# US 2021/0063504 A1 · Magnetic Sensor Array with Dual TMR Film

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0063504 A1
- Document ID: US20210063504A1
- Status: Published application
- Kind: A1
- Application number: 16/718,667
- Filed: 2019-12-18
- Published: 2021-03-04
- Earliest claimed: 2019-08-27
- Assignees: Western Digital Technologies, Inc.
- Applicants: Western Digital Technologies, Inc.
- Inventors: Yuankai ZHENG; Christian KAISER; Zhitao DIAO; Chih-Ching HU; Chen-Jung CHIEN; Yung-Hung WANG; Dujiang WAN; Ronghui ZHOU; Ming MAO; Ming JIANG; Daniele MAURI
- Web page: https://patentgrep.com/patent/US20210063504A1

## CPC

- G01R 33/098: {comprising tunnel junctions, e.g. tunnel magnetoresistance sensors}
- G01R 33/0052: {Manufacturing aspects; Manufacturing of single devices, i.e. of semiconductor magnetic sensor chips (devices based on galvano-magnetic effect or the like H10N50/85)}
- H01F 10/3254: {the spacer being semiconducting or insulating, e.g. for spin tunnel junction [STJ]}
- H01F 10/3272: {by use of anti-parallel coupled [APC] ferromagnetic layers, e.g. artificial ferrimagnets [AFI], artificial [AAF] or synthetic [SAF] anti-ferromagnets}
- H01F 41/302: {for applying spin-exchange-coupled multilayers, e.g. nanostructured superlattices (spin-exchange-coupled multilayers H01F10/32)}
- H10B 61/00: Magnetic memory devices, e.g. magnetoresistive RAM [MRAM] devices
- H10N 50/01: Manufacture or treatment
- H10N 50/10: Magnetoresistive devices
- H10N 50/85: Materials of the active region
- H10N 59/00: Integrated devices, or assemblies of multiple devices, comprising at least one galvanomagnetic or Hall-effect element covered by groups H10N50/00 - H10N52/00 (MRAM devices H10B61/00)
- G01R: MEASURING ELECTRIC VARIABLES; MEASURING MAGNETIC VARIABLES (indicating correct tuning of resonant circuits H03J3/12)
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES
- H10B: ELECTRONIC MEMORY DEVICES
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR

## Abstract

A tunneling magnetoresistance (TMR) sensor device is disclosed that includes one or more TMR sensors. The TMR sensor device comprises a first resistor comprising a first TMR film, a second resistor comprising a second TMR film different than the first TMR film, a third resistor comprising the second TMR film, and a fourth resistor comprising the first TMR film. The first TMR film comprises a reference layer having a first magnetization direction anti-parallel to a second magnetization direction of a pinned layer. The second TMR film comprises a reference layer having a first magnetization direction parallel to a second magnetization direction of a first pinned layer, and a second pinned layer having a third magnetization direction anti-parallel to the first magnetization direction of the reference layer and the second magnetization direction of the first pinned layer.

## Claims

### Claim 1

A tunneling magnetoresistance (TMR) sensor device, comprising:
at least one TMR sensor comprising a first TMR film, the first TMR film comprising a first reference layer having a first magnetization direction and a first pinned layer having a second magnetization direction, the first magnetization direction of the first reference layer being anti-parallel to the second magnetization direction of the first pinned layer,
wherein the first pinned layer comprises a Co/CoFe/Co multi-layer stack having a thickness between about 20 Angstroms and about 30 Angstroms, and
wherein the first reference layer comprises a CoFe/Ta/CoFeB/CoFe multilayer stack having a thickness between about 21 Angstroms and about 37 Angstroms; and
at least one TMR sensor comprising a second TMR film, the second TMR film comprising a second reference layer having a third magnetization direction, a second pinned layer having the third magnetization direction, and a third pinned layer having a fourth magnetization direction, the third magnetization direction of the second reference layer and the second pinned layer being anti-parallel to the fourth magnetization direction of the third pinned layer,
wherein the second pinned layer comprises a Co/CoFe/Co multi-layer stack having a thickness between about 20 Angstroms and about 30 Angstroms,
wherein the third pinned layer comprises a Co/CoFe/Co multi-layer stack having a thickness between about 35 Angstroms and about 55 Angstroms, and
wherein the second reference layer comprises a CoFe/Ta/CoFeB/CoFe multilayer stack having a thickness between about 21 Angstroms and about 37 Angstroms.

### Claim 2 (depends on 1)

The TMR sensor device of claim 1, wherein the at least one TMR sensor comprised of the first TMR film comprises a first TMR sensor and a fourth TMR sensor, and wherein the at least one TMR sensor comprised of the second TMR film comprises a second TMR sensor and a third TMR sensor.

### Claim 3 (depends on 2)

The TMR sensor device of claim 2, wherein the first TMR sensor is adjacent to the second TMR sensor and the third TMR sensor, the second TMR sensor is adjacent to the first TMR sensor and the fourth TMR sensor, the third TMR sensor is adjacent to the first TMR sensor and the fourth TMR sensor, and the fourth TMR sensor is adjacent to the second TMR sensor and the third TMR sensor.

### Claim 4 (depends on 1)

The TMR sensor device of claim 1, wherein the first TMR film further comprises a first free layer, a first barrier layer, a first spacer layer, a first antiferromagnetic layer, and a first seed layer, and wherein the first barrier layer is disposed between the first reference layer and the first free layer, the first spacer layer is disposed between the first reference layer and the first pinned layer, and the first antiferromagnetic layer is disposed between the first pinned layer and the first seed layer.

### Claim 5 (depends on 1)

The TMR sensor device of claim 1, wherein the second TMR film further comprises a second free layer, a second barrier layer, a second spacer layer, a third spacer layer, a second antiferromagnetic layer, and a second seed layer, and
wherein the second barrier layer is disposed between the second reference layer and the second free layer, the second spacer layer is disposed between the second reference layer and the third pinned layer, the third spacer layer is disposed between the third pinned layer and the second pinned layer, and the second antiferromagnetic layer is disposed between the second pinned layer and the second seed layer.

### Claim 6 (depends on 5)

The TMR sensor device of claim 5, wherein the first TMR film has a total thickness of about 120 Angstroms to about 630 Angstroms, and wherein the second TMR film has a total thickness of about 155 Angstroms to about 1,675 Angstroms.

### Claim 7 (depends on 1)

The TMR sensor device of claim 1, wherein a Co composition in CoFe of the Co/CoFe/Co multilayer stack of the first pinned layer is between about 25% and 70%, wherein a B composition in CoFeB of the CoFe/Ta/CoFeB/CoFe multilayer stack of the first reference layer is between about 15% and 25%, wherein a Co composition in CoFe of the Co/CoFe/Co multilayer stack of the second pinned layer is between about 25% and 70%, and wherein a Co composition in CoFe of the Co/CoFe/Co multilayer stack of the third pinned layer is between about 25% and 70%.

### Claim 8

A TMR sensor device, comprising:
a first resistor comprising a first TMR film, the first TMR film comprising a first reference layer having a first magnetization direction, wherein the first reference layer comprises a CoFe/Ta/CoFeB/CoFe multilayer stack having a thickness between about 21 Angstroms and about 37 Angstroms;
a second resistor comprising a second TMR film, the second TMR film comprising a second reference layer having a second magnetization direction, wherein the second reference layer comprises a CoFe/Ta/CoFeB/CoFe multilayer stack having a thickness between about 21 Angstroms and about 37 Angstroms, and wherein the first magnetization direction of the first reference layer of the first TMR film is anti-parallel to the second magnetization of the second reference layer of the second TMR film;
a third resistor comprising the second TMR film; and
a fourth resistor comprising the first TMR film.

### Claim 9 (depends on 8)

The TMR sensor device of claim 8, wherein the first TMR film further comprises a first free layer, a first barrier layer, a first spacer layer, a first pinned layer, a first antiferromagnetic layer, and a first seed layer,
wherein the first barrier layer is disposed between the first reference layer and the first free layer, the first spacer layer is disposed between the first reference layer and the first pinned layer, and the first antiferromagnetic layer is disposed between the first pinned layer and the first seed layer,
wherein the second TMR film further comprises a second free layer, a second barrier layer, a second spacer layer, a second pinned layer, a third spacer layer, a third pinned layer, a second antiferromagnetic layer, and a second seed layer, and
wherein the second barrier layer is disposed between the second reference layer and the second free layer, the second spacer layer is disposed between the second reference layer and the third pinned layer, the third spacer layer is disposed between the third pinned layer and the second pinned layer, and the second antiferromagnetic layer is disposed between the second pinned layer and the second seed layer.

### Claim 10 (depends on 9)

The TMR sensor device of claim 9, wherein the third pinned layer of the second TMR film has a third magnetization direction parallel to the first magnetization direction of the first reference layer of the first TMR film.

### Claim 11 (depends on 9)

The TMR sensor device of claim 9, wherein the first free layer of the first TMR film has a fourth magnetization direction parallel to a fifth magnetization direction of the second free layer of the second TMR film.

### Claim 12 (depends on 11)

The TMR sensor device of claim 11, wherein the fourth magnetization of the first free layer of the first TMR film is parallel to a sixth magnetization direction of the first pinned layer of the first TMR film.

### Claim 13 (depends on 9)

The TMR sensor device of claim 9, wherein the first pinned layer of the first TMR film comprises a Co/CoFe/Co multi-layer stack having a thickness between about 20 Angstroms and about 30 Angstroms, wherein the second pinned layer of the second TMR film comprises a Co/CoFe/Co multi-layer stack having a thickness between about 20 Angstroms and about 30 Angstroms, and wherein the third pinned layer of the second TMR film comprises a Co/CoFe/Co multi-layer stack having a thickness between about 35 Angstroms and about 55 Angstroms.

### Claim 14 (depends on 13)

The TMR sensor device of claim 13, wherein the first TMR film has a total thickness of about 120 Angstroms to about 630 Angstroms, and wherein the second TMR film has a total thickness of about 155 Angstroms to about 1,675 Angstroms.

### Claim 15

A method of fabricating a TMR sensor device having a first resistor, a second resistor, a third resistor, and a fourth resistor, comprising:
forming a first TMR film by:
depositing a first seed layer,
depositing a first antiferromagnetic layer on the first seed layer,
depositing a first pinned layer on the first antiferromagnetic layer, the first pinned layer comprising a Co/CoFe/Co multi-layer stack having a thickness between about 20 Angstroms and about 30 Angstroms,
depositing a first spacer layer on the first pinned layer,
depositing a first reference layer on the first spacer layer, the first reference layer comprising a CoFe/Ta/CoFeB/CoFe multilayer stack having a thickness between about 21 Angstroms and about 37 Angstroms,
depositing a first barrier layer on the first reference layer, and
depositing a first free layer on the first barrier layer;
magnetically annealing the first TMR film to change a first magnetization direction of the first reference layer to be anti-parallel to a second magnetization direction of the first pinned layer;
forming a second TMR film by:
depositing a second seed layer,
depositing a second antiferromagnetic layer on the second seed layer,
depositing a second pinned layer on the second antiferromagnetic layer, the second pinned layer comprising a Co/CoFe/Co multi-layer stack having a thickness between about 20 Angstroms and about 30 Angstroms,
depositing a second spacer layer on the second pinned layer,
depositing a third pinned layer on the second spacer layer, the third pinned layer comprising a Co/CoFe/Co multi-layer stack having a thickness between about 35 Angstroms and about 55 Angstroms,
depositing a third spacer layer on the third pinned layer,
depositing a second reference layer on the third spacer layer, the second reference layer comprising a CoFe/Ta/CoFeB/CoFe multilayer stack having a thickness between about 21 Angstroms and about 37 Angstroms,
depositing a second barrier layer on the second reference layer, and
depositing a second free layer on the second barrier layer;
magnetically annealing the second TMR film to change a third magnetization direction of the third pinned layer to be anti-parallel to a fourth magnetization direction of the second reference layer, wherein the first magnetization direction of the first reference layer of the first TMR film is anti-parallel to the fourth magnetization direction of the second reference layer of the second TMR film;
forming the first resistor and the fourth resistor from the first TMR film; and
forming the second resistor and the third resistor from the second TMR film, wherein the first resistor is adjacent to the second resistor and the third resistor, the second resistor is adjacent to the first resistor and the fourth resistor, the third resistor is adjacent to the first resistor and the fourth resistor, and the fourth resistor is adjacent to the second resistor and the third resistor.

### Claim 16 (depends on 15)

The method of claim 15, wherein the first TMR film and the second TMR film are magnetically annealed in a magnetic oven at a temperature between about 250 degrees Celsius and about 300 degrees Celsius under a magnetic field of between about 1 Tesla to about 5 Tesla.

### Claim 17 (depends on 15)

The method of claim 15, wherein forming the first resistor and the fourth resistor from the first TMR film comprises depositing the first TMR film over a first bottom lead and a second bottom lead, and forming a first top lead over the first bottom lead and a second top lead over the second bottom lead.

### Claim 18 (depends on 15)

The method of claim 15, wherein forming the second resistor and the third resistor from the second TMR film comprises depositing the second TMR film over a third bottom lead and a fourth bottom lead, and forming a third top lead over the third bottom lead and a fourth top lead over the fourth bottom lead.

### Claim 19 (depends on 15)

The method of claim 15, wherein the first TMR film has a total thickness of about 120 Angstroms to about 630 Angstroms, and wherein the second TMR film has a total thickness of about 155 Angstroms to about 1,675 Angstroms.

### Claim 20 (depends on 15)

The method of claim 15, wherein the first, second, third, and fourth resistors are TMR sensors.