# US 2021/0071280 A1 · Grain-oriented electrical steel sheet and manufacturing method therefor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0071280 A1
- Document ID: US20210071280A1
- Status: Published application
- Kind: A1
- Application number: 16/958,195
- Filed: 2018-12-17
- Published: 2021-03-11
- Earliest claimed: 2017-12-26
- Assignees: Posco
- Applicants: Posco
- Inventors: Kyu-Seok HAN; Jae Kyoum KIM; Chang Soo PARK; Jin-Wook SEO; Jong-Tae PARK
- Web page: https://patentgrep.com/patent/US20210071280A1

## CPC

- C21D 9/46: for sheet metals
- C22C 38/004: {Very low carbon steels, i.e. having a carbon content of less than 0,01%}
- C21D 6/00: Heat treatment of ferrous alloys
- C21D 6/001: {containing Ni (C21D6/004 takes precedence)}
- C21D 6/005: {containing Mn}
- C21D 6/008: {containing Si}
- C21D 8/12: during manufacturing of articles with special electromagnetic properties
- C21D 8/1222: {Hot rolling}
- C21D 8/1233: {Cold rolling}
- C21D 8/1255: {with diffusion of elements, e.g. decarburising, nitriding}
- C21D 8/1272: {Final recrystallisation annealing}
- C22C 38/001: {containing N}
- C22C 38/002: {containing In, Mg, or other elements not provided for in one single group C22C38/001 - C22C38/60}
- C22C 38/008: {containing tin}
- C22C 38/02: containing silicon
- C22C 38/04: containing manganese
- C22C 38/12: containing tungsten, tantalum, molybdenum, vanadium, or niobium
- C22C 38/16: containing copper
- C22C 38/20: with copper
- C22C 38/22: with molybdenum or tungsten
- C22C 38/32: with boron
- C22C 38/34: with more than 1.5% by weight of silicon
- C22C 38/60: containing lead, selenium, tellurium, or antimony, or more than 0.04% by weight of sulfur
- H01F 1/147: Alloys characterised by their composition {(treatment thereof for enhancing their electromagnetic properties C21D8/12)}
- C21D 2201/05: Grain orientation
- C22C 2202/02: Magnetic
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES

## Abstract

A grain-oriented electrical steel sheet according to an embodiment of the present invention contains, in a unit of wt %, Si at 2.0 wt % to 4.5 wt %, C at 0.005 wt % or less (excluding 0 wt %), Mn at 0.001 wt % to 0.08 wt %, P at 0.001 wt % to 0.1 wt %, Cu at 0.001 wt % to 0.1 wt %, S at 0.0005 wt % to 0.05 wt %, Se at 0.0005 wt % to 0.05 wt %, B at 0.0001 wt % to 0.01 wt %, Mo at 0.01 wt % to 0.2 wt %, and the remainder of Fe and inevitable impurities. A sum amount of S and Se is 0.005 to 0.05 wt %.

## Claims

### Claim 1

A grain-oriented electrical steel sheet, comprising
in a unit of wt %, Si at 2.0 wt % to 4.5 wt %, C at 0.005 wt % or less (excluding 0 wt %), Mn at 0.001 wt % to 0.08 wt %, P at 0.001 wt % to 0.1 wt %, Cu at 0.001 wt % to 0.1 wt %, S at 0.0005 wt % to 0.05 wt %, Se at 0.0005 wt % to 0.05 wt %, B at 0.0001 wt % to 0.01 wt %, Mo at 0.01 wt % to 0.2 wt %, and the remainder of Fe and inevitable impurities,
wherein a sum amount of S and Se is 0.005 to 0.05 wt %.

### Claim 2 (depends on 1)

The grain-oriented electrical steel sheet of claim 1, further comprising
B at 0.0011 to 0.01 wt %.

### Claim 3 (depends on 1)

The grain-oriented electrical steel sheet of claim 1, further comprising
Al at 0.0001 to 0.01 wt % and N at 0.0005 to 0.005 wt %.

### Claim 4 (depends on 1)

The grain-oriented electrical steel sheet of claim 1, further comprising
at least one of Cr at 0.001 to 0.1 wt %, Sn at 0.005 to 0.2 wt %, and Sb at 0.005 to 0.2 wt %.

### Claim 5

A manufacturing method of a grain-oriented electrical steel sheet, comprising:
preparing a slab that contains, in a unit of wt %, Si at 2.0 wt % to 4.5 wt %, C at 0.005 wt % or less (excluding 0 wt %), Mn at 0.001 wt % to 0.08 wt %, P at 0.001 wt % to 0.1 wt %, Cu at 0.001 wt % to 0.1 wt %, S at 0.0005 wt % to 0.05 wt %, Se at 0.0005 wt % to 0.05 wt %, B at 0.0001 wt % to 0.01 wt %, Mo at 0.01 wt % to 0.2 wt %, and the remainder of Fe and inevitable impurities, and in which a sum amount of S and Se is 0.005 to 0.05 wt %;
heating the slab;
hot rolling the slab to prepare a hot rolled sheet;
cold rolling the hot rolled sheet to prepare a cold rolled sheet;
primary recrystallization annealing the cold rolled sheet; and
secondary recrystallization annealing the cold rolled sheet in which the first recrystallization annealing is completed.

### Claim 6 (depends on 5)

The manufacturing method of the grain-oriented electrical steel sheet of claim 5, wherein
after the preparing of the hot rolled sheet, the hot rolled sheet has an edge crack maximum depth of 20 mm or less.

### Claim 7 (depends on 5)

The manufacturing method of the grain-oriented electrical steel sheet of claim 5, wherein
the cold rolled sheet in which the first recrystallization annealing is completed includes one or more precipitates of (Fe,Mn,Cu)S and (Fe,Mn,Cu)Se.

### Claim 8 (depends on 5)

The manufacturing method of the grain-oriented electrical steel sheet of claim 5, wherein
the primary recrystallization annealing is performed in a hydrogen and nitrogen mixed atmosphere at a dew point temperature of 50° C. to 70° C.