# US 2021/0066748 A1 · Solid electrolyte for sodium batteries

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0066748 A1
- Document ID: US20210066748A1
- Status: Published application
- Kind: A1
- Application number: 16/961,757
- Filed: 2019-01-14
- Published: 2021-03-04
- Earliest claimed: 2018-01-12
- Assignees: University of Houston System
- Applicants: University of Houston System
- Inventors: Yan Yao; Xiaowei Chi
- Web page: https://patentgrep.com/patent/US20210066748A1

## CPC

- C03C 3/16: containing phosphorus
- H01M 10/0562: Solid materials
- C03C 3/321: {Chalcogenide glasses, e.g. containing S, Se, Te}
- C03C 4/14: for electro-conductive glass
- H01M 10/054: Accumulators with insertion or intercalation of metals other than lithium, e.g. with magnesium or aluminium
- C03C 2204/00: Glasses, glazes or enamels with special properties
- H01M 10/39: working at high temperature
- H01M 2300/0074: Ion conductive at high temperature
- Y02E 60/10: Energy storage using batteries
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A class of improved solid-state electrolytes and methods for forming such electrolytes are discussed herein. The improved electrolytes may be a sodium oxy-sulfide, such as with a nominal composition of Na3PS4 _xOx (0<x≤2). The electrolytes can be synthesized from using a simple one-step ball-milling method. The ball-milling may be performed at high rotation speeds. The resulting ball-milled materials may further be optionally pressed. The pressing may be performed at low or room temperatures and/or relatively low pressure, and the resulting electrolytes achieve high relative densities. The solid-state electrolyte forms a highly dense layer that approaches a continuous glass that is nearly flawless, is mainly amorphous, and/or maintains a stable low-resistance interface with Na metal and Na-alloy electrodes.

## Claims

### Claim 1

A method for forming an electrolyte comprising:
ball-milling starting materials comprising at least one sodium sulfide material and at least one oxide material; and
pressing resulting ball-milled materials to form a sodium oxy-sulfide glass that is a solid-state electrolyte.

### Claim 2 (depends on 1)

The method of claim 1, wherein the starting materials are Na2S, P2S5, and P2O5 mixed with a molar ratio of 75:(25−y):y where y≠0.

### Claim 3 (depends on 2)

The method of claim 2, wherein 0<y≤20.

### Claim 4 (depends on 2)

The method of claim 2, wherein the sodium oxy-sulfide glass is Na3PS4−xOx with 0<x≤2.

### Claim 5 (depends on 4)

The method of claim 4, wherein x=0.25.

### Claim 6 (depends on 1)

The method of claim 1, wherein the ball milling step is performed at 100° C. or less.

### Claim 7 (depends on 1)

The method of claim 1, wherein the pressing step is performed at a pressure between 100-450 MPa.

### Claim 8 (depends on 1)

The method of claim 1, wherein the electrolyte is a nearly flawless glass.

### Claim 9 (depends on 8)

The method of claim 8, wherein the electrolyte is mainly amorphous.

### Claim 10 (depends on 1)

The method of claim 1, wherein a relative density of the solid-state electrolyte is 95% or greater.

### Claim 11 (depends on 1)

The method of claim 1, wherein the solid-state electrolyte is capable of performing 250 hours or longer with a Na metal or Na-based alloy electrode at 0.2 mA/cm2.

### Claim 12 (depends on 1)

The method of claim 1, wherein the ball milling step is performed at 500 rpm or greater.

### Claim 13

A battery comprising:
at least one sodium metal or sodium-based alloy electrode;
a second electrode; and
a solid-state electrolyte, wherein the electrolyte comprises a sodium oxy-sulfide glass.

### Claim 14 (depends on 13)

The battery of claim 13, wherein the sodium oxy-sulfide glass is a nearly flawless glass.

### Claim 15 (depends on 14)

The battery of claim 14, wherein the sodium oxy-sulfide glass is mainly amorphous.

### Claim 16 (depends on 13)

The battery of claim 13, wherein the sodium oxy-sulfide glass is Na3PS4−xOx with 0<x≤2.

### Claim 17 (depends on 16)

The battery of claim 16, wherein x=0.25.

### Claim 18 (depends on 13)

The battery of claim 13, wherein a relative density of the sodium oxy-sulfide glass is 95% or greater.

### Claim 19 (depends on 13)

The battery of claim 13, wherein the electrolyte further comprises other sulfide materials, and the other sulfide materials are sandwiched between the sodium oxy-sulfide glass.

### Claim 20 (depends on 13)

The battery of claim 13, wherein the electrolyte is capable of performing 250 hours or longer with the sodium metal or the sodium-based alloy electrode at 0.2 mA/cm2.