# US 2021/0071277 A1 · Steel sheet with excellent bake hardening properties and plating adhesion and manufacturing method therefor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0071277 A1
- Document ID: US20210071277A1
- Status: Published application
- Kind: A1
- Application number: 16/955,383
- Filed: 2018-11-30
- Published: 2021-03-11
- Earliest claimed: 2017-12-24
- Assignees: Posco
- Applicants: Posco
- Inventors: Sang-Ho HAN; Je-Woong LEE
- Web page: https://patentgrep.com/patent/US20210071277A1

## CPC

- C21D 9/46: for sheet metals
- B32B 15/013: {one layer being formed of an iron alloy or steel, another layer being formed of a metal other than iron or aluminium}
- C21D 6/002: {containing Cr (C21D6/004 takes precedence)}
- C21D 6/005: {containing Mn}
- C21D 6/008: {containing Si}
- C21D 8/02: during manufacturing of plates or strips (C21D8/12 takes precedence)
- C21D 8/0226: {Hot rolling}
- C21D 8/0236: {Cold rolling}
- C21D 8/0263: {following hot rolling}
- C21D 8/0273: {Final recrystallisation annealing}
- C22C 38/001: {containing N}
- C22C 38/002: {containing In, Mg, or other elements not provided for in one single group C22C38/001 - C22C38/60}
- C22C 38/02: containing silicon
- C22C 38/04: containing manganese
- C22C 38/06: containing aluminium
- C22C 38/22: with molybdenum or tungsten
- C22C 38/32: with boron
- C22C 38/38: with more than 1.5% by weight of manganese
- C22C 38/60: containing lead, selenium, tellurium, or antimony, or more than 0.04% by weight of sulfur
- C23C 2/02: Pretreatment of the material to be coated, e.g. for coating on selected surface areas (C23C2/30 takes precedence)
- C23C 2/0224: {Two or more thermal pretreatments}
- C23C 2/06: Zinc or cadmium or alloys based thereon
- C23C 2/28: Thermal after-treatment, e.g. treatment in oil bath
- C23C 2/29: {Cooling or quenching}
- C23C 2/40: Plates; Strips
- C21D 2211/005: Ferrite
- C21D 2211/008: Martensite
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

Provided is a steel sheet used as a material for an automotive exterior panel, etc., and a method for manufacturing the same. More particularly, provided is a cold-rolled steel sheet and a hot-dip galvanized steel sheet, which have excellent bake hardening properties, plating adhesion, and anti-aging properties, and a method of manufacturing the same.

## Claims

### Claim 1

A steel sheet having excellent bake hardening and plating adhesion, comprising:
in weight %, 0.005 to 0.08% of carbon (C), 1.3 to 2.3% of manganese (Mn), 0.03% or less (excluding 0%) of phosphorus (P), 0.01% or less (excluding 0%) of sulfur (S), 0.01% or less (excluding 0%) of nitrogen (N), 0.01 to 0.06% of aluminum (sol.Al), 1.0% or less (excluding 0%) of chromium (Cr), 0.1% or less (excluding 0%) of antimony (Sb), at least one selected from the group consisting of silicon (Si): 0.3% or less (excluding 0%), molybdenum (Mo): 0.2% or less (excluding 0%) and boron (B): 0.003% or less (excluding 0%), a remainder of iron (Fe), and unavoidable impurities, and
as a microstructure, in area %, 1 to 5% of martensite and remaining ferrite,
wherein a relationship (Cgb/Cf) between an Sb average area occupancy ratio (Cgb, %) of grain boundaries of a martensite phase and a ferrite phase and an average Sb area occupancy ratio (Cf, %) in a ferrite phase within 1 μm around the martensite phase, determined by the following relationship 1, at a point of ¼t in a thickness direction of the steel sheet (where t denotes a thickness (mm) of a cold rolled steel sheet is 3.5 or more,
Cgb/Cf≥3.5 [Relationship 1]
(where Cgb (%) indicates an Sb average area occupancy ratio of grain boundaries of a martensitic phase and a ferrite phase at a point of ¼t of a cold rolled steel sheet, and Cf (%) indicates an average Sb area occupancy ratio of a ferrite phase within 1 μm around the martensite phase).

### Claim 2 (depends on 1)

The steel sheet having excellent bake hardening and plating adhesion of claim 1, wherein the steel sheet further comprises a hot-dip galvanized layer formed on a surface.

### Claim 3 (depends on 2)

The steel sheet having excellent bake hardening and plating adhesion of claim 2, wherein the hot-dip galvanized layer is an alloyed hot-dip galvanized layer.

### Claim 4 (depends on 1)

The steel sheet having excellent bake hardening and plating adhesion of claim 1, wherein the steel sheet has a yield strength of 210 to 270 MPa and a yield ratio (YS/TS) of 0.6 or less.

### Claim 5

A method of manufacturing a steel sheet having excellent bake hardening and plating adhesion, comprising:
reheating a slab including, in weight %, 0.005 to 0.08% of carbon (C), 1.3 to 2.3% of manganese (Mn), 0.03% or less (excluding 0%) of phosphorus (P), 0.01% or less (excluding 0%) of sulfur (S), 0.01% or less (excluding 0%) of nitrogen (N), 0.01 to 0.06% of aluminum (sol.Al), 1.0% or less (excluding 0%) of chromium (Cr), 0.1% or less (excluding 0%) of antimony (Sb), at least one selected from the group consisting of silicon (Si): 0.3% or less (excluding 0%), molybdenum (Mo): 0.2% or less (excluding 0%) and boron (B): 0.003% or less (excluding 0%), a remainder of iron (Fe), and unavoidable impurities;
hot rolling the reheated slab at a temperature in a range of 850 to 1150° C. to obtain a hot rolled steel sheet;
cooling the hot rolled steel sheet to a temperature range of 550 to 750° C. at an average cooling rate of 10 to 70° C./sec;
coiling the cooled hot rolled steel sheet at a temperature in a range of 550 to 750° C.;
cold rolling the hot rolled steel sheet to obtain a cold rolled steel sheet;
continuously annealing the cold rolled steel sheet under a hydrogen concentration of 3 to 30% by volume at a temperature in a range of Ac1+20° C. to Ac3−20° C.; and
primary cooling the continuously annealed cold rolled steel sheet to 630 to 670° C. at an average cooling rate of 2 to 10° C./sec.

### Claim 6 (depends on 5)

The method of manufacturing a steel sheet having excellent bake hardening and plating adhesion of claim 5, wherein a rolling reduction during the cold rolling is 40 to 80%.

### Claim 7 (depends on 5)

The method of manufacturing a steel sheet having excellent bake hardening and plating adhesion of claim 5, wherein the cold rolling is performed using a rolling mill comprised of 5 or 6 stands, and an initial stand reduction ratio is set to 25 to 37%.

### Claim 8 (depends on 5)

The method of manufacturing a steel sheet having excellent bake hardening and plating adhesion of claim 5, further comprising:
secondary cooling the primary cooled cold rolled steel sheet until the primary cooled cold rolled steel sheet is immersed in a hot-dip galvanizing bath maintained at 440 to 480° C. at an average cooling rate of 4 to 20° C./sec;
immersing the secondary cooled cold rolled steel sheet in a hot-dip galvanizing bath maintained at 440 to 480° C. to obtain a hot-dip galvanized steel sheet; and
final cooling the hot-dip galvanized steel sheet to (Ms-100) ° C. or less at an average cooling rate of 3° C./sec or more.

### Claim 9 (depends on 8)

The method of manufacturing a steel sheet having excellent bake hardening and plating adhesion of claim 8, further comprising obtaining an alloyed hot-dip galvanized steel sheet by an alloying heat treatment of the hot-dip galvanized steel sheet before the final cooling.

### Claim 10 (depends on 9)

The method of manufacturing a steel sheet having excellent bake hardening and plating adhesion of claim 9, wherein the alloying heat treatment is performed at a temperature in a range of 500 to 540° C.

### Claim 11 (depends on 9)

The method of manufacturing a steel sheet having excellent bake hardening and plating adhesion of claim 9, further comprising temper rolling the hot-dip galvanized steel sheet or the alloyed hot-dip galvanized steel sheet.

### Claim 12 (depends on 11)

The method of manufacturing a steel sheet having excellent bake hardening and plating adhesion of claim 11, wherein a rolling reduction during the temper rolling is 0.3 to 1.6%.