# US 2021/0077997 A1 · Method of Manufacture of Microfluidic or Microtiter Device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0077997 A1
- Document ID: US20210077997A1
- Status: Published application
- Kind: A1
- Application number: 17/086,530
- Filed: 2020-11-02
- Published: 2021-03-18
- Earliest claimed: 2015-02-25
- Assignees: Stratec Consumables GmbH
- Applicants: STRATEC Consumables GmbH
- Inventors: Maximilian Pitzek; Andrej Peterca; Nora Doppelmayer
- Web page: https://patentgrep.com/patent/US20210077997A1

## CPC

- B01L 3/5085: {for multiple samples, e.g. microtitration plates}
- B01L 3/502707: {characterised by the manufacture of the container or its components}
- B29C 45/561: {Injection-compression moulding}
- B01L 2200/12: Specific details about manufacturing devices
- B01L 2300/0829: Multi-well plates; Microtitration plates
- B29C 2045/0094: {injection moulding of small-sized articles, e.g. microarticles, ultra thin articles}
- B29C 2045/564: {Compression drive means acting independently from the mould closing and clamping means}
- B01L: CHEMICAL OR PHYSICAL LABORATORY APPARATUS FOR GENERAL USE
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)

## Abstract

A method of manufacturing a microfluidic or microtiter device, the method comprises fabricating, by a single compression injection molding operation, a microfluidic or microtiter device having one or more indentations, in which a base thickness of the one or more indentations is less than 400 μm. In embodiments, the fabricating step comprises: forming a mold cavity; filling the mold cavity with molten material; closing the mold cavity; and driving one or more molding formations complementary to the one or more indentations into the mold cavity.

## Claims

### Claim 1

A method of manufacturing a monolithic microfluidic or microtiter device, the method comprising:
providing a mold cavity with mold formations, wherein the mold cavity is complimentary to the desired configuration of the molded monolithic microfluidic or microtiter device;
heating a polymer material to a molten state;
compression injecting the molten polymer material into the mold cavity; and
setting the polymer material to become transparent; and
obtaining the entire molded monolithic microfluidic or microtiter device having
a ridge around the periphery of the underside of the plate and one or more first wells with a base, wherein a base thickness of the one or more wells is less than 400 μm, a variation of the base thickness is less than 10% and a base has a low background fluorescence; and
second wells at the periphery surrounding the first wells providing a frame around an array of first wells.

### Claim 2 (depends on 1)

The method according to claim 1, further comprising the step of cooling the mold cavity, the cooling comprising cooling different parts of the mold cavity to different temperatures.

### Claim 3 (depends on 1)

The method according to claim 1, in which the microfluidic or microtiter device is a microtiter plate having an array of wells.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the one or more molding formations are mold pins, one pin for each well.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the step of providing the mold cavity comprises driving a plurality of mold parts together.

### Claim 6 (depends on 4)

The method according to claim 4, wherein, for at least a portion of a length of the mold pins which forms a corresponding well, the mold pins are tapered so as to be narrower at a distal end.

### Claim 7 (depends on 1)

The method according to claim 1, wherein providing the mold cavity comprises driving the molding formations into the mold cavity from one side of the mold cavity towards an opposite side of the mold cavity so that a distal end of each molding formation reaches a position within 400 μm of a surface of the opposite side of the cavity.

### Claim 8 (depends on 7)

The method according to claim 7, wherein a distal end of each molding formation reaches a position within 300 μm of a surface of the opposite side of the cavity.

### Claim 9 (depends on 7)

The method according to claim 7, wherein a distal end of each molding formation reaches a position within 250 μm of a surface of the opposite side of the cavity.

### Claim 10 (depends on 1)

The method according to claim 1, further comprising the step of cooling the mold cavity, the cooling comprising cooling different parts of the mold cavity to different temperatures.

### Claim 11 (depends on 1)

The method according to claim 1, further comprising the step of directing a cooling gas around a periphery of at least some of the molding formations.

### Claim 12 (depends on 1)

The method according to claim 1, in which the microfluidic or microtiter device is a microtiter plate having an array of wells.

### Claim 13 (depends on 1)

The method according to claim 1, in which the polymer is selected from a list consisting of:
Cyclo Olephine Polymer grades with glass transition temperature (Tg) between 100 and 160° C.;
Cyclo Olephine Copolymer grades with glass transition temperature (Tg) between 100 and 160° C.;
Polypropylene;
Polystyrene;
Polycarbonate;
Polymethyl methacrylate;
PVC (Polyvinyl chloride);
PPE (Polyphenyl ether);
SAN (Styrene-acrylonitrile),
PET (Polyethylene terephthalate);
PE (Polyethylene); and
copolymers and blends of any permutation of these polymers.