# US 2021/0039982 A1 · Hot-formed, chemically prestressable glass articles with a low proportion of crystals and methods and devices for producing

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0039982 A1
- Document ID: US20210039982A1
- Status: Published application
- Kind: A1
- Application number: 16/986,196
- Filed: 2020-08-05
- Published: 2021-02-11
- Earliest claimed: 2019-08-05
- Assignees: Schott AG
- Applicants: Schott AG
- Inventors: Thomas Schmiady; Thomas Seuthe; Jörg Hessenkemper; Sebastian Leukel; Susanne Krüger
- Web page: https://patentgrep.com/patent/US20210039982A1

## CPC

- C03C 3/097: containing phosphorus, niobium or tantalum
- C03B 17/064: {by the overflow downdraw fusion process; Isopipes therefor}
- C03B 18/06: using mechanical means, e.g. restrictor bars, edge rollers
- C03B 18/16: Construction of the float tank; Use of material for the float tank; Coating or protection of the tank wall
- C03B 18/18: Controlling or regulating the temperature of the float bath; Composition or purification of the float bath
- C03B 25/08: of glass sheets
- C03C 3/083: containing aluminium oxide or an iron compound
- C03C 3/085: containing an oxide of a divalent metal
- C03C 3/087: containing calcium oxide, e.g. common sheet or container glass
- C03C 3/091: containing aluminium
- C03C 3/093: containing zinc or zirconium
- C03C 21/002: {to perform ion-exchange between alkali ions (C03C21/005 takes precedence)}
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES

## Abstract

A hot-formed, chemically prestressable glass article having a low percentage of crystals or crystallites, in particular a plate-shaped, chemically prestressable glass article, as well as to a method and a device for its production are provided. The glass article has a composition including the components SiO2, Al2O3, and Li2O and a content of seed formers (ZrO2, SnO2, and TiO2) of at least 0.8 wt %, as well as at most ten crystals, including crystallites, per kilogram of glass, which have a maximum diameter greater than 1 μm and up to at most 5 μm.

## Claims

### Claim 1

A chemically prestressable, hot-formed, plate-shaped glass article, comprising:
a composition comprising SiO2, Al2O3, and Li2O;
a content of ZrO2, SnO2, and TiO2 in a sum total of at least 0.8 wt %; and
at most ten crystals, including crystallites, per kilogram of glass, which have a maximum diameter greater than 1 μm and up to at most 5 μm.

### Claim 2 (depends on 1)

The glass article of claim 1, wherein the maximum diameter is up to at most 2 μm.

### Claim 3 (depends on 1)

The glass article of claim 1, further comprising a temperature with a maximum crystal growth rate Kgmax of 925° C. to 1100° C. and a maximum crystal growth rate of 2 μm/min to 16 μm/min at the temperature Kgmax.

### Claim 4 (depends on 1)

The glass article of claim 1, wherein the maximum crystal growth rate of is 5.9 μm/min to 6.4 μm/min.

### Claim 5 (depends on 1)

The glass article of claim 1, wherein the composition comprises, in wt %:
SiO2 57 to 69,
Al2O3 17 to 25,
B2O3 0 to 7,
Li2O 3 to 5.5,
Na2O 0.3 to 7, and
a sum of a content of Al2O3 and SiO2 between at least 75 and at most 92.

### Claim 6 (depends on 5)

The glass article of claim 5, wherein the composition comprises:
SiO2 61 to 67,
Al2O3 17 to 21,
B2O3 0 to 4.5,
Li2O 3.5 to 5,
Na2O 0.8 to 4.5,
K2O 0 to 1
MgO 0 to 2
CaO 0 to 4.5,
SrO 0 to 2,
ZnO 0 to 3
P2O5 0 to 3
ZrO2 0 to 3,
TiO2 0 to 3, and
SnO2 0 to 2.

### Claim 7 (depends on 6)

The glass article of claim 6, wherein the composition further comprises contaminants and/or refining agents and/or coloring constituents in amounts up to 2 wt %.

### Claim 8 (depends on 1)

The glass article of claim 1, further comprising a thickness that is at least 0.4 mm and at most 3 mm.

### Claim 9 (depends on 1)

The glass article of claim 1, further comprising a thickness that is at least 0.5 mm.

### Claim 10 (depends on 1)

The glass article of claim 1, further comprising a thickness that is at most 1 mm.

### Claim 11

A method for the production of a chemically prestressable, hot-formed, plate-shaped glass article, comprising:
providing a glass having a composition comprising SiO2, Al2O3, and Li2O; a content of ZrO2, SnO2, and TiO2 in a sum total of at least 0.8 wt %; and at most ten crystals, including crystallites, per kilogram of glass, which have a maximum diameter greater than 1 μm and up to at most 5 μm;
hot forming the glass to the plate-shaped glass article using a process selected from a group consisting of a float method, a down-draw method, and an overflow fusion method.

### Claim 12 (depends on 11)

The method of claim 11, wherein the process is a float method comprising:
heating of a lip tile or a spout region by heating units beneath the lip tile in a partial flow of the glass that flows opposite to a drawing direction Y and comes into contact with restrictor tiles; and
keeping a glass temperature above an upper devitrification temperature OEG of the glass.

### Claim 13 (depends on 12)

The method of claim 12, further comprising keeping a viscosity of the glass in a shear region at the restrictor tiles smaller than lg(η/dPas)=3.5.

### Claim 14 (depends on 12)

The method of claim 12, further comprising increasing a flow rate by constriction at the restrictor tiles and extension tiles.

### Claim 15 (depends on 12)

The method of claim 12, further comprising minimizing the entry of seeds from condensates from vaporized tin or glass constituents by an exchange of atmosphere at a distance of 0 m to 3 m behind a spout or lip tile in the drawing direction Y by more than fiftyfold/h of a nominal volume in comparison to an operation without exchange of atmosphere.

### Claim 16 (depends on 12)

The method of claim 12, further comprising adjusting a surface temperature of a knurl or top roller to reduce seed formation in the border region.

### Claim 17 (depends on 16)

The method of claim 16, further comprising removing adhesions, condensates or glass cakings at the top rollers or knurls.

### Claim 18 (depends on 11)

The method of claim 11, further comprising maintaining a cooling gradient of the glass in the shaping region of the float bath, within which the viscosity of the glass that is to be hot-formed is lg(η/dPas)=4 to 7.6, of at least 25 K/m to preferably at most 35 K/m.

### Claim 19 (depends on 11)

The method of claim 11, further comprising maintaining a cooling rate of the glass in the shaping region of 28 K/min +/−5 K/min.

### Claim 20

A device for the production of a chemically prestressable, hot-formed, plate-shaped glass article, comprising a heating unit arranged in a region of a lip tile or spout that directly adjoins the lip tile or spout and beneath the lip tile or spout.