# US 2021/0070968 A1 · Process for Producing Polymer Compositions Having Multimodal Molecular Weight Distribution

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0070968 A1
- Document ID: US20210070968A1
- Status: Published application
- Kind: A1
- Application number: 16/644,817
- Filed: 2018-06-28
- Published: 2021-03-11
- Earliest claimed: 2017-09-28
- Applicants: ExxonMobil Chemical Patents Inc.
- Inventors: Dongming Li
- Web page: https://patentgrep.com/patent/US20210070968A1

## CPC

- C08L 23/0815: {with aliphatic 1-olefins containing one carbon-to-carbon double bond}
- B29C 48/022: {characterised by the choice of material}
- C08J 3/005: {Processes for mixing polymers}
- C08L 2203/30: used for thermoforming
- C08L 2205/025: containing two or more polymers of the same hierarchy C08L, and differing only in parameters such as density, comonomer content, molecular weight, structure
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)

## Abstract

A process is described for producing a multimodal polymer composition comprising a high molecular weight polymer (1) and a low molecular weight polymer (2), wherein the weight ratio of polymer (1) to polymer (2) is at a first value, x. The process comprises compounding in a first compounding stage a mixture of polymer (1) and polymer (2), wherein the weight ratio of polymer (1) to polymer (2) in the mixture is at a second value, y, such that y>x to form a first blend. Polymer (2) is then added to the first blend and the mixture of polymer (2) and the first blend is compounded in a second compounding stage to produce a second blend.

## Claims

### Claim 1

A process of producing a multimodal polymer composition comprising a high molecular weight polymer (1) and a low molecular weight polymer (2), wherein the weight ratio of polymer (1) to polymer (2) is at a first value x, the process comprising:
(a) compounding a mixture of polymer (1) and polymer (2) in a first compounding stage to form a first blend, wherein the weight ratio of polymer (1) to polymer (2) in the first blend is at a second value, y, such that 1<y>x;
(b) adding polymer (2) to the first blend; and
(c) compounding the mixture of polymer (2) and the first blend in a second compounding stage to produce a second blend.

### Claim 2 (depends on 1)

The process of claim 1, wherein the weight ratio of polymer (1) to polymer (2) in the second blend is equal to x.

### Claim 3 (depends on 1)

The process of claim 1, wherein the weight ratio of polymer (1) to polymer (2) in the second blend is greater than x and at least one further addition of polymer (2) and at least one further compounding stage are conducted to produce a final blend in which the weight ratio of polymer (1) to polymer (2) is equal to x.

### Claim 4 (depends on 1)

The process of claim 1, wherein x is from 0.1 to 1.5.

### Claim 5 (depends on 1)

The process of claim 1, wherein y is from 1.5× to 6×.

### Claim 6 (depends on 1)

The process of claim 1, wherein each of the high molecular weight polymer (1) and the low molecular weight polymer (2) comprises polyethylene.

### Claim 7 (depends on 1)

The process of claim 1, wherein the high molecular weight polymer (1) has an I2 less than 20 g/10 minutes at 190° C. and a load of 21.6 kg.

### Claim 8 (depends on 1)

The process of claim 1, wherein the low molecular weight polymer (2) has an I2 of at least 1 g/10 minutes at 190° C. and a load of 2.16 kg.

### Claim 9 (depends on 1)

The process of claim 1, wherein each of the high molecular weight polymer (1) and the low molecular weight polymer (2) has a molecular weight distribution (Mw/Mn) less than 8.0.

### Claim 10 (depends on 1)

The process of claim 1, wherein the first and second compounding stages are conducted in separate extruders.

### Claim 11 (depends on 1)

The process of claim 1, wherein the first and second compounding stages are conducted during separate passes through the same extruder.

### Claim 12 (depends on 1)

The process of claim 1, wherein the first and second compounding stages are conducted in separate mixing zones of the same extruder during a single pass through the extruder.

### Claim 13 (depends on 1)

The process of claim 1, wherein the first compounding stage is conducted at a temperature from 200 to 250° C.

### Claim 14 (depends on 1)

The process of claim 1, wherein the second compounding stage is conducted at a temperature from 200 to 250° C.

### Claim 15 (depends on 1)

A multimodal polymer composition formed from the process of claim 1.

### Claim 16 (depends on 15)

The multimodal polymer composition of claim 15, wherein the multimodal polymer composition has a large gel count less than 1 per square meter.

### Claim 17 (depends on 15)

The multimodal polymer composition of claim 15, wherein the multimodal polymer composition has a small gel count less than 50,000 per square meter.

### Claim 18 (depends on 15)

The multimodal polymer composition of claim 15, wherein the multimodal polymer composition has a normalized total defect area (TDA) less than 1,000 ppm.

### Claim 19 (depends on 15)

The multimodal polymer composition of claim 15, wherein the multimodal polymer composition has an elongation at break greater than 600% according to ASTM D 638.

### Claim 20 (depends on 15)

An article comprising the multimodal polymer composition of claim 15.