# US 2021/0063903 A1 · Toner and method of producing toner

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0063903 A1
- Document ID: US20210063903A1
- Status: Published application
- Kind: A1
- Application number: 17/002,879
- Filed: 2020-08-26
- Published: 2021-03-04
- Earliest claimed: 2019-08-29
- Assignees: Canon Kabushiki Kaisha
- Applicants: Canon Kabushiki Kaisha
- Inventors: Takaho Shibata; Yuichi Mizo; Koh Ishigami; Takakuni Kobori; Masaharu Miura; Takeshi Ohtsu; Yosuke Iwasaki; Daisuke Yamashita; Ryo Nakajima; Wakiko Katsumata; Hitoshi Sano; Kenta Mitsuiki; Rei Hijikawa
- Web page: https://patentgrep.com/patent/US20210063903A1

## CPC

- G03G 9/08755: {Polyesters}
- G03G 9/081: {by mixing the toner components in a liquefied state; melt kneading; reactive mixing}
- G03G 9/0815: {Post-treatment}
- G03G 9/0819: {characterised by the dimensions of the particles}
- G03G 9/08728: {Polymers of esters}
- G03G: ELECTROGRAPHY; ELECTROPHOTOGRAPHY; MAGNETOGRAPHY

## Abstract

A toner containing a toner particle that contains a binder resin including a polyester resin, and a polyolefin resin having —COOM that is a neutralized carboxy group with a monovalent metal ion M, wherein the polyolefin resin having —COOM is a polymer in which a vinyl polymer is bonded to a polyolefin, a content of a monomer unit containing —COOM in the polyolefin resin having —COOM is 1 to 20 mass %, and in a FT-IR spectrum obtained through measurement of a large particle size-side particle group and a small particle size-side particle group obtained by dividing the toner into two substantially equal parts, on a number basis, a ratio of the intensity of a maximum absorption peak in a range from 1545 cm−1 to 1555 cm−1 with respect to the intensity of a maximum absorption peak in a range from 1713 cm−1 to 1723 cm−1 exhibits a specific relationship.

## Claims

### Claim 1

A toner comprising a toner particle that contains
a binder resin including a polyester resin, and
a polyolefin resin having —COOM that is a neutralized carboxy group with a monovalent metal ion M, wherein
the polyolefin resin having —COOM is a polymer in which a vinyl polymer is bonded to a polyolefin;
a content ratio of a monomer unit containing —COOM in the polyolefin resin having —COOM is from 1 mass % to 20 mass %;
the toner satisfies an expression (1);
1.10≤(As/Bs)/(Al/Bl)≤2.00 (1)
where
when the toner is divided into two groups, i.e. a first group and a second group with an inertial classifier, the first group including a larger size of the toner particles, and the second group including smaller size of the toner particles, and the number of the toner particles in the first group being substantially equal to the number of the toner particles in the second group,
As denotes a ratio of an intensity of a maximum absorption peak in a range from 1545 cm−1 to 1555 cm−1, assigned to —COOM contained in the polyolefin resin, with respect to an intensity of a maximum absorption peak in a range from 1713 cm−1 to 1723 cm−1, assigned to carbonyl in the polyester resin, in a FT-IR spectrum obtained through measurement of the second group in accordance with an ATR method, using Ge as an ATR crystal, and under a condition where an infrared light incidence angle is set to 45°;
Bs denotes a ratio of an intensity of a maximum absorption peak in a range from 1545 cm−1 to 1555 cm−1, assigned to —COOM contained in the polyolefin resin, with respect to an intensity of a maximum absorption peak in a range from 1713 cm−1 to 1723 cm−1, assigned to carbonyl in the polyester resin, in a FT-IR spectrum obtained through measurement of the second group in accordance with an ATR method, using diamond as an ATR crystal, and under a condition where an infrared light incidence angle is set to 45°;
Al denotes a ratio of an intensity of a maximum absorption peak in a range from 1545 cm−1 to 1555 cm−1, assigned to —COOM contained in the polyolefin resin, with respect to an intensity of a maximum absorption peak in a range from 1713 cm−1 to 1723 cm−1, assigned to carbonyl in the polyester resin, in a FT-IR spectrum obtained through measurement of the first group in accordance with an ATR method, using Ge as an ATR crystal, and under a condition where an infrared light incidence angle is set to 45°; and
Bl denotes a ratio of an intensity of a maximum absorption peak in a range from 1545 cm−1 to 1555 cm−1, assigned to —COOM contained in the polyolefin resin, with respect to an intensity of a maximum absorption peak in a range from 1713 cm−1 to 1723 cm−1, assigned to carbonyl in the polyester resin, in a FT-IR spectrum obtained through measurement of the first group in accordance with an ATR method, using diamond as an ATR crystal, and under a condition where an infrared light incidence angle is set to 45°.

### Claim 2 (depends on 1)

The toner according to claim 1, wherein
the toner has a number-basis median diameter D50 of from 3.0 μm to 6.0 μm; and
a span value of the toner obtained in accordance with expression (2) below is from 0.20 to 0.80:
Span value=(D90−D10)/D50 (2)
where D90 is a particle diameter of the toner at which a cumulative number of particles in increasing order of particle diameter is 90%, and D10 is a particle diameter of the toner at which a cumulative number of particles in increasing order of particle diameter is 10%.

### Claim 3 (depends on 1)

The toner according to claim 1, wherein As, Bs, Al and Bl satisfy expression (1′) below:
1.50≤(As/Bs)/(Al/Bl)≤2.00 (1′).

### Claim 4 (depends on 1)

The toner according to claim 1, wherein a content ratio of the vinyl polymer in the polyolefin resin having —COOM is from 80 mass % to 95 mass %.

### Claim 5 (depends on 1)

The toner according to claim 1, wherein the metal ion M is Li+.

### Claim 6 (depends on 1)

The toner according to claim 1, wherein a content ratio of the monomer unit containing —COOM in the polyolefin resin having —COOM is from 6 mass % to 20 mass %.

### Claim 7 (depends on 1)

The toner according to claim 1, wherein the vinyl polymer has a structure derived from a cycloalkyl (meth)acrylate.

### Claim 8 (depends on 1)

The toner according to claim 1, wherein an absolute value σs of an average value of surface charge density of the second group and an absolute value σl of an average value of surface charge density of the first group satisfy expression (3) below:
1.05≤σs/σl≤1.50 (3).

### Claim 9 (depends on 1)

The toner according to claim 1, wherein the monomer unit containing —COOM is represented by formula (C) below:
wherein X is a hydrogen atom or —COOM; Y is —(CH2)m—COOM, where m is an integer from 0 to 3; and Z is a hydrogen atom, a C1 to C3 alkyl group, or —COOM.

### Claim 10 (depends on 1)

A method of producing the toner according to claim 1, the method comprising the steps of:
obtaining a kneaded product by melt-kneading a resin composition containing the polyolefin resin having —COOM and the binder resin including the polyester resin;
obtaining a cooled product by cooling the kneaded product;
obtaining a toner particle by pulverizing the cooled product; and
subjecting the toner particle to a thermal treatment by a hot air current, wherein the hot air current has a temperature of 110° C. or higher.