# US 2021/0077985 A1 · Manufacturing hyrdocracking catalyst

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0077985 A1
- Document ID: US20210077985A1
- Status: Published application
- Kind: A1
- Application number: 16/569,550
- Filed: 2019-09-12
- Published: 2021-03-18
- Earliest claimed: 2019-09-12
- Assignees: Saudi Arabian Oil Company; JGC Catalysts and Chemicals Ltd.
- Applicants: Saudi Arabian Oil Company; JGC Catalysts and Chemicals Ltd.
- Inventors: Robert Peter Hodgkins; Omer Refa Koseoglu; Koji Uchida; Tomoyasu Kagawa; Mitsunori Watabe
- Web page: https://patentgrep.com/patent/US20210077985A1

## CPC

- B01J 29/084: {Y-type faujasite}
- B01J 6/001: {Calcining}
- B01J 29/08: of the faujasite type, e.g. type X or Y
- B01J 29/088: {Y-type faujasite}
- B01J 29/106: {Y-type faujasite}
- B01J 29/126: {Y-type faujasite}
- B01J 29/146: {Y-type faujasite}
- B01J 29/166: {Y-type faujasite}
- B01J 29/89: Silicates, aluminosilicates or borosilicates of titanium, zirconium or hafnium {(B01J29/005 takes precedence)}
- B01J 35/617: {500-1000 m2/g}
- B01J 37/0009: {Use of binding agents; Moulding; Pressing; Powdering; Granulating; Addition of materials ameliorating the mechanical properties of the product catalyst}
- B01J 37/0201: {Impregnation}
- B01J 37/30: Ion-exchange
- C10G 47/14: the catalyst containing platinum group metals or compounds thereof
- C10G 47/16: Crystalline alumino-silicate carriers
- C10G 49/04: containing nickel, cobalt, chromium, molybdenum, or tungsten metals, or compounds thereof
- C10G 49/06: containing platinum group metals or compounds thereof
- C10G 49/08: containing crystalline alumino-silicates, e.g. molecular sieves
- B01J 35/70: characterised by their crystalline properties, e.g. semi-crystalline (catalysts comprising carbon B01J21/18; molecular sieves B01J29/00)
- B01J 2029/081: {Increasing the silica/alumina ratio; Desalumination}
- B01J 2229/16: to increase the Si/Al ratio; Dealumination
- B01J 2229/183: in framework positions
- B01J 2229/186: not in framework positions
- B01J 2229/20: to introduce other elements in the catalyst composition comprising the molecular sieve, but not specially in or on the molecular sieve itself
- B01J 2229/34: Reaction with organic or organometallic compounds
- B01J 2229/37: Acid treatment
- B01J 2229/42: Addition of matrix or binder particles
- B01J 2235/00: Indexing scheme associated with group B01J35/00, related to the analysis techniques used to determine the catalysts form or properties
- C07C 2529/10: containing iron group metals, noble metals or copper
- C07C 2529/12: Noble metals
- C07C 2529/14: Iron group metals or copper
- C07C 2529/16: containing arsenic, antimony, bismuth, vanadium, niobium, tantalum, polonium, chromium, molybdenum, tungsten, manganese, technetium or rhenium
- C07C 2529/89: Silicates, aluminosilicates or borosilicates of titanium, zirconium or hafnium
- C10G 47/18: the catalyst containing platinum group metals or compounds thereof
- C10G 47/20: the catalyst containing other metals or compounds thereof
- C10G 2300/70: Catalyst aspects
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C10G: CRACKING HYDROCARBON OILS; PRODUCTION OF LIQUID HYDROCARBON MIXTURES, e.g. BY DESTRUCTIVE HYDROGENATION, OLIGOMERISATION, POLYMERISATION (cracking to hydrogen or synthesis gas C01B; cracking or pyrolysis of hydrocarbon gases to individual hydrocarbons or mixtures thereof of definite or specified constitution C07C; cracking to cokes C10B); RECOVERY OF HYDROCARBON OILS FROM OIL-SHALE, OIL-SAND, OR GASES; REFINING MIXTURES MAINLY CONSISTING OF HYDROCARBONS; REFORMING OF NAPHTHA; MINERAL WAXES
- C07C: ACYCLIC OR CARBOCYCLIC COMPOUNDS

## Abstract

A method including subjecting an ultra-stable Y-type zeolite having a low silica-to-alumina molar ratio (SAR), such as in a range of 3 to 6, to acid treatment and heteroatom incorporation contemporaneously to give a framework-modified ultra-stable Y-type zeolite.

## Claims

### Claim 1

A method of producing a hydrocracking catalyst for hydrocarbon oil, comprising:
exchanging at least 80% of sodium (Na) ions in a Y-type zeolite with ammonium (NH4) ions to convert the Y-type zeolite to an ultra-stable Y-type zeolite comprising a silica-to-alumina molar ratio (SAR) in a range of 3 to 6; and
subjecting the ultra-stable Y-type zeolite to acid treatment and heteroatom incorporation contemporaneously to give a framework-modified ultra-stable Y-type zeolite comprising an SAR of at least 20, wherein heteroatoms incorporated into a framework of the ultra-stable Y-type zeolite in the heteroatom incorporation comprise titanium atoms and further comprise zirconium atoms or hafnium atoms, or both.

### Claim 2 (depends on 1)

The method of claim 1, wherein exchanging at least 80% of Na ions in the Y-type zeolite with NH4 ions comprises ion exchange and calcination, and wherein the framework-modified ultra-stable Y-type zeolite is a framework-substituted ultra-stable Y-type zeolite in which aluminum atoms in a framework of the ultra-stable Y-type zeolite are replaced with the heteroatoms.

### Claim 3 (depends on 1)

The method of claim 1, wherein the acid treatment and the heteroatom incorporation comprise preparing a suspension of the ultra-stable Y-type zeolite in water, adding acid to the suspension, and adding a solution comprising the heteroatoms to the suspension, and wherein the framework-modified ultra-stable Y-type zeolite comprising an SAR of at least 30.

### Claim 4 (depends on 3)

The method of claim 3, wherein the acid comprises sulfuric acid, nitric acid, hydrochloric acid, or carboxylic acids, or any combinations thereof, and wherein the solution comprises an aqueous solution.

### Claim 5 (depends on 3)

The method of claim 3, wherein the solution comprises a first aqueous solution comprising the titanium atoms and a second aqueous solution comprising zirconium atoms or hafnium atoms.

### Claim 6 (depends on 3)

The method of claim 3, wherein the acid treatment and heteroatom incorporation comprises neutralizing the suspension to give the framework-modified ultra-stable Y-type zeolite, and wherein the framework-modified ultra-stable Y-type zeolite comprises an SAR in a range of 20 to 100.

### Claim 7 (depends on 1)

The method of claim 1, wherein the framework-modified ultra-stable Y-type zeolite comprises an SAR of at least 40 and a crystal lattice constant in a range of 2.430 nanometers (nm) to 2.450 nm.

### Claim 8 (depends on 1)

The method of claim 1, comprising preparing a support of the hydrocracking catalyst, the support comprising the framework-modified ultra-stable Y-type zeolite and an inorganic oxide as a granulating agent or binder.

### Claim 9 (depends on 8)

The method of claim 8, wherein the inorganic oxide comprises alumina, silica, titania, silica-alumina, alum ina-titania, alum ina-zirconia, alum ina-boria, phosphorus-alumina, silica-alum ina-boria, phosphorus-alum ina-boria, phosphorus-alumina-silica, silica-alumina-titania, or silica-alum ina-zirconia, or any combinations thereof.

### Claim 10 (depends on 8)

The method of claim 8, comprising impregnating the support with an active phase metal.

### Claim 11 (depends on 8)

The method of claim 8, comprising impregnating the support with a hydrogenative metal such that the support carries the hydrogenative metal.

### Claim 12 (depends on 1)

The method of claim 1, comprising forming the hydrocracking catalyst with the framework-modified ultra-stable Y-type zeolite in a catalyst support of the hydrocracking catalyst, wherein the framework-modified ultra-stable Y-type zeolite comprises a specific surface area in a range of 600 square meter per gram (m2/g) to 900 m2/g.

### Claim 13

A method of producing a hydrocracking catalyst, comprising
preparing a suspension of an ultra-stable Y-type zeolite in a liquid, the ultra-stable Y-type zeolite having a silica-to-alumina molar ratio (SAR) in a range of 3 to 6;
performing acid treatment on the ultra-stable Y-type zeolite to increase the SAR of the ultra-stable Y-type zeolite, the acid treatment comprising adding an acid to the suspension;
adding heteroatoms to the suspension contemporaneous with performing the acid treatment to incorporate the heteroatoms into a framework of the ultra-stable Y-type zeolite to give a framework-substituted ultra-stable Y-type zeolite having an SAR of at least 20; and
impregnating a hydrogenative metal on a catalyst support comprising the framework-substituted ultra-stable Y-type zeolite.

### Claim 14 (depends on 13)

The method of claim 13, wherein the heteroatoms added to the suspension and incorporated into the framework comprise titanium atoms and further comprise zirconium atoms or hafnium atoms, or both, wherein to incorporate the heteroatoms into the framework comprises to replace aluminum atoms in the framework with the heteroatoms, and wherein the framework-substituted ultra-stable Y-type zeolite has an SAR of at least 30.

### Claim 15 (depends on 13)

The method of claim 13, comprising replacing at least 80% of sodium (Na) ions in a Y-type zeolite with ammonium (NH4) ions to give the ultra-stable Y-type zeolite, and wherein the framework-substituted ultra-stable Y-type zeolite comprises a specific surface area in the range of 600 square meter per gram (m2/g) to 900 m2/g.

### Claim 16 (depends on 15)

The method of claim 15, wherein replacing at least 80% of Na ions in the Y-type zeolite with NH4 ions comprises ion exchange and calcination, wherein the suspension comprises a mass ratio of the liquid to solid in a range of 5 to 15, wherein the liquid in the suspension comprises water, and wherein the framework-substituted ultra-stable Y-type zeolite has an SAR of at least 40.

### Claim 17 (depends on 13)

The method of claim 13, wherein the framework-substituted ultra-stable Y-type zeolite comprises a crystal lattice constant in a range of 2.430 nanometers (nm) to 2.450 nm, and wherein the hydrogenative metal is less than 40% by mass of the hydrocracking catalyst.

### Claim 18 (depends on 13)

The method of claim 13, comprising forming the hydrocracking catalyst with a catalyst support comprising the framework-substituted ultra-stable Y-type zeolite, and wherein the framework-substituted ultra-stable Y-type zeolite comprises an SAR in a range of 30 to 100.

### Claim 19 (depends on 13)

The method of claim 13, wherein the hydrogenative metal comprises a metal component comprising iron, cobalt, nickel, rhodium, palladium, silver, iridium, platinum, gold, chromium, molybdenum, or tungsten, or any combinations thereof.

### Claim 20

A method of forming a framework-modified ultra-stable Y-type zeolite for a catalyst support of a hydrocracking catalyst, comprising:
subjecting an ultra-stable Y-type zeolite having a silica-to-alumina molar ratio (SAR) in a range of 3 to 6 to acid treatment and heteroatom incorporation contemporaneously to give the framework-modified ultra-stable Y-type zeolite; and
wherein the framework-modified ultra-stable Y-type zeolite comprises an SAR of at least 30 and a specific surface area of at least 600 square meter per gram (m2/g).

### Claim 21 (depends on 20)

The method of claim 20, comprising:
performing a first ion-exchange on a Y-type zeolite to exchange sodium ions of the Y-type zeolite with ammonium ions to give a first ammonium-exchanged Y-type zeolite;
calcining the first ammonium-exchanged Y-type zeolite;
performing a second ion-exchange on the first ammonium-exchanged Y-type zeolite as calcined to exchange sodium ions of the first ammonium-exchanged Y-type zeolite as calcined with ammonium ions to give a second ammonium-exchanged Y-type zeolite; and
calcining the second ammonium-exchanged Y-type zeolite to give the ultra-stable Y-type zeolite.

### Claim 22 (depends on 21)

The method of claim 21, wherein at least 80% of sodium ions in the Y-type zeolite are replaced with ammonium ions, and wherein the framework-modified ultra-stable Y-type zeolite comprises a crystal lattice constant in the range of 2.430 nanometers (nm) to 2.450 nm.

### Claim 23 (depends on 20)

The method of claim 20, comprising preparing a suspension of the ultra-stable Y-type zeolite in water, wherein subjecting the ultra-stable Y-type zeolite to acid treatment and heteroatom incorporation contemporaneously comprises mixing acid with the suspension so that a pH of the suspension is less than 2.0, mixing heteroatoms with the suspension, and neutralizing the suspension to give the framework-modified ultra-stable Y-type zeolite.

### Claim 24 (depends on 20)

The method of claim 20, comprising preparing the catalyst support having the framework-modified ultra-stable Y-type zeolite as a component for the hydrocracking catalyst, wherein the framework-modified ultra-stable Y-type zeolite comprises an SAR of at least 40.