# US 2021/0047709 A1 · Method for the recovery of zinc

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0047709 A1
- Document ID: US20210047709A1
- Status: Published application
- Kind: A1
- Application number: 17/042,261
- Filed: 2019-03-29
- Published: 2021-02-18
- Earliest claimed: 2018-03-30
- Assignees: Tata Steel Nederland Technology B.V.
- Applicants: Tata Steel Nederland Technology B.V.
- Inventors: Johannes HAGE; Hendrikus Koenraad Albertus MEIJER; Tim PEETERS
- Web page: https://patentgrep.com/patent/US20210047709A1

## CPC

- C21B 13/0026: {introduction of iron oxide in the flame of a burner or a hot gas stream}
- C22B 19/36: in blast or reverberatory furnaces
- C22B 19/08: in blast furnaces
- F27D 17/25: using cyclones
- Y02P 10/134: by avoiding CO2, e.g. using hydrogen
- C21B: MANUFACTURE OF IRON OR STEEL (preliminary treatment of ferrous ores or scrap C22B1/00)
- C22B: PRODUCTION AND REFINING OF METALS (electrolytic C25); PRETREATMENT OF RAW MATERIALS
- F27D: DETAILS OR ACCESSORIES OF FURNACES, KILNS, OVENS OR RETORTS, IN SO FAR AS THEY ARE OF KINDS OCCURRING IN MORE THAN ONE KIND OF FURNACE
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A method for the recovery of zinc from zinc containing materials using a smelting apparatus for smelting a metalliferous feed material, wherein the smelting apparatus includes a smelting vessel, a smelt cyclone mounted on the smelting vessel and in connection with the inside of the smelting vessel and an off-gas duct connected to the smelt cyclone, and wherein the method includes the steps of: injecting the feed material with a carrier gas into the smelt cyclone, injecting an oxygen containing gas into the smelt cyclone, injecting coal with a carrier gas into the smelting vessel, injecting an oxygen containing gas into the smelting vessel, optionally injecting fluxes with a carrier gas into the smelting vessel, wherein the zinc containing materials are injected into the smelt cyclone and/or into the smelting vessel.

## Claims

### Claim 1

A method for the recovery of zinc from zinc containing materials using a smelting apparatus for smelting a metalliferous feed material, wherein the smelting apparatus comprises a smelting vessel, a smelt cyclone mounted on the smelting vessel and in connection with the inside of the smelting vessel and an off-gas duct connected to the smelt cyclone, wherein the method comprises the steps of:
injecting the feed material with a carrier gas into the smelt cyclone,
injecting an oxygen containing gas into the smelt cyclone,
injecting coal with a carrier gas into the smelting vessel,
injecting an oxygen containing gas into the smelting vessel,
optionally injecting fluxes with a carrier gas into the smelting vessel,
wherein the zinc containing materials are injected into the smelt cyclone and/or into the smelting vessel.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the zinc containing materials injected into the smelting vessel are injected above and/or in a slag layer on the liquid feed material in the smelting vessel.

### Claim 3 (depends on 2)

The method according to claim 2, wherein the zinc containing materials injected into the smelting vessel are injected at a first and/or a second level wherein the first level is between the smelt cyclone and the slag layer on the liquid metal in the smelting vessel and wherein the injection at the second level is carried out through a supply lance into the slag layer.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the particle size of the zinc containing materials injected into the smelt cyclone are in a range of at most 2.0 mm.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the particle size of the zinc containing materials injected into the smelt vessel at the first level have a particle size of at most 15 cm.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the particle size of the zinc containing materials injected at the second level into the slag layer have a particle size of at most 50 μm.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the off-gas is guided through an inclined off-gas duct part downstream of the smelting vessel and the smelt cyclone.

### Claim 8 (depends on 1)

The method according to claim 1, wherein the off-gas is cooled/quenched in an upright off-gas duct part downstream of the inclined off-gas duct part.

### Claim 9 (depends on 8)

The method according to claim 8, wherein the off-gas is cooled/quenched to a temperature of ≤1200° C.

### Claim 10 (depends on 1)

The method according to claim 1, wherein the off-gas is passed through a cooling tower followed by a cold dust cyclone.

### Claim 11 (depends on 1)

The method according to claim 1, wherein the off-gas is passed through a high temperature dust cyclone.

### Claim 12 (depends on 1)

The method according to claim 1, wherein the off-gas is used to drive a steam driven electric generator.

### Claim 13 (depends on 1)

The method according to claim 1, wherein at least part of the zinc oxide containing dust recovered from the off-gas is injected into the smelting vessel.

### Claim 14 (depends on 1)

The method according to claim 1, wherein the off-gas from the smelting apparatus is controlled by controlling the amount of oxygen injected into the smelt cyclone and/or into the smelting vessel.

### Claim 15 (depends on 1)

The method according to claim 1, wherein the off-gas from the smelting apparatus is controlled by controlling the amount of oxygen injected into the process such that the conditions in the off-gas are oxidising.

### Claim 16 (depends on 1)

The method according to claim 1, wherein a controlled amount of oxygen is injected into the off-gas upstream of the inclined off-gas duct part.

### Claim 17 (depends on 1)

The method according to claim 1, wherein the particle size of the zinc containing materials injected into the smelt cyclone are in a range of at most 1.5 mm.

### Claim 18 (depends on 1)

The method according to claim 1, wherein the particle size of the zinc containing materials injected into the smelt cyclone are in a range of at most 1.0 mm.

### Claim 19 (depends on 1)

The method according to claim 1, wherein the particle size of the zinc containing materials injected into the smelt vessel at the first level have a particle size of at most 10 cm.

### Claim 20 (depends on 1)

The method according to claim 1, wherein the particle size of the zinc containing materials injected into the smelt vessel at the first level have a particle size of at most 5 cm.

### Claim 21 (depends on 1)

The method according to claim 1, wherein the particle size of the zinc containing materials injected at the second level into the slag layer have a particle size of at most 30 μm.

### Claim 22 (depends on 1)

The method according to claim 1, wherein the particle size of the zinc containing materials injected at the second level into the slag layer have a particle size of at most 20 μm.

### Claim 23 (depends on 8)

The method according to claim 8, wherein the off-gas is cooled/quenched to a temperature of ≤1050° C.

### Claim 24 (depends on 8)

The method according to claim 8, wherein the off-gas is cooled/quenched to a temperature of ≤900° C.