# US 2021/0017080 A1 · Inorganic fiber toughened inorganic composite artificial stone panel and preparation method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2021/0017080 A1
- Document ID: US20210017080A1
- Status: Published application
- Kind: A1
- Application number: 16/933,429
- Filed: 2020-07-20
- Published: 2021-01-21
- Earliest claimed: 2019-07-19
- Assignees: Guangdong Topnice New Materials Technology Co., Ltd.
- Applicants: GuangDong TopNice New Materials Technology CO., LTD.
- Inventors: Fucai LIU; Min XIAO; Bin LI; Zengyong ZHENG; Heming HUANG
- Web page: https://patentgrep.com/patent/US20210017080A1

## CPC

- B32B 18/00: Layered products essentially comprising ceramics, e.g. refractory products
- C04B 28/04: Portland cements
- B28B 1/522: {for producing multi-layered articles (B28B1/526, B28B1/527 take precedence)}
- B28B 3/006: {Pressing by atmospheric pressure, as a result of vacuum generation or by gas or liquid pressure acting directly upon the material, e.g. jets of compressed air (moulds for treating with gases or degassing B28B7/44; compacting concrete by means of vacuum in general E04G21/061)}
- B28B 11/0845: {for smoothing}
- B28B 11/24: for curing, setting or hardening (processes for influencing or modifying the setting or hardening ability of mortars, concrete or artificial stone compositions, in general C04B40/00)
- C04B 14/06: Quartz; Sand
- C04B 14/068: {Specific natural sands, e.g. sea -, beach -, dune - or desert sand}
- C04B 14/386: {Carbon (carbon nanotubes C04B14/026)}
- C04B 14/42: Glass
- C04B 14/4625: {Alumina}
- C04B 14/4668: {of vulcanic origin}
- C04B 24/2623: {Polyvinylalcohols; Polyvinylacetates}
- C04B 24/2652: {Nitrogen containing polymers, e.g. polyacrylamides, polyacrylonitriles}
- C04B 40/0071: {making use of a rise in pressure}
- C04B 40/0082: {making use of a rise in temperature, e.g. caused by an exothermic reaction}
- C04B 40/0089: {making use of vacuum or reduced pressure}
- C04B 2103/302: {Water reducers}
- C04B 2111/00008: {Obtaining or using nanotechnology related materials}
- C04B 2111/00612: {as one or more layers of a layered structure}
- C04B 2111/542: {Artificial natural stone}
- C04B 2201/50: for the mechanical strength
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- B28B: SHAPING CLAY OR OTHER CERAMIC COMPOSITIONS; SHAPING SLAG; SHAPING MIXTURES CONTAINING CEMENTITIOUS MATERIAL, e.g. PLASTER (foundry moulding B22C; working stone or stone-like material B28D; shaping of substances in a plastic state, in general B29C; making layered products not composed wholly of these substances B32B)

## Abstract

An inorganic fiber toughened inorganic composite artificial stone panel and a preparation method thereof are disclosed. The panel includes a surface layer and a toughened base layer. The surface layer includes the the following components in parts by weight: 40-70 parts of quartz sand, 10-30 parts of quartz powder, 20-45 parts of inorganic active powder, 0.5-4 parts of pigment, 0.3-1 parts of water reducing agent and 3-10 parts of water. The toughened base layer includes the following components in parts by weight: 40-60 parts of inorganic active powder, 45-65 parts of sand, 0.8-1.5 parts of water reducing agent, 6-14 parts of water, 0.4-2 parts of inorganic fiber and 0.8-2.5 parts of toughener.

## Claims

### Claim 1

An inorganic fiber toughened inorganic composite artificial stone panel, comprising a surface layer and a toughened base layer,
wherein the surface layer includes materials having the following components in parts by weight: 40-70 parts of quartz sand, 10-30 parts of quartz powder, 20-45 parts of inorganic active powder, 0.5-4 parts of pigment, 0.3-1 parts of water reducing agent and 3-10 parts of water; and
wherein the toughened base layer includes materials having the following components in parts by weight: 40-60 parts of inorganic active powder, 45-65 parts of sand, 0.8-1.5 parts of water reducing agent, 6-14 parts of water, 0.4-2 parts of inorganic fiber and 0.8-2.5 parts of toughener.

### Claim 2 (depends on 1)

The inorganic fiber toughened inorganic composite artificial stone panel according to claim 1, wherein the inorganic active powder is mainly composed of pure white Portland cement doped with active powder, the pure white Portland cement has a strength grade of more than 42.5, and the active powder is at least one selected from the group consisting of white silicon powder, mineral powder, nano calcium oxide, nano silicon oxide, and sintered high white kaolin powder.

### Claim 3 (depends on 1)

The inorganic fiber toughened inorganic composite artificial stone panel according to claim 1, the quartz sand has a fineness modulus of 2.0-3.0, a content of silicon dioxide above 93%, and a hardness of a raw stone above 7.

### Claim 4 (depends on 1)

The inorganic fiber toughened inorganic composite artificial stone panel according to claim 1, the quartz powder has a fineness of 600 mesh or more, a content of silicon dioxide above 93%, and a hardness of a raw stone above 7.

### Claim 5 (depends on 1)

The inorganic fiber toughened inorganic composite artificial stone panel according to claim 1, wherein the sand is selected from one or more of river sand, manufactured sand and quartz sand.

### Claim 6 (depends on 1)

The inorganic fiber toughened inorganic composite artificial stone panel according to claim 1, wherein the inorganic fiber is selected from one or more of glass fiber, carbon fiber, basalt fiber, boron fiber, ceramic fiber and alumina fiber which have a diameter of 0.02-0.08 mm, a length of 6-12mm and a tensile strength of more than 1,000 MPa.

### Claim 7 (depends on 1)

The inorganic fiber toughened inorganic composite artificial stone panel according to claim 1, wherein the toughener is selected from one or more of polyvinyl alcohol glue and acrylamide glue.

### Claim 8 (depends on 1)

The inorganic fiber toughened inorganic composite artificial stone panel according to claim 1, wherein a total thickness of the panel is 15-50 mm, and a thickness of the surface layer is 4-6mm.

### Claim 9 (depends on 1)

A preparation method of the inorganic fiber toughened inorganic composite artificial stone panel according to claim 1, comprising the steps of:
S1, uniformly stirring and mixing first raw materials and second raw materials, respectively, according to the predetermined ratio to obtain a first mixed material and a second mixed material, wherein the first raw materials are used for the surface layer and second raw materials are used for the toughened base layer;
S2, preparing a panel mold, calculating and weighing the first mixed material prepared in step Si according to a thickness of the surface layer and uniformly arranging the first mixed material in the panel mold, then calculating and weighing the second mixed material prepared in step Si according to a thickness of the toughened base layer and uniformly arranging the second mixed material on the first mixed material in the panel mold;
S3, covering an isolated moisturizing film on the second mixed material in the panel mold of step S2, and then putting the panel mold into a vacuum compressor to concurrently perform a vacuum exhaust and a vibrating compression to obtain a compressed plate;
S4, curing the compressed plate obtained in step S3 at a temperature of 40° C. for 6 to 8 hours, then heating the compressed plate to 80-90° C. and curing the compressed plate at 80-90° C. for 12-16 hours, and obtaining a rough plate; and
S5, performing a bottom scraping, a thickening and a polishing on the rough plate obtained in step S4 after removing the isolation moisturizing film to obtain the inorganic fiber toughened inorganic composite artificial stone panel.

### Claim 10 (depends on 9)

The preparation method of the inorganic fiber toughened inorganic composite artificial stone panel according to claim 9, wherein in step S 1, time for stirring and mixing the first raw materials and second raw materials is not less than 10 minutes, respectively; Vebe consistency testing time of the first mixed material and the second mixed material is 5-30 seconds, respectively; and the initial setting time of the first mixed material and the second mixed material after the stirring and mixing is not less than 60 minutes.

### Claim 11 (depends on 9)

The preparation method of the inorganic fiber toughened inorganic composite artificial stone panel according to claim 9, wherein in step S3, time for the vacuum exhaust is not less than 60 seconds, time for the vibrating compression is not less than 120 seconds; and a vacuum pressure for the vacuum exhaust is -0.07-0.1 MPa, a pressure load of the vacuum compressor is not less than 1 MPa, and a pressure of the vacuum compressor is not less than 5000 kN.

### Claim 12 (depends on 9)

The preparation method of the inorganic fiber toughened inorganic composite artificial stone panel according to claim 9, wherein in step S4, a humidity is kept above 75% during the curing at 80-90° C.

### Claim 13 (depends on 9)

The preparation method of the inorganic fiber toughened inorganic composite artificial stone panel according to claim 9, wherein the inorganic active powder is mainly composed of pure white Portland cement doped with active powder, the pure white Portland cement has a strength grade of more than 42.5, and the active powder is at least one selected from the group consisting of white silicon powder, mineral powder, nano calcium oxide, nano silicon oxide, and sintered high white kaolin powder.

### Claim 14 (depends on 9)

The preparation method of the inorganic fiber toughened inorganic composite artificial stone panel according to claim 9, the quartz sand has a fineness modulus of 2.0-3.0, a content of silicon dioxide above 93%, and a hardness of a raw stone above 7.

### Claim 15 (depends on 9)

The preparation method of the inorganic fiber toughened inorganic composite artificial stone panel according to claim 9, the quartz powder has a fineness of 600 mesh or more, a content of silicon dioxide above 93%, and a hardness of a raw stone above 7.

### Claim 16 (depends on 9)

The preparation method of the inorganic fiber toughened inorganic composite artificial stone panel according to claim 9, wherein the sand is selected from one or more of river sand, manufactured sand and quartz sand.

### Claim 17 (depends on 9)

The preparation method of the inorganic fiber toughened inorganic composite artificial stone panel according to claim 9, the inorganic fiber is selected from one or more of glass fiber, carbon fiber, basalt fiber, boron fiber, ceramic fiber and alumina fiber which have a diameter of 0.02-0.08 mm, a length of 6-12mm and a tensile strength of more than 1,000 MPa.

### Claim 18 (depends on 9)

The preparation method of the inorganic fiber toughened inorganic composite artificial stone panel according to claim 9, wherein the toughener is selected from one or more of polyvinyl alcohol glue and acrylamide glue.

### Claim 19 (depends on 9)

The preparation method of the inorganic fiber toughened inorganic composite artificial stone panel according to claim 9, wherein a total thickness of the panel is 15-50 mm, and a thickness of the surface layer is 4-6 mm.
