# US 2021/0062333 A1 · Moissanite ornament and method for coating diamond film on surface of moissanite ornament

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0062333 A1
- Document ID: US20210062333A1
- Status: Published application
- Kind: A1
- Application number: 16/559,636
- Filed: 2019-09-04
- Published: 2021-03-04
- Earliest claimed: 2019-09-04
- Assignees: Aaa Gems Co., Limited
- Applicants: Aaa Gems Co., Limited
- Inventors: Jinxin HE; Fanxiu LV; Lifu HEI
- Web page: https://patentgrep.com/patent/US20210062333A1

## CPC

- C23C 16/276: {using plasma jets}
- C23C 16/0227: {by cleaning or etching}
- C23C 16/0254: {Physical treatment to alter the texture of the surface, e.g. scratching or polishing}
- C23C 16/272: {using DC, AC or RF discharges}
- C23C 16/274: {using microwave discharges}
- C23C 16/4583: {the substrate being supported substantially horizontally}
- C23C 16/50: using electric discharges {(generation and control of plasma in discharge tubes for surface treatment H01J37/32, H01J37/34)}
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

A moissanite ornament, wherein the surface of the moissanite is coated with a diamond film. A method for coating a diamond film on a surface of a moissanite, including: Step 1: performing ultrasonic grinding pretreatment on the moissanite ornament in the nano-diamond powder suspension; Step 2: taking the moissanite ornament out from the nano-diamond powder suspension, and washing clean; Step 3: pressing the moissanite ornament into a preset shape-preserving sample platform to maintain; Step 4: placing, the moissanite ornament together with the shape-preserving sample platform into a diamond film deposition furnace to perform a plasma treatment; Step 5: introducing methane to conduct in-situ diamond film deposition. The moissanite coated with the diamond film on the surface provided by the present disclosure can greatly improve the surface hardness while maintaining the optical properties of the moissanite, thereby improving the scratch resistance performance of the moissanite.

## Claims

### Claim 1

A moissanite ornament, comprising a surface of the moissanite ornament is coated with a diamond film, and Mohs hardness scale of the moissanite jewelry is 9.9 to 10.00.

### Claim 2 (depends on 1)

The moissanite ornament according to claim 1, wherein the diamond film has an average grain size from 100 nm to 200 nm.

### Claim 3

A method for coating a diamond film on a surface of a moissanite ornament, comprising
Step 1: performing ultrasonic grinding pretreatment on the moissanite ornament in the in a nano-diamond powder suspension;
Step 2: taking the moissanite ornament out from the nano-diamond powder suspension, and washing clean;
Step 3: pressing the moissanite ornament into a preset shape-preserving sample platform to maintain;
Step 4: placing the moissanite ornament together with the shape-preserving sample platform into a diamond film deposition furnace to perform a plasma treatment;
Step 5: introducing methane to conduct in-situ diamond film deposition;
wherein the ultrasonic grinding pretreatment time is from 2 h to 6 h; a material of the shape-preserving sample platform in step 3 is pure copper; and
the plasma treatment in step 4 employs direct current arc plasma jet or microwave plasma jet to remove an influence of organic roots on deposition of diamond film, in which the organic roots is derived from the nano-diamond powder suspension on the surface of moissanite ornament.

### Claim 4 (depends on 3)

The method for plating a diamond film on a surface of a moissanite ornament according to claim 3, wherein nano-diamond powders in the nano-diamond powder suspension in the step 1 has a particle size of 5 nm to 200 nm, a concentration of the nano-diamond powder in the nano-diamond powder suspension is from 5% to 20%.

### Claim 5

(canceled)

### Claim 6

(canceled)

### Claim 7 (depends on 3)

The method for coating a diamond film on a surface of a moissanite ornament according to claim 3, wherein the shape-preserving sample platform is provided with a recess for maintaining a moissanite ornament, and a pressure to press the moissanite ornament into the recess is 50 Kgf to 250 Kgf in step 3.

### Claim 8

(canceled)

### Claim 9 (depends on 3)

The method for coating a diamond film on a surface of a moissanite ornament according to claim 3, wherein a temperature of the plasma treatment is from 700° C. to 1000° C. and the plasma treatment time is 5 min to 30 min.

### Claim 10 (depends on 3)

The method for coating a diamond film on a surface of a moissanite ornament according to claim 3, wherein a concentration of the methane in step 5 is from 0.5% to 10%, a pressure of the diamond film deposition furnace is 3 kPa to 20 kPa, and a deposition time is 5 min to 120 min.