# US 2020/0403216 A1 · Early transition metal stabilized high capacity cobalt free cathodes for lithium-ion batteries

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0403216 A1
- Document ID: US20200403216A1
- Status: Published application
- Kind: A1
- Application number: 16/448,169
- Filed: 2019-06-21
- Published: 2020-12-24
- Earliest claimed: 2019-06-21
- Assignees: UT-Battelle, LLC
- Applicants: Ut-Battelle, LLC
- Inventors: Jagjit Nanda; Ilias Belharouak; Ethan C. Self; Devendrasinh Udaisinh Darbar
- Web page: https://patentgrep.com/patent/US20200403216A1

## CPC

- H01M 4/131: Electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/0404: {by coating on electrode collectors}
- H01M 4/1391: of electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/366: {as layered products}
- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- H01M 4/5825: {Oxygenated metallic salts or polyanionic structures, e.g. borates, phosphates, silicates, olivines}
- H01M 4/623: {fluorinated polymers}
- H01M 4/625: {Carbon or graphite}
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 10/0568: characterised by the solutes
- H01M 10/0569: characterised by the solvents
- H01M 2004/028: {Positive electrodes}
- H01M 2300/0037: Mixture of solvents
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A cathode for a lithium battery includes LiNi0.5-x/2Mn0.5-x/2MxO2 where M is at least one selected from the group consisting of Mo, Ti, Cr, Zr and V, and x is between 0.005-0.02. The LiNi0.5-x/2Mn0.5-x/2MxO2 can be coated with Mn2P2O7. The Mn2P2O7 can be 1-3 wt. %, based on the total weight of the LiNi0.5-x/2Mn0.5-x/2 MxO2 and Mn2P2O7. A cathode composition, a lithium battery, and a method of making a lithium battery are also disclosed.

## Claims

### Claim 1

A cathode for a lithium battery, comprising LiNi0.5-x/2Mn0.5-x/2MxO2 where M is at least one selected from the group consisting of Mo, Ti, Cr, Zr and V, and x is between 0.005-0.02.

### Claim 2 (depends on 1)

The cathode of claim 1, wherein the LiNi0.5-x/2 Mn0.5-x/2MxO2 is coated with Mn2P2O7.

### Claim 3 (depends on 2)

The cathode of claim 2, wherein the Mn2P2O7 is 1-3 wt. %, based on the total weight of the LiNi0.5-x/2Mn0.5-x/2MxO2 and Mn2P2O7.

### Claim 4 (depends on 1)

The cathode of claim 1, wherein the LiNi0.5-x/2 Mn0.5-x/2MxO2 is provided as particles having a diameter of from 50 to 500 nm.

### Claim 5 (depends on 4)

The cathode of claim 4, wherein the LiNi0.5-x/2Mn0.5-x/2MxO2 is coated with Mn2P2O7, and the coating is between 1 and 5 nm thick.

### Claim 6 (depends on 1)

The cathode of claim 1, wherein M is Mo.

### Claim 7 (depends on 1)

The cathode of claim 1, wherein the cathode is cobalt free.

### Claim 8 (depends on 1)

The cathode of claim 1, wherein M is substituted at cation sites.

### Claim 9 (depends on 1)

The cathode of claim 1, further comprising a conductive carbon and a binder.

### Claim 10 (depends on 1)

The cathode of claim 1, wherein the LiNi0.5-x/2Mn0.5-x/2MxO2 is a solid solution wherein the lithium concentration is in excess between 15 to 30 at % to form a lithium excess composition.

### Claim 11 (depends on 1)

The cathode of claim 1, wherein with usable capacity of the cathode attains 180 mAh/g when cycled to 4.5 V vs. Li/Li+.

### Claim 12

A cathode composition for a lithium battery, comprising LiNi0.5-x/2Mn0.5-x/2MxO2, where M is at least one selected from the group consisting of M=Mo, Ti, Cr, Zr and V, and x is 0.005-0.02.

### Claim 13 (depends on 12)

The cathode composition of claim 12, wherein the LiNi0.5-x/2Mn0.5-x/2MxO2, is provided as particles, and the particles are coated with Mn2P2O7.

### Claim 14 (depends on 13)

The cathode composition of claim 13, wherein the Mn2P2O7 coating is 1-3 wt %, based on the total weight of the LiNi0.5-x/2 Mn0.5-x/2MxO2 and Mn2P2O7.

### Claim 15 (depends on 13)

The cathode composition of claim 13, wherein the LiNi0.5-x/2 Mn0.5-x/2MxO2 is provided as particles having a diameter of from 50 to 500 nm.

### Claim 16 (depends on 15)

The cathode composition of claim 15, wherein the LiNi0.5-x/2Mn0.5-x/2MxO2 is coated with Mn2P2O7, and the coating is between 1 and 5 nm thick.

### Claim 17 (depends on 1)

The cathode of claim 1, further comprising conductive carbon and a binder.

### Claim 18

A lithium battery, comprising:
a cathode comprising LiNi0.5-x/2Mn0.5-x/2MxO2, where M is at least one selected from the group consisting of Mo, Ti, Cr, Zr and V, and x is 0.005 to 0.02;
an anode;
a separator; and
an electrolyte.

### Claim 19 (depends on 18)

The battery of claim 18, wherein the LiNi0.5-x/2Mn0.5-x/2MxO2, is provided as particles, and the particles are coated with Mn2P2O7.

### Claim 20 (depends on 19)

The battery of claim 19, wherein the Mn2P2O7 coating is 1-3 wt %, based on the total weight of the LiNi0.5-x/2 Mn0.5-x/2MxO2 and Mn2P2O7.

### Claim 21 (depends on 18)

The battery of claim 18, wherein the LiNi0.5-x/2 Mn0.5-x/2MxO2 is provided as particles having a diameter of from 50 to 500 nm.

### Claim 22 (depends on 21)

The battery of claim 21, wherein the LiNi0.5-x/2Mn0.5-x/2MxO2 is coated with Mn2P2O7, and the coating is between 1 and 5 nm thick.

### Claim 23 (depends on 18)

The battery of claim 18, wherein the cathode is cobalt free.

### Claim 24 (depends on 18)

The battery of claim 18, wherein M is substituted at cation sites.

### Claim 25 (depends on 18)

The battery of claim 18, wherein with usable capacity of the cathode attains 180 mAh/g when cycled between 2.0-4.5 V vs. Li/Li+.

### Claim 26

A method of making a lithium battery, comprising the steps of:
providing LiNi0.5-x/2Mn0.5-x/2MxO2, where M is at least one selected from the group consisting of Mo, Ti, Cr, Zr and V, and x is 0.005 to 0.02;
mixing the LiNi0.5-x/2Mn0.5-x/2MxO2 with conductive carbon, a binder and a solvent to form a slurry, and casting the slurry onto a current collector and drying the slurry to form a cathode;
combining the cathode with an anode, a separator and an electrolyte to form a battery.

### Claim 27 (depends on 26)

The method of claim 26, wherein the LiNi0.5-x/2 Mn0.5-x/2MxO2 is provided as particles having a diameter of from 50 to 500 nm.

### Claim 28 (depends on 27)

The method of claim 27, wherein the LiNi0.5-x/2Mn0.5-x/2MxO2 particles are coated with Mn2P2O7.

### Claim 29 (depends on 28)

The method of claim 28, wherein the coating is between 1 and 5 nm thick.

### Claim 30 (depends on 26)

The method of claim 26, wherein the binder is PVDF.

### Claim 31 (depends on 26)

The method of claim 26, wherein the solvent is N-Methyl-2-Pyrrolidone (NMP).

### Claim 32 (depends on 26)

The method in claim 26, wherein the electrolyte is 1.2 M LiPF6 in EC-EMC in 3:7 weight ratio.

### Claim 33 (depends on 26)

The method in claim 26, wherein the anode composition is a mixture of graphite and a binder.