# US 2020/0403194 A1 · Battery packaging material, method for manufacturing the same, and battery

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2020/0403194 A1
- Document ID: US20200403194A1
- Status: Published application
- Kind: A1
- Application number: 16/968,446
- Filed: 2019-02-06
- Published: 2020-12-24
- Earliest claimed: 2018-02-07
- Assignees: Dai Nippon Printing Co., Ltd.
- Applicants: Dai Nippon Printing Co., Ltd.
- Inventors: Makoto AMANO; Takanori YAMASHITA
- Web page: https://patentgrep.com/patent/US20200403194A1

## CPC

- B32B 7/12: using interposed adhesives or interposed materials with bonding properties
- H01M 50/124: having a layered structure
- B32B 15/085: comprising polyolefins
- B32B 15/09: comprising polyesters
- B32B 15/20: comprising aluminium or copper {(B32B15/016 and B32B15/017 take precedence)}
- B32B 27/32: comprising polyolefins {(comprising vinyl (co)polymers or acrylic (co)polymers B32B27/30)}
- B32B 27/325: {comprising polycycloolefins}
- B32B 27/36: comprising polyesters
- H01M 50/105: Pouches or flexible bags
- H01M 50/119: Metals
- H01M 50/121: Organic material
- H01M 50/1243: {characterised by the internal coating on the casing}
- H01M 50/1245: {characterised by the external coating on the casing}
- H01M 50/129: with two or more layers of only organic material
- H01M 50/131: characterised by physical properties, e.g. gas permeability, size or heat resistance
- H01M 50/133: Thickness
- H01M 50/136: Flexibility or foldability
- H01M 50/178: for pouch or flexible bag cells
- H01M 50/193: Organic material
- H01M 50/198: characterised by physical properties, e.g. adhesiveness or hardness
- H01M 50/55: on the same side of the cell
- H01M 50/553: Terminals adapted for prismatic, pouch or rectangular cells
- H01M 50/557: Plate-shaped terminals
- H01M 50/562: characterised by the material
- B32B 2250/03: 3 layers
- B32B 2255/06: on metal layer
- B32B 2255/20: Inorganic coating
- B32B 2307/304: Insulating
- B32B 2307/306: Resistant to heat
- B32B 2307/31: Heat sealable
- B32B 2307/732: Dimensional properties
- B32B 2307/748: Releasability
- B32B 2439/40: Closed containers
- B32B 2457/10: Batteries
- H01G 2/10: Housing; Encapsulation
- H01G 9/08: Housing; Encapsulation
- H01G 11/78: Cases; Housings; Encapsulations; Mountings
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 2220/20: Batteries in motive systems, e.g. vehicle, ship, plane
- Y02E 60/10: Energy storage using batteries
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- H01G: CAPACITORS; CAPACITORS, RECTIFIERS, DETECTORS, SWITCHING DEVICES, LIGHT-SENSITIVE OR TEMPERATURE-SENSITIVE DEVICES OF THE ELECTROLYTIC TYPE (selection of specified materials as dielectric H01B3/00; capacitors having potential barriers H10D1/62, H10K10/10)
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A battery packaging material is configured from a laminate including, at a minimum, a polyester film layer, an aluminum alloy foil layer, and a heat fusible resin layer in the stated order. The thickness of the polyester film layer is 23-27 μm (inclusive), the thickness of the aluminum alloy foil layer is 27-43 μm (inclusive), the thickness of the heat fusible resin layer is 70-100 μm (inclusive), and the insulation breakdown voltage of the surface of the polyester film layer side is 13 kV or greater.

## Claims

### Claim 1

A battery packaging material comprising a laminate in which, at least, a polyester film layer, an aluminum alloy foil layer, and a heat-sealable resin layer are laminated in this order,
wherein a thickness of the polyester film layer is 23 μm or more and 27 μm or less,
a thickness of the aluminum alloy foil layer is 27 μm or more and 43 μm or less, a thickness of the heat-sealable resin layer is 70 μm or more and 100 μm or less, and
a dielectric breakdown voltage of a surface on a side of the polyester film layer is 13 kV or more.

### Claim 2 (depends on 1)

The battery packaging material according to claim 1, wherein a logarithmic decrement ΔE at 80° C. in rigid-body pendulum measurement of a surface on a side of the heat-sealable resin layer of the laminate is 0.04 or more.

### Claim 3 (depends on 1)

The battery packaging material according to claim 1, wherein the polyester film layer comprises a stretched polyethylene terephthalate film.

### Claim 4 (depends on 1)

The battery packaging material according to claim 1, wherein the heat-sealable resin layer comprises a random polypropylene film.

### Claim 5 (depends on 1)

The battery packaging material according to claim 1, wherein the aluminum alloy foil layer comprises an aluminum alloy having a composition defined in JIS H4160:1994 A8021H-O.

### Claim 6 (depends on 1)

The battery packaging material according to claim 1, wherein a temperature difference T1 and a temperature difference T2 are measured by the following method, and a value obtained by dividing the temperature difference T2 by the temperature difference T1 is 0.55 or more.
(Measurement of temperature difference T1)
By differential scanning calorimetry, the temperature difference T1 between an extrapolation melting onset temperature and an extrapolation melting termination temperature of a melting peak temperature of the heat-sealable resin layer is measured.
(Measurement of temperature difference T2)
In an environment of a temperature of 85° C., the heat-sealable resin layer is allowed to stand for 72 hours in an electrolyte which is a solution in which a concentration of lithium hexafluorophosphate is 1 mol/l and a volume ratio of ethylene carbonate, diethyl carbonate and dimethyl carbonate is 1:1:1, and then dried. By differential scanning calorimetry, the temperature difference T2 between the extrapolation melting onset temperature and the extrapolation melting termination temperature of the melting peak temperature of the heat-sealable resin layer after drying is measured.

### Claim 7 (depends on 1)

The battery packaging material according to claim 1, wherein the logarithmic decrement ΔE at 120° C. in the rigid-body pendulum measurement of a surface of the heat-sealable resin layer on a side of the aluminum alloy foil layer is 0.50 or less.

### Claim 8 (depends on 1)

The battery packaging material according to claim 1, wherein the battery packaging material is used for a vehicle battery.

### Claim 9 (depends on 1)

A battery comprising a battery element comprising at least a positive electrode, a negative electrode, and an electrolyte, the battery element being stored in a package comprising the battery packaging material according to claim 1.

### Claim 10 (depends on 1)

A battery comprising:
a battery element comprising at least a positive electrode, a negative electrode, and an electrolyte;
a package for sealing the battery element; and
a metal terminal electrically connected to each of the positive electrode and the negative electrode and protruding to the outside of the package,
wherein the package comprises the battery packaging material according to claim 1, and
an adhesive film is present between the metal terminal and the package.

### Claim 11 (depends on 10)

The battery according to claim 10, wherein a thickness of the metal terminal is 100 μm or more.

### Claim 12 (depends on 10)

The battery according to claim 10, wherein a thickness of the adhesive film is 70 μm or more.

### Claim 13

A method for manufacturing a battery packaging material comprising a step of laminating at least, a polyester film layer, an aluminum alloy foil layer, and a heat-sealable resin layer in this order to obtain a laminate, wherein
a thickness of the polyester film layer is 23 μm or more and 27 μm or less,
a thickness of the aluminum alloy foil layer is 27 μm or more and 43 μm or less,
a thickness of the heat-sealable resin layer is 70 μm or more and 100 μm or less, and
a dielectric breakdown voltage of a surface on a side of the polyester film layer is 13 kV or more.