# US 2021/0062330 A1 · Selective cobalt deposition on copper surfaces

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0062330 A1
- Document ID: US20210062330A1
- Status: Published application
- Kind: A1
- Application number: 17/002,296
- Filed: 2020-08-25
- Published: 2021-03-04
- Earliest claimed: 2019-08-30
- Assignees: Applied Materials, Inc.
- Applicants: Applied Materials, Inc.
- Inventors: Wenjing XU; Yufei HU; Gang SHEN; Feng CHEN
- Web page: https://patentgrep.com/patent/US20210062330A1

## CPC

- C23C 16/04: Coating on selected surface areas, e.g. using masks
- C23C 16/06: characterised by the deposition of metallic material
- C23C 16/16: from metal carbonyl compounds
- C23C 16/18: from metallo-organic compounds
- C23C 16/45502: {Flow conditions in reaction chamber}
- C23C 16/52: Controlling or regulating the coating process {(C23C16/45557, C23C16/279 take precedence)}
- C23C 16/56: After-treatment
- H10P 14/432: {using selective deposition}
- H10W 20/037: {the barrier, adhesion or liner layers being on top of a main fill metal}
- H10W 20/425: {Barrier, adhesion or liner layers}
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A method for capping a copper surface on a substrate. In embodiments, the methods include exposing a substrate including a copper surface and a dielectric surface to a cobalt precursor gas and a process gas including a reducing agent to selectively form a first cobalt capping layer over the copper surface while leaving exposed the dielectric surface during a vapor deposition process, wherein a flow rate ratio of process gas to cobalt precursor gas is at least 300:1.

## Claims

### Claim 1

A method for capping a copper surface on a substrate, comprising:
exposing a substrate comprising a copper surface and a dielectric surface to a cobalt precursor gas and a process gas comprising a reducing agent to selectively form a first cobalt capping layer over the copper surface while leaving exposed the dielectric surface during a vapor deposition process, wherein a flow rate ratio of process gas to cobalt precursor gas is at least 300:1.

### Claim 2 (depends on 1)

The method of claim 1, wherein the process gas comprising a reducing agent is flowed into a process chamber at a rate of at least 8000 sccm.

### Claim 3 (depends on 1)

The method of claim 1, wherein the process gas further comprises ammonia (NH3) gas at a flow rate of at least 500 sccm.

### Claim 4 (depends on 1)

The method of claim 1, wherein the cobalt precursor gas is flowed into a process chamber process chamber at a rate of about 10 to about 30 sccm.

### Claim 5 (depends on 1)

The method of claim 1, wherein the process gas comprises hydrogen (H2), ammonia (NH3), and combinations thereof.

### Claim 6 (depends on 1)

The method of claim 1, wherein cobalt precursor gas is flowed into a process chamber at a rate of about 10 to about 30 sccm, and wherein the process gas comprises hydrogen (H2) flowed into the process chamber at a rate of at least 8000 sccm, and ammonia (NH3) flowed into the process chamber at a rate of at least 500 sccm.

### Claim 7 (depends on 1)

The method of claim 1, further comprising igniting an ammonia plasma after selectively forming the first cobalt capping layer.

### Claim 8 (depends on 1)

The method of claim 1, wherein exposing a substrate comprising a copper surface and a dielectric surface to a gaseous reducing agent and a cobalt precursor gas is performed for a time period of about 3 seconds to about 15 seconds.

### Claim 9 (depends on 1)

The method of claim 1, wherein exposing a substrate comprising a copper surface and a dielectric surface to a gaseous reducing agent and a cobalt precursor gas is performed at a temperature of about 200° C. to about 250° C.

### Claim 10 (depends on 1)

The method of claim 1, further comprising exposing the first cobalt capping layer to a second cobalt precursor gas and a second process gas comprising a reducing agent to deposit a second cobalt capping layer atop the first cobalt capping layer.

### Claim 11 (depends on 10)

The method of claim 10, wherein a deposition cycle comprises performing a vapor deposition process 2 or more times to deposit a plurality of cobalt capping layers.

### Claim 12 (depends on 1, 10)

The method of claim 10, wherein each of a plurality of cobalt capping layers is deposited to a thickness of about 3 angstroms to about 5 angstroms. 13, The method of claim 1, wherein the cobalt precursor gas comprises a cobalt precursor which has a general chemical formula (CO)x.COyLz, wherein:
X is 1, 2, 3, 4, 5, 6, 7, 8, 9, 10, 11, or 12;
Y is 1, 2, 3, 4, or 5;
Z is 1, 2, 3, 4, 5, 6, 7, or 8; and
L is a ligand independently selected from the group consisting of cyclopentadienyl, alkylcyclopentadienyl, methylcyclopentadienyl, pentamethylcyclopentadienyl, pentadienyl, alkylpentadienyl, cyclobutadienyl, butadienyl, allyl, ethylene, propylene, alkenes, dialkenes, alkynes, nitrosyl, ammonia, derivatives thereof, and combinations thereof.

### Claim 14 (depends on 1)

The method of claim 1, wherein the cobalt precursor gas comprises a cobalt precursor selected from the group consisting of tricarbonyl allyl cobalt, cyclopentadienyl cobalt bis(carbonyl), methylcyclopentadienyl cobalt bis(carbonyl), ethylcyclopentadienyl cobalt bis(carbonyl), pentamethylcyclopentadienyl cobalt bis(carbonyl), dicobalt octa(carbonyl), nitrosyl cobalt tris(carbonyl), bis(cyclopentadienyl) cobalt, (cyclopentadienyl) cobalt (cyclohexadienyl), cyclopentadienyl cobalt (1,3-hexadienyl), (cyclobutadienyl) cobalt (cyclopentadienyl), bis(methylcyclopentadienyl) cobalt, (cyclopentadienyl) cobalt (5-methylcyclopentadienyl), bis(ethylene) cobalt (pentamethylcyclopentadienyl), derivatives thereof, complexes thereof, plasmas thereof, and combinations thereof.

### Claim 15 (depends on 1)

The method of claim 1, wherein the cobalt precursor gas comprises cyclopentadienyl cobalt bis(carbonyl).

### Claim 16

A method for capping a copper surface on a substrate, comprising:
positioning a substrate within a processing chamber, wherein the substrate comprises a copper surface and a dielectric surface; and
exposing the copper surface to a cobalt precursor gas and a process gas comprising a reducing agent to selectively form a first cobalt capping layer over the copper surface while leaving exposed the dielectric surface during a vapor deposition process, wherein a flow rate of the cobalt precursor gas is about 10 to about 30 sccm and a flow rate of the process gas includes hydrogen (H2) flowed into a process chamber at a rate of at least 8000 sccm.

### Claim 17 (depends on 16)

The method of claim 16, wherein the process gas further comprises ammonia (NH3) gas at a flow rate of at least 500 sccm.

### Claim 18

A non-transitory computer readable medium having instructions stored thereon that, when executed, cause a method of capping a copper surface on a substrate to be performed, the method comprising:
exposing a substrate comprising a copper surface and a dielectric surface to a cobalt precursor gas and a process gas comprising a reducing agent to selectively form a first cobalt capping layer over the copper surface while leaving exposed the dielectric surface during a vapor deposition process, wherein a flow rate ratio of process gas to cobalt precursor gas is at least 300:1.

### Claim 19 (depends on 18)

The non-transitory computer readable medium of claim 18, wherein the method further comprises flowing the cobalt precursor gas into a process chamber at a rate of about 10 to about 30 sccm, and wherein the process gas comprises hydrogen (H2) flowed into the process chamber at a rate of at least 8000 sccm.

### Claim 20 (depends on 18)

The non-transitory computer readable medium of claim 18, wherein the process gas further comprises ammonia (NH3) gas provided at a flow rate of at least 500 sccm.