# US 2021/0066533 A1 · Dicing method for separating wafers comprising a plurality of solar cell stacks

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0066533 A1
- Document ID: US20210066533A1
- Status: Published application
- Kind: A1
- Application number: 17/007,676
- Filed: 2020-08-31
- Published: 2021-03-04
- Earliest claimed: 2019-08-29
- Assignees: AZUR SPACE Solar Power GmbH
- Applicants: AZUR SPACE Solar Power GmbH
- Inventors: Steffen SOMMER; Wolfgang KOESTLER; Alexander FREY
- Web page: https://patentgrep.com/patent/US20210066533A1

## CPC

- H10F 71/00: Manufacture or treatment of devices covered by this subclass (patterning processes to connect thin photovoltaic cells in integrated devices, or assemblies of multiple devices, having photovoltaic cells H10F19/33; manufacture or treatment of encapsulations or containers for integrated devices, or assemblies of multiple devices, having photovoltaic cells H10F19/80; manufacture or treatment of integrated devices, or assemblies of multiple devices, comprising at least one element in which radiation controls the flow of current H10F39/00)
- B23K 26/364: for making a groove or trench, e.g. for scribing a break initiation groove
- H10F 10/142: comprising multiple PN homojunctions, e.g. tandem cells
- H10F 19/20: comprising photovoltaic cells in arrays in or on a single semiconductor substrate, the photovoltaic cells having planar junctions (having multiple thin-film photovoltaic cells deposited on the same substrate H10F19/31)
- H10F 19/804: {Materials of encapsulations}
- H10P 54/00: Cutting or separating of wafers, substrates or parts of devices
- B23K 2101/40: Semiconductor devices
- B23K 2103/56: {being semiconducting}
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A dicing method for separating a wafer comprising a plurality of solar cells stack along at least one parting line, at least having the steps of: providing the wafer with a top, a bottom, an adhesive layer which is integrally bonded with the top and a cover glass layer which is integrally bonded with the adhesive layer, wherein the wafer includes a plurality of solar cell stacks, each having a germanium substrate layer forming the bottom of the wafer, a germanium sub-cell and at least two III-V sub-cells; creating a separating trench along the parting line by means of laser ablation, which extends from a bottom of the wafer through the wafer and the adhesive layer at least up to a top of the cover glass layer; and dividing the cover glass layer along the separating trench.

## Claims

### Claim 1

A dicing method for separating a wafer along at least one parting line, the method comprising:
providing the wafer having a top, a bottom, an adhesive layer that is integrally bonded to the top and a cover glass layer that is integrally bonded to the adhesive layer, the wafer having at least two solar cell stacks, each of the at least two solar cell stacks comprising a germanium substrate layer forming the bottom of the wafer, a germanium sub-cell and at least two III-V sub-cells;
creating a separating trench that extends from a bottom of the wafer through the wafer and through the adhesive layer at least up to a bottom of the cover glass layer adjoining the adhesive layer along the parting line via laser ablation; and
dividing the cover glass layer along the separating trench.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the separating trench is created up to an area of the cover glass layer adjoining the adhesive layer.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the separation of the cover glass layer is carried out by breaking or by sawing.

### Claim 4 (depends on 1)

The method according to claim 1, wherein, for the laser ablation, a laser is moved on the bottom of the wafer along at least one track, which extends along or parallel to the parting line, and wherein an energy input takes place along the track via a focused laser beam.

### Claim 5 (depends on 4)

The method according to claim 4, wherein the energy input takes place along at least 2 and at most 30 tracks.

### Claim 6 (depends on 1)

The method according to claim 1, wherein, in an ablation passage, an energy input takes place along n tracks with 1<n<30 and the ablation pass being repeated at least once, wherein the number n of the tracks remains the same or is reduced with each repetition, and wherein the number n is reduced with at least one repetition.

### Claim 7 (depends on 6)

The method according to claim 6, wherein the ablation pass is repeated at least once and at most 40 times.

### Claim 8 (depends on 1)

The method according to claim 1, wherein, in one ablation pass, an energy input is carried out with a first power density and with a first focal plane and the ablation pass is repeated at least once, wherein the power density and/or the focus plane is changed in at least one repetition.

### Claim 9 (depends on 1)

The method according to claim 1, wherein, prior to creating the trench, the top of the cover glass layer is integrally bonded with a foil.

### Claim 10 (depends on 1)

The method according to claim 1, wherein the adhesive layer comprises silicon and has a layer thickness of at least 5 μm.

### Claim 11 (depends on 1)

The method according to claim 1, wherein the cover glass layer has a layer thickness of at least 50 μm.

### Claim 12 (depends on 1)

The method according to claim 1, wherein the energy input is carried out via a pulsed laser, and wherein a duration of the pulse is between 10 fs and 100 ns and/or a wavelength is between 315 nm and 1070 nm or between 1.5 μm and 10.6 μm.