel sheets made of press-hardenable manganese-boron steel, wherein at least one of the steel sheets has a coating made of aluminium, comprising:
feeding an additional wire into a melt bath generated by a laser beam,
wherein the additional wire contains at least one austenite-stabilising alloy element,
wherein the laser beam is set into oscillation such that the laser beam oscillates transverse to a welding direction,
and wherein oscillation frequency of the laser beam is at least 200 Hz.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the one or more steel sheets are joined during laser beam welding in a butt joint or an overlap joint with a gap of less than 0.8 mm.

### Claim 3 (depends on 1)

The method according to claim 1, wherein an amplitude of the oscillation of the laser beam is less than 2 mm.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the laser beam welding is carried out at an advance speed of more than 4 m/min.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the oscillation of the laser beam is carried out with a linear, circular, or polygonal oscillation profile.

### Claim 6 (depends on 1)

The method according to claim 1, wherein a geometry of a weld seam is detected, and wherein at least one of the oscillation frequency and an amplitude of the oscillating laser beam is varied as a function of the detected geometry of the weld seam.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the additional wire has a carbon mass proportion of at least 0.1% by weight.

### Claim 8 (depends on 1)

The method according to claim 1, wherein the additional wire has the following composition:
0.1 to 4.0% by weight C,
0.5 to 2.0% by weight Si,
1.0 to 2.5% by weight Mn,
0.5 to 2.0% by weight Cr+Mo,
1.0 to 4.0% by weight Ni, and
remainder iron and unavoidable impurities.

### Claim 9 (depends on 1)

The method according to claim 1, wherein the additional wire is heated prior to the feeding into the melt bath at least in a longitudinal section to a temperature of at least 50° C.

### Claim 10 (depends on 1)

The method according to claim 1, wherein inert gas is applied to the melt bath during the laser beam welding.

### Claim 11 (depends on 1)

The method according to claim 1, wherein the one or more steel sheets have a sheet thickness in the range of 0.5 to 4 mm.

### Claim 12 (depends on 1)

The method according to claim 1, wherein the one or more steel sheets have at least one of a different sheet thickness and a different tensile strength.

### Claim 13 (depends on 1)

The method according to claim 1, wherein the oscillation frequency is at least 500 Hz.

### Claim 14 (depends on 2)

The method according to claim 2, wherein the gap is less than 0.6 mm.

### Claim 15 (depends on 2)

The method according to claim 2, wherein the gap is less than 0.4 mm.

### Claim 16 (depends on 3)

The method according to claim 3, wherein the amplitude of the oscillation of the laser beam is less than 1 mm.

### Claim 17 (depends on 4)

The method according to claim 4, wherein the laser beam welding is carried out at an advance speed in the range of 5 to 8 m/min.

### Claim 18 (depends on 7)

The method according to claim 7, wherein the additional wire has a carbon mass proportion of around at least 0.3% by weight.

### Claim 19 (depends on 9)

The method according to claim 9, wherein the additional wire is heated prior to the feeding into the melt bath at least in a longitudinal section to a temperature of at least 90° C.

### Claim 20 (depends on 11)

The method according to claim 11, wherein the at least one or more steel sheets have a sheet thickness in the range of 0.8 to 2.5 mm.