# US 2021/0062380 A1 · Plant-based functional polypropylene spunbond non-woven fabric and preparation method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0062380 A1
- Document ID: US20210062380A1
- Status: Published application
- Kind: A1
- Application number: 17/009,015
- Filed: 2020-09-01
- Published: 2021-03-04
- Earliest claimed: 2019-09-02
- Assignees: Bestee Material (Tsingtao) Co., Ltd.
- Applicants: Bestee Material (Tsingtao) Co., Ltd.
- Inventors: Xiaohua HUANG; Xiaoqian HUANG; Yu LIU; Jie LIU; Xiaolong HUANG; Li ZHEN
- Web page: https://patentgrep.com/patent/US20210062380A1

## CPC

- D04H 3/16: with bonds between thermoplastic filaments produced in association with filament formation, e.g. immediately following extrusion
- C08J 3/226: {using a polymer as a carrier}
- D01F 1/10: Other agents for modifying properties
- D01F 6/06: from polypropylene
- D01F 6/46: of polyolefins
- D04H 3/007: Addition polymers
- C08J 2323/12: Polypropene
- C08J 2423/12: Polypropene
- D04H: MAKING TEXTILE FABRICS, e.g. FROM FIBRES OR FILAMENTARY MATERIAL (weaving D03; knitting D04B; braiding D04C; net-making D04G; sewing D05B; tufting D05C; finishing non-woven fabrics D06); FABRICS MADE BY SUCH PROCESSES OR APPARATUS, e.g. FELTS, NON-WOVEN FABRICS; COTTON-WOOL; WADDING {; NON-WOVEN FABRICS FROM STAPLE FIBRES, FILAMENTS OR YARNS, BONDED WITH AT LEAST ONE WEB-LIKE MATERIAL DURING THEIR CONSOLIDATION}(non-woven fabrics having an intermediate or external layer of a different kind, e.g. of woven fabric, B32B)
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- D01F: CHEMICAL FEATURES IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS, THREADS, FIBRES, BRISTLES OR RIBBONS; APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OF CARBON FILAMENTS

## Abstract

A plant-based functional polypropylene spunbond non-woven fabric and a preparation method of the plant-based functional polypropylene spunbond non-woven fabric are provided. The plant-based functional polypropylene spunbond non-woven fabric contains a plant herb water-soluble extract in a weight percentage range of approximately 0.2%-1.5%. The plant-based functional polypropylene spunbond non-woven fabric has moisture regain in a range of approximately 0.2%-3%, a longitudinal breaking strength of approximately ≥18.5 N/5 cm, a transverse breaking strength of approximately ≤9.5 N/5 cm, a thickness in a range of approximately 0.2 mm-0.5 mm, a weight per unit area in a range of approximately 20 g/m2-40 g/m2, and a fiber diameter in a range of approximately 10 μm-30 μm.

## Claims

### Claim 1

A plant-based functional polypropylene spunbond non-woven fabric, comprising:
a plant herb water-soluble extract in a weight percentage range of approximately 0.2%-1.5%.

### Claim 2 (depends on 1)

The plant-based functional polypropylene spunbond non-woven fabric according to claim 1, wherein:
moisture regain is in a range of approximately 0.2%-3%;
a longitudinal breaking strength is approximately ≥18.5 N/5 cm; and
a transverse breaking strength is approximately ≤9.5 N/5 cm.

### Claim 3 (depends on 1)

The plant-based functional polypropylene spunbond non-woven fabric according to claim 1, wherein:
a thickness is in a range of approximately 0.2 mm-0.5 mm,
a weight per unit area is in a range of approximately 20 g/m2-40 g/m2, and
a polypropylene fiber diameter is in a range of approximately 10 μm-30 μm.

### Claim 4 (depends on 1)

The plant-based functional polypropylene spunbond non-woven fabric according to claim 1, wherein:
the plant herb water-soluble extract includes a honeysuckle extract, a mint extract, a wormwood extract, an echinacea polyphenols extract, an apple extract, a rose extract, a grass coral extract, a raspberry extract, a mulberry extract, a cinnamon extract, a ginger extract, an angelica extract, or a combination thereof.

### Claim 5 (depends on 1)

The plant-based functional polypropylene spunbond non-woven fabric according to claim 1, further including:
a polypropylene resin, as a raw material;
antioxidants, including dihydrotanshinone I, epicatechin and glycerin for preventing the plant herb water-soluble extract from changing color at a high temperature; and
a modifier, including sodium-n-methyl-n-oleyl taurate and cocamidopropyl betaine for improving dispersibility of the plant herb water-soluble extract in the polypropylene resin.

### Claim 6

A preparation method of a plant-based functional polypropylene spunbond non-woven fabric, comprising:
preparing a modified plant-based functional polypropylene masterbatch, including:
melting a polypropylene resin,
adding antioxidants into the polypropylene resin, and
after adding the antioxidants, adding a modifier and a plant herb water-soluble extract into the polypropylene resin.

### Claim 7 (depends on 6)

The method according to claim 6, wherein:
a melting temperature is in a range of approximately 195° C.-220° C.;
after adding the antioxidants, the polypropylene resin is stirred at approximately 800 rad/min-1000 rad/min for approximately 10 minutes-15 minutes; and
when adding the modifier and the plant herb water-soluble extract, the polypropylene resin is stirred at a high speed for approximately 20 minutes-40 minutes and cooled to approximately 180° C.-190° C.

### Claim 8 (depends on 6)

The method according to claim 6, wherein:
the antioxidants include dihydrotanshinone I, epicatechin and glycerin.

### Claim 9 (depends on 6)

The method according to claim 6, wherein:
a mass ratio of dihydrotanshinone I, epicatechin, and glycerin is approximately (1-5):(1-3):(3-10).

### Claim 10 (depends on 6)

The method according to claim 6, wherein:
the modifier includes sodium-n-methyl-n-oleyl taurate and cocamidopropyl betaine, and
a mass ratio of sodium-n-methyl-n-oleyl taurate and cocamidopropyl betaine is approximately (0.1-0.5):(0.5-3).

### Claim 11 (depends on 6)

The method according to claim 6, further including:
mixing the modified plant-based functional polypropylene masterbatch with a polypropylene raw material to obtain a mixture, wherein a mass ratio of the plant herb water-soluble extract in the plant-based functional polypropylene masterbatch over the polypropylene raw material is in a range of approximately 0.2%-1.5%; and
preparing a spinning melt by melting the mixture.

### Claim 12 (depends on 11)

The method according to claim 11, further including:
a spinning process, including using a screw extruder, extruding the spinning melt from a spinning port in a spunbond manner, to prepare a polypropylene fiber bundle; and
a post-processing process, including pressure-rolling, hot-rolling, wherein:
a temperature of a roller is in a range of approximately 140° C.-165° C.,
a pressure is in a range of approximately 56 d/cm-70 d/cm, and
a temperature of the hot-rolling is in a range of approximately 160° C.-170° C.

### Claim 13 (depends on 12)

The method according to claim 12, wherein:
a diameter of the spinning port is in a range of approximately 10 μm-30 μm.

### Claim 14 (depends on 12)

The method according to claim 12, further including:
an oiling process, wherein an oil includes polyvinylpyrrolidone and emulsified silicone oil, and a mass ratio of the polyvinylpyrrolidone and the emulsified silicone oil is in a range of approximately (1-3):(3-9).

### Claim 15 (depends on 6)

The method according to claim 6, wherein:
the plant herb water-soluble extract includes a honeysuckle extract, a mint extract, a wormwood extract, an echinacea polyphenols extract, an apple extract, a rose extract, a grass coral extract, a raspberry extract, a mulberry extract, a cinnamon extract, a ginger extract, an angelica extract, or a combination thereof.

### Claim 16 (depends on 6)

The method according to claim 6, wherein:
a mass ratio of the modifier and the plant herb water-soluble extract is in a range of approximately (0.1-0.5):(8-10).

### Claim 17 (depends on 6)

The method according to claim 6, further including:
a hot rolling with a pattern roller, wherein a temperature of the hot rolling is in a range of approximately approximately 160° C.-168° C.

### Claim 18 (depends on 6)

The method according to claim 6, wherein the plant-based functional polypropylene spunbond non-woven fabric has:
moisture regain in a range of approximately 0.2%-3%;
a longitudinal breaking strength of approximately ≥18.5 N/5 cm; and
a transverse breaking strength of approximately ≤9.5 N/5 cm.

### Claim 19 (depends on 6)

The method according to claim 6, wherein the plant-based functional polypropylene spunbond non-woven fabric has:
a thickness in a range of approximately 0.2 mm-0.5 mm,
a weight per unit area in a range of approximately 20 g/m2-40 g/m2, and
a polypropylene fiber diameter in a range of approximately 10 μm-30 μm.

### Claim 20 (depends on 6)

A plant-based functional polypropylene spunbond non-woven fabric, prepared by the method according to claim 6.