# US 2021/0078081 A1 · Silver powder and method for producing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0078081 A1
- Document ID: US20210078081A1
- Status: Published application
- Kind: A1
- Application number: 17/086,552
- Filed: 2020-11-02
- Published: 2021-03-18
- Earliest claimed: 2015-10-30
- Assignees: Dowa Electronics Materials Co., Ltd.
- Applicants: Dowa Electronics Materials Co., Ltd.
- Inventors: Atsushi Ebara; Kenichi Inoue; Yoshiyuki Michiaki; Takahiro Yamada; Masahiro Yoshida
- Web page: https://patentgrep.com/patent/US20210078081A1

## CPC

- B22F 9/082: {atomising using a fluid (using centrifugal force B22F9/10)}
- B22F 1/00: Metallic powder; Treatment of metallic powder, e.g. to facilitate working or to improve properties
- B22F 1/05: Metallic powder characterised by the size or surface area of the particles
- B22F 1/06: Metallic powder characterised by the shape of the particles (nanosized particles B22F1/054)
- C09D 5/24: Electrically-conducting paints {(conductive materials H01B1/00)}
- C09D 7/69: {Particle size larger than 1000 nm}
- C22C 5/06: Alloys based on silver
- H01B 1/02: mainly consisting of metals or alloys
- H01B 1/22: the conductive material comprising metals or alloys
- B22F 2009/0828: {with water}
- B22F 2301/255: Silver or gold
- B22F 2304/10: Micron size particles, i.e. above 1 micrometer up to 500 micrometer
- C08K 2003/0806: {Silver}
- C08K 2201/001: Conductive additives
- C08K 2201/005: Additives being defined by their particle size in general
- C08K 2201/006: Additives being defined by their surface area
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- H01B: CABLES; CONDUCTORS; INSULATORS; SELECTION OF MATERIALS FOR THEIR CONDUCTIVE, INSULATING OR DIELECTRIC PROPERTIES (selection for magnetic properties H01F1/00; waveguides H01P {; printed circuits H05K})
- C08K: Use of inorganic or non-macromolecular organic substances as compounding ingredients (paints, inks, varnishes, dyes, polishes, adhesives C09)

## Abstract

There is provided a silver powder which has a small average particle diameter and a small thermal shrinkage percentage, and a method for producing the same. While a molten metal of silver heated to a temperature (1292 to 1692° C.), which is higher than the melting point (962° C.) of silver by 330 to 730° C., is allowed to drop, a high-pressure water is sprayed onto the molten metal of silver (preferably at a water pressure of 90 to 160 MPa) to rapidly cool and solidify the molten metal of silver to powderize silver to produce a silver powder which has an average particle diameter of 1 to 6 μm and a shrinkage percentage of not greater than 8% (preferably not greater than 7%) at 500° C., the product of the average particle diameter by the shrinkage percentage at 500° C. being 1 to 11 μm·% (preferably 1.5 to 10.5 μm·%).

## Claims

### Claim at position 1

1-2. (canceled)

### Claim 3

A silver powder which has an average particle diameter of 1 to 6 μm and a shrinkage percentage of not higher than 8% at 500 and wherein a product of the average particle diameter and the shrinkage percentage at 500° C. is 1 to 11 μm·%.

### Claim 4 (depends on 3)

A silver powder as set forth in claim 3, wherein a value obtained by dividing a product of a BET specific surface area (m2/g) and a tap density (g/m3) by a crystallite diameter (m) is 1×1013 to 6×1013 (m−2).

### Claim 5 (depends on 3)

A silver powder as set forth in claim 3, which has a carbon content of not higher than 0.1% by weight.

### Claim 6 (depends on 3)

A conductive paste which contains a solvent, a resin and a conductive powder which is a silver powder as set forth in claim 3.