# US 2021/0069683 A1 · Catalytic hydrocarbon dehydrogenation

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0069683 A1
- Document ID: US20210069683A1
- Status: Published application
- Kind: A1
- Application number: 16/566,801
- Filed: 2019-09-10
- Published: 2021-03-11
- Earliest claimed: 2019-09-10
- Assignees: Saudi Arabian Oil Company
- Applicants: Saudi Arabian Oil Company
- Inventors: Mohammed Abdulmajeed Al-Daous; Hussam A. Bahlouli
- Web page: https://patentgrep.com/patent/US20210069683A1

## CPC

- B01J 23/626: {with tin}
- B01J 29/06: Crystalline aluminosilicate zeolites; Isomorphous compounds thereof
- B01J 23/58: with alkali- or alkaline earth metals
- B01J 29/60: of the type L, as exemplified by patent document US3216789
- B01J 29/62: Noble metals
- B01J 35/615: {100-500 m2/g}
- B01J 35/617: {500-1000 m2/g}
- C07C 5/325: {of the platinum group}
- C07C 5/3337: {of the platinum group}
- B01J 21/066: {Zirconium or hafnium; Oxides or hydroxides thereof}
- B01J 2229/42: Addition of matrix or binder particles
- C07C 2521/06: Silicon, titanium, zirconium or hafnium; Oxides or hydroxides thereof
- C07C 2529/06: Crystalline aluminosilicate zeolites; Isomorphous compounds thereof
- C07C 2529/62: Noble metals
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C07C: ACYCLIC OR CARBOCYCLIC COMPOUNDS

## Abstract

A catalyst for dehydrogenation of hydrocarbons includes a support including zirconium oxide and Linde type L zeolite (L-zeolite). A concentration of the zirconium oxide in the catalyst is in a range of from 0.1 weight percent (wt. %) to 20 wt. %. The catalyst includes from 5 wt. % to 15 wt. % of an alkali metal or alkaline earth metal. The catalyst includes from 0.1 wt. % to 10 wt. % of tin. The catalyst includes from 0.1 wt. % to 8 wt. % of a platinum group metal. The alkali metal or alkaline earth metal, tin, and platinum group metal are disposed on the support.

## Claims

### Claim 1

A catalyst for dehydrogenation of hydrocarbons, the catalyst comprising:
a support comprising zirconium oxide and Linde type L zeolite (L-zeolite), wherein a concentration of the zirconium oxide in the catalyst is in a range of from 0.1 weight percent (wt. %) to 20 wt. %;
from 5 wt. % to 15 wt. % of an alkali metal or alkaline earth metal, the alkali metal or alkaline earth metal disposed on the support;
from 0.1 wt. % to 10 wt. % of tin, the tin disposed on the support; and
from 0.1 wt. % to 8 wt. % of a platinum group metal, the platinum group metal disposed on the support.

### Claim 2 (depends on 1)

The catalyst of claim 1, wherein the alkali metal or alkaline earth metal is selected from the group consisting of lithium, sodium, potassium, rubidium, cesium, beryllium, magnesium, calcium, and barium.

### Claim 3 (depends on 2)

The catalyst of claim 2, wherein the alkali metal is potassium or cesium.

### Claim 4 (depends on 2)

The catalyst of claim 2, wherein the platinum group metal is selected from the group consisting of platinum, ruthenium, iridium, rhodium, and palladium.

### Claim 5 (depends on 2)

The catalyst of claim 2, wherein the catalyst is configured to dehydrogenate hydrocarbons including 3 to 6 carbon atoms at an operating temperature in a range of from about 500 degrees Celsius (° C.) to about 800° C. and an operating pressure in a range of from about 0.01 bar to about 10 bar.

### Claim 6 (depends on 5)

The catalyst of claim 5, wherein the catalyst is configured to dehydrogenate hydrocarbons including 3 to 6 carbon atoms in the presence of a diluent gas comprising hydrogen, steam, inert gas, or combinations thereof.

### Claim 7 (depends on 6)

The catalyst of claim 6, wherein a concentration of hydrogen in the diluent gas is in a range of from 5 volume percent (vol. %) to 30 vol. %.

### Claim 8

A method of dehydrogenating hydrocarbons, the method comprising:
subjecting hydrocarbons to be dehydrogenated to an operating temperature in a range of from about 500 degrees Celsius (° C.) to about 800° C. within a reactor, wherein the hydrocarbons to be hydrogenated comprise n-pentane;
subjecting the hydrocarbons to be dehydrogenated to an operating pressure in a range of from about 0.01 bar to about 10 bar within the reactor;
while subjecting the hydrocarbons to be dehydrogenated to the operating temperature and operating pressure within the reactor,
introducing a diluent gas to the hydrocarbons to be dehydrogenated, the diluent gas comprising hydrogen and inert gas; and
using a catalyst disposed within the reactor to dehydrogenate the hydrocarbons to be dehydrogenated in the presence of the diluent gas within the reactor, the catalyst comprising:
a support comprising zirconium oxide and L-zeolite, wherein a concentration of the zirconium oxide in the catalyst is in a range of from 0.1 weight percent (wt. %) to 20 wt. %;
from 5 wt. % to 15 wt. % of an alkali metal or alkaline earth metal, the alkali metal or alkaline earth metal disposed on the support;
from 0.1 wt. % to 10 wt. % of tin, the tin disposed on the support; and
from 0.1 wt. % to 8 wt. % of a platinum group metal, the platinum group metal disposed on the support, wherein the catalyst forms catalyst grains of about 200 micrometers (μm) to about 500 μm in size.

### Claim 9 (depends on 8)

The method of claim 8, wherein the alkali metal or alkaline earth metal is selected from the group consisting of lithium, sodium, potassium, rubidium, cesium, beryllium, magnesium, calcium, and barium.

### Claim 10 (depends on 9)

The method of claim 9, wherein the alkali metal is potassium or cesium.

### Claim 11 (depends on 9)

The method of claim 9, wherein a ratio of hydrogen to inert gas in the diluent gas is in a range of from 11:70 to 71:10.

### Claim 12 (depends on 9)

The method of claim 9, further comprising, before using the catalyst to dehydrogenate the hydrocarbons to be dehydrogenated, activating the catalyst, wherein activating the catalyst comprises:
placing the catalyst grains within the reactor;
flowing a stream comprising oxygen to the catalyst grains within the reactor; while flowing the stream comprising oxygen to the catalyst grains, increasing a temperature within the reactor to 450° C.;
after the temperature within the reactor reaches 450° C., flowing a stream comprising an inert gas to the catalyst grains within the reactor;
while flowing the stream comprising the inert gas to the catalyst grains, decreasing the temperature within the reactor to 400° C.;
after the temperature within the reactor reaches 400° C., flowing a stream comprising hydrogen to the catalyst grains within the reactor; and
adjusting the temperature within the reactor to the operating temperature.

### Claim 13

A method of preparing a catalyst for dehydrogenation of hydrocarbons, the method comprising:
mixing a Linde type L zeolite (L-zeolite) with an aqueous solution of a first additive to form a first slurry, the first additive comprising a salt or complex comprising zirconium;
drying the first slurry in the presence of oxygen to form a first solid;
mixing the first solid with an aqueous solution of a second additive to form a second slurry, the second additive comprising a salt comprising an alkali metal or an alkaline earth metal;
drying the second slurry to form a second solid;
mixing the second solid with an ethanolic solution of a third additive to form a third slurry, the third additive comprising a salt or complex comprising tin;
drying the third slurry to form a third solid;
mixing the third solid with an aqueous solution of a fourth additive to form a fourth slurry, the fourth additive comprising a salt or complex comprising a platinum group metal;
drying the fourth slurry in the presence of oxygen to form the catalyst having a composition comprising:
from 0.1 weight percent (wt. %) to 20 wt. % of zirconium derived from the first additive; from 5 wt. % to 15 wt. % of the alkali metal or alkaline earth metal derived from the second additive;
from 0.1 wt. % to 10 wt. % of the tin derived from the third additive;
from 0.1 wt. % to 8 wt. % of the platinum group metal derived from the fourth additive;
and
a balance of L-zeolite.

### Claim 14 (depends on 13)

The method of claim 13, wherein the first additive is selected from the group consisting of zirconium oxynitrate, zirconium oxychloride, zirconium acetate, and zirconium acetylacetonate.

### Claim 15 (depends on 13)

The method of claim 13, wherein an anionic portion of the salt in the second additive is selected from the group consisting of nitrate ion, nitrite ion, sulfate ion, hydroxide ion, and halide ion.

### Claim 16 (depends on 13)

The method of claim 13, wherein the third additive is selected from the group consisting of tin(II) chloride dehydrate, tin(IV) chloride hydrate, and tin(IV) bis(acetylacetonate).

### Claim 17 (depends on 13)

The method of claim 13, wherein the fourth additive is selected from the group consisting of dihydrogen hexachloroplatinate hexahydrate, tetraammineplatinum dihydroxide, tetraammineplatinum dinitrate, and tetraammineplatinum dichloride.

### Claim 18 (depends on 13)

The method of claim 13, further comprising, before mixing the L-zeolite with the aqueous solution of the first additive, treating the L-zeolite such that a Brunauer-Emmett-Teller (BET) surface area of the L-zeolite is at least 200 square meters per gram, wherein treating the L-zeolite comprises:
heating the L-zeolite to a first temperature in the presence of oxygen;
maintaining the L-zeolite at the first temperature in the presence of oxygen for a first time duration;
heating the L-zeolite to a second temperature in the presence of oxygen, wherein the second temperature is greater than the first temperature; and
maintaining the L-zeolite at the second temperature in the presence of oxygen for a second time duration.

### Claim 19 (depends on 18)

The method of claim 18, wherein:
the first temperature is in a range of from about 100 degrees Celsius (° C.) to about 150° C.; the first time duration is in a range of from about 1 hour to about 10 hours;
the second temperature is in a range of from about 550° C. to about 700° C.; and the second time duration is in a range of from about 12 hours to about 24 hours.

### Claim 20 (depends on 19)

The method of claim 19, wherein:
heating the L-zeolite to the first temperature comprises heating the L-zeolite at a temperature increase rate of about 5° C. per minute; and
heating the L-zeolite to the second temperature comprises heating the L-zeolite at a temperature increase rate of about 2° C. per minute.
