# US 2021/0078039 A1 · Method for coating the visible surfaces of motor vehicle wheel rims

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0078039 A1
- Document ID: US20210078039A1
- Status: Published application
- Kind: A1
- Application number: 16/772,355
- Filed: 2018-12-11
- Published: 2021-03-18
- Earliest claimed: 2017-12-11
- Inventors: Beata KUCHARSKA
- Web page: https://patentgrep.com/patent/US20210078039A1

## CPC

- B05D 5/067: {Metallic effect}
- B05D 1/02: performed by spraying
- B05D 3/0254: {After-treatment}
- B05D 5/068: {achieved by multilayers (B05D5/066 takes precedence)}
- B05D 7/576: {each layer being cured, at least partially, separately}
- B05D 7/574: {at least some layers being let to dry at least partially before applying the next layer (B05D7/577 takes precedence)}
- B05D 2202/00: Metallic substrate
- B05D 2202/10: based on Fe
- B05D 2202/25: based on Al
- B05D 2601/02: used for pigmentation effect, e.g. metallic effect
- B05D 2601/08: Aluminium flakes or platelets
- B05D 2601/10: Other metals
- B60B 2900/572: Visual appearance
- B05D: PROCESSES FOR APPLYING FLUENT MATERIALS TO SURFACES, IN GENERAL (conveying articles or workpieces through baths of liquid B65G, e.g. B65G49/02)
- B60B: VEHICLE WHEELS (making wheels or wheel parts by rolling B21H1/00, by forging, hammering or pressing B21K1/28); CASTORS; AXLES FOR WHEELS OR CASTORS; INCREASING WHEEL ADHESION

## Abstract

In a method for coating motor vehicle wheel rims, a polymer priming layer, a polymer intermediate layer, a decorative layer of a heat-cured polymer layer with embedded flake-like metal pigments covering the visible surface of the decorative layer, and a polymer cover layer are consecutively applied to the wheel rim metal surface. The coated wheel rims achieve a polished metal appearance without substantial extra costs by producing the polymer intermediate layer with a high-gloss surface and applying the decorative layer to the high-gloss surface of the polymer intermediate layer in the wet spraying method with a layer thickness of max. 2 μm, where it is dried at ambient temperature and, before applying the polymer cover layer, it is fixed to the polymer intermediate layer via a thermal post-treatment so that it adheres to the surface thereof with a cross-cut pull-off strength of Gt=0 to Gt=2.

## Claims

### Claim 1

A method for coating the visible surfaces of motor vehicle wheel rims made of aluminum or steel, in which
a polymer primer layer (A) is first applied to the mechanically processed metal surface of the wheel rim, which layer evens out the irregularities of the mechanical processing,
then a polymer intermediate layer (B) is applied to the surface of the polymer primer layer (A),
then a decorative layer (C) is applied to the surface of the polymer intermediate layer (B), which decorative layer comprises a thermally cured polymer layer with embedded platelet-shaped metal pigments, which cover the visible surface of the decorative layer (C),
and finally the surface of the decorative layer (C) is covered by a polymer topcoat (D),
wherein
the polymer intermediate layer (B) is produced with a high-gloss surface with a gloss grade according to DIN67530/ISO2813 of more than 95,
the decorative layer (C) is applied by wet spraying with a layer thickness of a maximum of 2 μm to the high-gloss surface of the polymer intermediate layer (B) and is dried there at ambient temperature, and
prior to the application of the polymer topcoat (D), the decorative layer (C) is fixed on the surface of the polymer intermediate layer (B) by a thermal aftertreatment such that it adheres to the surface with a cross-cut tear strength according to DIN EN ISO 2409 of Gt=0 to Gt=2.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the thermal post-treatment of the decorative layer (C) is carried out at a temperature of more than 140° C.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the thermal post-treatment of the decorative layer (C) is carried out at a temperature of 180° C. to 200° C.

### Claim 4 (depends on 1)

The method according to claim 1, wherein color pigments are additionally added to the decorative layer (C).

### Claim 5 (depends on 1)

The method according to claim 1, wherein the combined surfaces of the platelet-shaped metal pigments contained in the decorative layer (C) and facing the observer are greater by at least the factor 3 than the area of the decorative layer (C).