# US 2021/0078079 A1 · Method for producing an abrasion-resistant coating on surface of 3d printed titanium alloy components

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0078079 A1
- Document ID: US20210078079A1
- Status: Published application
- Kind: A1
- Application number: 17/001,618
- Filed: 2020-08-24
- Published: 2021-03-18
- Earliest claimed: 2019-09-16
- Assignees: Jiangnan University
- Applicants: Jiangnan University
- Inventors: Meiping WU; Xiaojin MIAO; Peipei LU; Xiu YE; Hang WANG; Xin LIU
- Web page: https://patentgrep.com/patent/US20210078079A1

## CPC

- B22F 3/24: After-treatment of workpieces or articles {(B22F3/1146 takes precedence)}
- B22F 9/082: {atomising using a fluid (using centrifugal force B22F9/10)}
- B22F 10/00: Additive manufacturing of workpieces or articles from metallic powder (apparatus or devices therefor B22F12/00)
- B22F 10/28: Powder bed fusion, e.g. selective laser melting [SLM] or electron beam melting [EBM]
- B22F 10/68: Cleaning or washing
- B33Y 10/00: Processes of additive manufacturing
- B33Y 40/20: Post-treatment, e.g. curing, coating or polishing
- B33Y 70/00: Materials specially adapted for additive manufacturing
- B33Y 80/00: Products made by additive manufacturing
- C23C 24/06: Compressing powdered coating material, e.g. by milling
- B22F 2003/242: {Coating}
- B22F 2003/247: {Removing material: carving, cleaning, grinding, hobbing, honing, lapping, polishing, milling, shaving, skiving, turning the surface}
- B22F 2003/248: {Thermal after-treatment}
- B22F 2009/0836: {with electric or magnetic field or induction}
- B22F 2301/205: Titanium, zirconium or hafnium
- B22F 2303/30: Coating alloy
- B22F 2304/10: Micron size particles, i.e. above 1 micrometer up to 500 micrometer
- B22F 2998/10: Processes characterised by the sequence of their steps
- B22F 2999/00: Aspects linked to processes or compositions used in powder metallurgy
- Y02P 10/25: Process efficiency
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- B33Y: ADDITIVE MANUFACTURING, i.e. MANUFACTURING OF THREE-DIMENSIONAL [3D] OBJECTS BY ADDITIVE DEPOSITION, ADDITIVE AGGLOMERATION OR ADDITIVE LAYERING, e.g. BY 3D PRINTING, STEREOLITHOGRAPHY OR SELECTIVE LASER SINTERING
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

The present invention relates to a method for producing an abrasion-resistant coating on surface of a 3D printed titanium alloy component, which belongs to the field of surface modification. The method comprises using spherical TC4 titanium alloy powder as a base material and adopting selective laser melting (SLM) technology to manufacture a 3D printed titanium alloy component in a layer-by-layer stacking manner, using graphene oxide to perform friction-induction treatment, and making the graphene oxide infiltrate into the surface of the TC4 titanium alloy component to obtain a graphene oxide surface coating. The goal of improving the friction and wear performance of the TC4 titanium alloy printed components is achieved. The preparation method is simple, and the steps are easy to operate. Introducing the graphene oxide is beneficial to reduce the generation of wear debris during the friction and wear processes and improve tribological characteristics of the base material.

## Claims

### Claim 1

A method for producing an abrasion-resistant coating on surface of a three-dimensional (3D) printed titanium alloy component, comprising:
using spherical TC4 titanium alloy powder with particle size of 4-70 μm as a printing material, and putting the spherical TC4 titanium alloy powder in a vacuum drying oven for drying treatment to obtain sufficiently dried TC4 titanium alloy powder;
adding the dried TC4 titanium alloy powder into a powder supplying bin of a selective laser melting (SLM) 3D printer, setting reasonable laser scanning parameters, laser-scanning and stacking the TC4 titanium alloy powder layer by layer until a component is formed, and then peeling off the formed component and polishing and cleaning the formed component to obtain a 3D printed titanium alloy component;
drying graphene oxide powder and adding the dried graphene oxide powder on top of a friction-induction tool and applying a pre-compression pressure of 5-10 N/m2 for 3-5 minutes on the graphene oxide powder to make it tightly and evenly spread on top of the friction-induction tool;
fixing the 3D printed titanium alloy component on a friction and wear testing machine and pressing the friction-induction tool tightly on the surface of the 3D printed titanium alloy component under a working pressure, and increasing the working pressure to make the graphene oxide powder react with the surface of the 3D printed titanium alloy component, and then performing reciprocating friction-induction operations along a planned path to infiltrate the graphene oxide powder into the 3D printed titanium alloy component to form an abrasion-resistant coating; and
washing the component with deionized water and blow-drying the component with a blow-dryer.

### Claim 2 (depends on 1)

The method for producing an abrasion-resistant coating on surface of a 3D printed titanium alloy component according to claim 1, wherein the temperature of the vacuum drying oven is 100-120° C., and the drying time is 2.5-3.5 hours.

### Claim 3 (depends on 1)

The method for producing an abrasion-resistant coating on surface of a 3D printed titanium alloy component according to claim 1, wherein the laser scanning parameters comprise 180-220 W laser power, 1200-1400 mm/s scan speed, 110-150 μm scan pitch and 28-32 μm scan thickness.

### Claim 4 (depends on 1)

The method for producing an abrasion-resistant coating on surface of a 3D printed titanium alloy component according to claim 1, wherein argon gas is used for protection during the forming of the 3D printed titanium alloy component, and wire cutting process is adopted to peel off the formed component.

### Claim 5 (depends on 1)

The method for producing an abrasion-resistant coating on surface of a 3D printed titanium alloy component according to claim 1, wherein the formed component is polished with an alumina polishing solution, washed with an ethanol solution and dried.

### Claim 6 (depends on 1)

The method for producing an abrasion-resistant coating on surface of a 3D printed titanium alloy component according to claim 1, wherein the 3D printed titanium alloy component is ground with 1000 grit, 1200 grit, 1500 grit and 2000 grit sandpapers in sequence.

### Claim 7 (depends on 1)

The method for producing an abrasion-resistant coating on surface of a 3D printed titanium alloy component according to claim 1, wherein the pre-compression pressure is 5-10 N/m2, and the working pressure is 12-15 N/m2.

### Claim 8 (depends on 1)