# US 2020/0403269 A1 · Lithium solid electrolyte and method of manufacture thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0403269 A1
- Document ID: US20200403269A1
- Status: Published application
- Kind: A1
- Application number: 16/860,326
- Filed: 2020-04-28
- Published: 2020-12-24
- Earliest claimed: 2019-06-18
- Assignees: Samsung Electronics Co., Ltd.; Massachusetts Institute of Technology
- Applicants: Samsung Electronics Co., Ltd.; Massachusetts Institute of Technology
- Inventors: Yuntong Zhu; Won Seok Chang; Jennifer Rupp; Lincoln Miara
- Web page: https://patentgrep.com/patent/US20200403269A1

## CPC

- H01M 10/052: Li-accumulators
- H01M 10/0562: Solid materials
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 2004/027: {Negative electrodes}
- H01M 2004/028: {Positive electrodes}
- H01M 2300/0068: inorganic
- H01M 2300/0077: based on zirconium oxide
- Y02E 60/10: Energy storage using batteries
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A method of manufacturing a lithium solid electrolyte, the method including: providing a composition including a lithium precursor, a lanthanum precursor, and a zirconium precursor; disposing the composition on a substrate having a temperature of 270° C. to 500° C. to form a film; and heat-treating the film at 300° C. to less than 750° C. for 1 hour to 100 hours to manufacture the lithium solid electrolyte.

## Claims

### Claim 1

A method of manufacturing a lithium solid electrolyte, the method comprising:
providing a composition comprising a lithium precursor, a lanthanum precursor, and a zirconium precursor;
disposing the composition on a substrate having a temperature of 270° C. to 500° C. to form a film; and
heat-treating the film at 300° C. to less than 750° C. for 1 hour to 100 hours to manufacture the lithium solid electrolyte.

### Claim 2 (depends on 1)

The method of claim 1, wherein the composition further comprises a Ca precursor, a Mg precursor, an Al precursor, a Ga precursor, or a combination thereof.

### Claim 3 (depends on 1)

The method of claim 1, wherein the lithium precursor is contained in the composition in an amount corresponding to a stoichiometric excess for a compound of Formula 1
Li(7.2-2x-3y)AxMyLa3Zr2O12 (1)
wherein A is Ca or Mg, M is Al or Ga, and wherein 0≤x≤0.5 and 0≤y≤0.5,
relative to a content of the lanthanum precursor, the zirconium precursor, and the Ca precursor, the Mg precursor, the Al precursor and the Ga precursor, if present.

### Claim 4 (depends on 3)

The method of claim 3, wherein the stoichiometric excess is 1% to 300%.

### Claim 5 (depends on 1)

The method of claim 1, wherein the lanthanum precursor and the zirconium precursor are contained in the composition in an amount corresponding to a stoichiometric amount for a compound of Formula 1
Li(7.2-2x-3y)AxMyLa3Zr2O12 (1)
wherein A is Ca or Mg, M is Al or Ga, and wherein 0≤x≤0.5 and 0≤y≤0.5,
relative to a content of the lanthanum precursor, the zirconium precursor, and the Ca precursor, the Mg precursor, the Al precursor, and the Ga precursor, if present.

### Claim 6 (depends on 1)

The method of claim 1, wherein a concentration of the lithium precursor, the lanthanum precursor, and the zirconium precursor is 0.01 molar to 0.1 molar, based on the compound of Formula 1
Li(7.2-2x-3y)AxMyLa3Zr2O12 (1)
wherein A is Ca or Mg, M is Al or Ga, and wherein 0≤x≤0.5and 0≤y≤0.5.

### Claim 7 (depends on 1)

The method of claim 1, wherein the composition is a solution.

### Claim 8 (depends on 1)

The method of claim 1, wherein the disposing of the composition comprises spraying the composition.

### Claim 9 (depends on 8)

The method of claim 8, wherein the spraying comprises using air as a carrier gas.

### Claim 10 (depends on 9)

The method of claim 9, wherein the spraying comprises spraying with a pressure at an atomizer of 0.01 megaPascals to 0.1 megaPascals.

### Claim 11 (depends on 10)

The method of claim 10, wherein the spraying comprises spraying in air at an ambient pressure.

### Claim 12 (depends on 1)

The method of claim 1, wherein the heat-treating comprises heat-treating at 450° C. to 550° C.

### Claim 13 (depends on 12)

The method of claim 12, wherein the heat-treating comprises heat-treating for 2 hours to 20 hours.

### Claim 14 (depends on 1)

The method of claim 1, wherein the lithium solid electrolyte has a thickness of 0.1 μm to 10 μm.

### Claim 15 (depends on 1)

The method of claim 1, wherein the lithium solid electrolyte has a degree of crystallinity of 50% to 99%.

### Claim 16 (depends on 1)

The method of claim 1, wherein the lithium solid electrolyte has a local stress 10 megaPascals to 10 gigaPascals, when determined by multi-beam optical sensing.

### Claim 17 (depends on 1)

The method of claim 1, wherein the lithium solid electrolyte has a residual stress of 10 megaPascals to 10 gigaPascals, when determined by multi-beam optical sensing.

### Claim 18 (depends on 1)

The method of claim 1,
wherein the lithium solid electrolyte has a peak in a Raman spectrum that corresponds to a peak in cubic Li7La3Zr2O12 phase between 350 cm−1 and 400 cm−1, and
wherein the peak in the Raman spectrum of the lithium solid electrolyte occurs at a wavenumber between 0 cm−1 and 50 cm−1 greater than a wavenumber of the corresponding peak in cubic Li7La3Zr2O12.

### Claim 19

A lithium solid electrolyte of Formula 1
Li(7.2-2x-3y)AxMyLa3Zr2O12 (1)
wherein A is Ca or Mg, M is Al or Ga, and wherein 0≤x≤0.5 and 0≤y≤0.5, and having a having a local stress of 10 megaPascals to 10 gigaPascals, when determined by multi-beam optical sensing.

### Claim 20 (depends on 19)

The lithium solid electrolyte of claim 19,
wherein the lithium solid electrolyte has a residual stress of 10 megaPascals to 10 gigaPascals, when determined by multi-beam optical sensing.

### Claim 21 (depends on 20)

The lithium solid electrolyte of claim 20, wherein the lithium solid electrolyte has a peak in a Raman spectrum that corresponds to a peak of cubic Li7La3Zr2O12 between 350 cm−1 and 400 cm−1, and
wherein the peak in the Raman spectrum of the lithium solid electrolyte occurs at a wavenumber between 1 cm−1 and 50 cm−1 greater than a wavenumber of the corresponding peak of cubic Li7La3Zr2O12.

### Claim 22 (depends on 1)

A negative electrode for a lithium battery, the negative electrode comprising:
lithium metal; and
the lithium solid electrolyte of claim 1 on the lithium metal.

### Claim 23 (depends on 19)

A negative electrode for a lithium battery, the negative electrode comprising:
lithium metal; and
the lithium solid electrolyte of claim 19 on the lithium metal.

### Claim 24 (depends on 1)

A lithium battery comprising:
a positive electrode;
a negative electrode; and
the lithium solid electrolyte of claim 1 between the positive electrode and the negative electrode.

### Claim 25 (depends on 19)

A lithium battery comprising:
a positive electrode;
a negative electrode; and
the lithium solid electrolyte of claim 19 between the positive electrode and the negative electrode.